Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Shear Strength | 35.0 MPa | 5080 psi | 0°, Short Beam |
Hexcel® HexPly® ES 84 120°C Curing Epoxy Matrix, Aramid Balanced fabric 175 g/m2 Information provided by HexCel |
|||
Shear Strength | 35.0 MPa @Temperature 135 °C |
5080 psi @Temperature 275 °F |
0º, ILSS Short Beam, Wet; EN2563 |
Hexcel® HexPly® M42 180°C (350°F) Curing Epoxy Matrix, 50%/G939 HS Carbon Information provided by HexCel |
|||
Shear Strength | 35.0 MPa @Temperature 100 °C |
5080 psi @Temperature 212 °F |
0º, ILSS (Short Beam), Wet; EN2563 |
Hexcel® HexPly® M12 135°C Curing Epoxy Matrix, 45% 46280 Fiber Information provided by HexCel |
|||
Shear Strength | 35.0 MPa @Thickness >=5.00 mm |
5080 psi @Thickness >=0.197 in |
24hr/23°C/50% RH; IEC/EN 60893-2 5.5 |
Elektro-Isola Etronax P EP Phenolic, Polyester Fabric Reinforcement, Light Yellow, Sheets Description: This material is exceptionally strong and tough. Very low water absorption and the lowest swelling in water. High resistance to chemicals, including SF6 gas. Applications: Can be used i.. |
|||
Shear Strength | 35.0 MPa @Thickness >=5.00 mm |
5080 psi @Thickness >=0.197 in |
24hr/23°C/50% RH; IEC/EN 60893-2 5.5 |
Elektro-Isola Etronit I Phenolic, Paper Reinforcement, Dark Brown, Sheets Description: High-voltage insulation material at mains frequency. High breakdown voltage in oil and reasonable breakdown voltage in air at normal air humidity.Application: Insulation material in hig.. |
|||
Shear Strength | 35.0 MPa @Thickness >=5.00 mm |
5080 psi @Thickness >=0.197 in |
24hr/23°C/50% RH; IEC/EN 60893-2 5.5 |
Elektro-Isola Etronit II Phenolic, Paper Reinforcement, Dark Brown, Sheets Description: Mechanical and electrical applications used at normal air humidity. Very good electrical values.Information provided by Elektro-Isola |
|||
Shear Strength | 35.0 MPa @Thickness >=5.00 mm |
5080 psi @Thickness >=0.197 in |
24hr/23°C/50% RH; IEC/EN 60893-2 5.5 |
Elektro-Isola Etronit IIQ Phenolic, Paper Reinforcement, Dark Brown, Sheets Description: Mechanically a good Etronit type with electrical properties adequate for insulation in low-voltage applications. Applications: Used in electrical appliances, bus-bar carriers, partition.. |
|||
Shear Strength | 35.0 MPa @Thickness >=5.00 mm |
5080 psi @Thickness >=0.197 in |
24hr/23°C/50% RH; IEC/EN 60893-2 5.5 |
Elektro-Isola Etronit IIQ R Phenolic, Paper Reinforcement, Yellow, Sheets Description: Mechanically a good Etronit type with electrical properties adequate for insulation in low-voltage applications. Applications: Used in electrical appliances, bus-bar carriers, partition.. |
|||
Shear Strength | 35.0 MPa @Thickness >=5.00 mm |
5080 psi @Thickness >=0.197 in |
24hr/23°C/50% RH; IEC/EN 60893-2 5.5 |
Elektro-Isola Etronit IIQ R XX Phenolic, Paper Reinforcement, Yellow, Sheets Description: Mechanically a good Etronit type with electrical properties adequate for insulation in low-voltage applications. Applications: Used in electrical appliances, bus-bar carriers, partition.. |
|||
Shear Strength | 35.0 MPa @Thickness >=5.00 mm |
5080 psi @Thickness >=0.197 in |
24hr/23°C/50% RH; IEC/EN 60893-2 5.5 |
Elektro-Isola Etronit IIQ S AL Phenolic, Paper Reinforcement, Black with foil, Sheets Description: Mechanically a good Etronit type with electrical properties adequate for insulation in low-voltage applications. Material is black throughout. Elegant surface finish combined with good .. |
|||
Shear Strength | 35.0 MPa @Thickness >=5.00 mm |
5080 psi @Thickness >=0.197 in |
24hr/23°C/50% RH; IEC/EN 60893-2 5.5 |
Elektro-Isola Etronit IIQ S Phenolic, Paper Reinforcement, Black, Sheets Description: Mechanically a good Etronit type with electrical properties adequate for insulation in low-voltage applications. Material is black throughout. Elegant surface finish combined with good .. |
|||
Shear Strength | 35.0 MPa @Thickness >=5.00 mm |
5080 psi @Thickness >=0.197 in |
24hr/23°C/50% RH; IEC/EN 60893-2 5.5 |
Elektro-Isola Etronit IR Phenolic, Paper Reinforcement, Dark Brown, Sheets Description: High-voltage insulation material at mains frequency. High breakdown voltage in oil and reasonable breakdown voltage in air at normal air humidity. Very low water absorption.Application:.. |
|||
Shear Strength | 35.0 MPa @Thickness >=5.00 mm |
5080 psi @Thickness >=0.197 in |
24hr/23°C/50% RH; IEC/EN 60893-2 5.5 |
Elektro-Isola Etronit IS Phenolic, Paper Reinforcement, Dark Brown, Sheets Description: Very good high-voltage insulation material. Very high breakdown voltage, in particular parallel to the layers. Dimensionally stable.Application: Insulation material in high-voltage tap .. |
|||
Shear Strength | 35.0 MPa @Thickness >=5.00 mm |
5080 psi @Thickness >=0.197 in |
24hr/23°C/50% RH; IEC/EN 60893-2 5.5 |
Elektro-Isola Etronit MBM Phenolic/melamine, Paper Reinforcement, Grey/also other Colors, Sheets Description: The surfaces consist of melamine, which ensures a scratch-resistant, tracking-resistant surface. The surfaces are grey as standard, but other colors can be selected from the color chart.. |
|||
Shear Strength | 35.0 MPa @Thickness >=5.00 mm |
5080 psi @Thickness >=0.197 in |
24hr/23°C/50% RH; IEC/EN 60893-2 5.5 |
Elektro-Isola G-Etronax PM 953 Polyester, Glass Mat, Off White, Sheets Description: Good electrical properties such as high breakdown voltage in air and oil and highest arc resistance and tracking resistance. Self-extinguishing. Low smoke emission, halogen-free. Very m.. |
|||
Shear Strength | 35.0 MPa @Thickness >=5.00 mm |
5080 psi @Thickness >=0.197 in |
24hr/23°C/50% RH; IEC/EN 60893-2 5.5 |
Elektro-Isola G-Etronax PM GPO 3 Polyester, Glass Mat, Red, Sheets Description: Good electrical properties such as high breakdown voltage in air and oil and highest arc resistance and tracking resistance. Self-extinguishing. Low smoke emission, halogen-free.Applica.. |
|||
Shear Strength | 35.0 MPa @Thickness >=5.00 mm |
5080 psi @Thickness >=0.197 in |
24hr/23°C/50% RH; IEC/EN 60893-2 5.5 |
Elektro-Isola G-Etronax PM H Polyester, Glass Mat, Creme, Sheets Description: A reasonably-priced alternative to other high-temperature types. Low thermal conductivity. Applications: Used as, among other things, thermal insulation plates where high strength prope.. |
|||
Shear Strength | 35.0 MPa | 5080 psi | |
Cytec Thornel® P-100 Carbon Fiber/Epoxy Advanced Composite System Data provided by the manufacturer, Amoco Performance Products, Inc. Measured in proprietary aerospace grade epoxy formulations at 0.62 fiber content by volume.Thornel® products were sold by Amoco .. |
|||
Shear Strength | 35.0 MPa | 5080 psi | Short Beam |
Cytec Thornel® VCB-20 Carbon Cloth/Epoxy Composite Data provided by the manufacturer, Amoco Performance Products, Inc. Cured ply 0.47 mm thick, 55% fiber vol.Thornel® products were sold by Amoco and are now owned by Cytec. |
|||
Shear Strength | >= 35.0 MPa | >= 5080 psi | Parallel to laminations; IEC 1212-2 5.6 |
Hippe PI GC 301 Woven Glass Cloth Reinforced Phenolic Sheet Used in electrical and mechanical applications. Very good mechanical and electrical properties at high temperature.Information provided by Hippe. |
|||
Shear Strength | 35.0 MPa @Thickness >=5.00 mm |
5080 psi @Thickness >=0.197 in |
24hr/23°C/50% RH; IEC/EN 60893-2 5.5 |
Elektro-Isola Etronit 201 MBM Phenolic/melamine, Paper Reinforcement, Grey/also other Colors, Sheets Description: This material is not standardized, but the base material is the same as Etronit 201 M. The surfaces consist of melamine, which ensures a scratch-resistant, tracking-resistant surface. T.. |
|||
Shear Strength | 35.0 MPa @Thickness >=5.00 mm |
5080 psi @Thickness >=0.197 in |
24hr/23°C/50% RH; IEC/EN 60893-2 5.5 |
Elektro-Isola Etronit 201M Phenolic, Paper Reinforcement, Dark Brown, Sheets Description: Grade with high mechanical properties but the lowest electrical properties of all Etronit types. Used for mechanical applications.Applications: Dies, topplates and back-up plates for dr.. |
|||
Shear Strength | 35.0 MPa @Thickness >=5.00 mm |
5080 psi @Thickness >=0.197 in |
24hr/23°C/50% RH; IEC/EN 60893-2 5.5 |
Elektro-Isola Etronit 201M S Phenolic, Paper Reinforcement, Black, Sheets Description: Grade with high mechanical properties but the lowest electrical properties of all Etronit types. Used for mechanical applications. The material is black throughout. Used where the mecha.. |