Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Dart Drop | 3.50 g/micron | 88.9 g/mil | ASTM D1709 |
SABIC 118 Series Linear Low Density Polyethylene for Blown Film Product Description: 118 series resins are Linear Low Density Polyethylene grades suitable for general purpose packaging. Films produced using these resins yield good tensile properties, impact st.. |
|||
Dart Drop | 3.50 g/micron | 88.9 g/mil | F<sub>50</sub>,38mm dart 66mm height; ASTM D1709 |
Reliance Industries Reclair F18010 Polyethylene Butene comonomer based Linear Low Density Polyethylene blow film grade. Applications:lamination films. Information provided by Reliance Industries |
|||
Dart Drop | 3.50 g/micron | 88.9 g/mil | F 50; ASTM D1709/A |
NOVA Chemicals Novapol® PF-Y821-B Butene LLDPE Film Resin
(discontinued **) Film Properties. Features: Good stiffness and machinability, good clarity with LDPE.Applications: General purpose packaging, liners.Data provided by the manufacturer. |
|||
Dart Drop | 3.50 g/micron | 88.9 g/mil | F 50; ASTM D1709/A |
NOVA Chemicals Novapol® PF-Y821-D Butene LLDPE Film Resin
(discontinued **) Film Properties. Features: Good stiffness and machinability, good blocking resistance.Applications: Bags-on-roll, produce bags, garment film, trash bags.Data provided by the manufacturer. |
|||
Dart Drop | 3.50 g/micron | 88.9 g/mil | ASTM D1709 |
Lotte Chemical Titan TITANEX® LF2021 Linear low density polyethylene resin
(discontinued **) LF2021 is a pelleted linear low density polyethylene resin formulated with antioxidant, high antiblock and slip agent. This product is used for blown and cast film extrusion which offers outstandin.. |
|||
Dart Drop | 3.50 g/micron | 88.9 g/mil | ASTM D1709 |
Lotte Chemical Titan TITANEX® LF2024 Linear low density polyethylene resin
(discontinued **) LF2024 is a pelleted linear low density polyethylene resin formulated with antioxidant. This product is used for blown and cast film extrusion which offers outstanding toughness, extrudability and .. |
|||
Dart Drop | 3.50 g/micron | 88.9 g/mil | 1.5 in. dart/26 in. drop height; ASTM D 1709 |
Chevron Phillips HiD® 9640 HDPE Blown Film Resin
(discontinued **) Copolymerization Enhances Film Toughness, Unique Combination of Density and Melt Index, Excellent Strength Properties as well as Good Heat Seal, Lower Density Imparts a Softer Feel and Lesser Tenden.. |
|||
Dart Drop | 3.50 g/micron | 88.9 g/mil | 1.5 in. dart/26 in. drop height; ASTM D 1709 |
Chevron Phillips HiD® 9650 HDPE Blown Film Resin
(discontinued **) Resin Type: Linear Polyethylene CopolymerCharacteristics: Copolymerization Enhances Film Toughness, Excellent Film Drawdown, Unique Molecular Architecture Gives Moisture Barrier Properties Typical o.. |
|||
Dart Drop | 3.50 g/micron | 88.9 g/mil | F<sub>50</sub>,38mm dart 66mm height; ASTM D1709 |
Reliance Industries Reclair F19010 Polyethylene Blow film Linear Low Density Polyethylene grade. Reclair F19010 is butene comonomer based, with optimum levels of antioxidants, antiblocking agents, slip additives, and polymer processing aids. Th.. |
|||
Dart Drop | 3.50 g/micron | 88.9 g/mil | |
Dow LDPE 682I Low Density Polyethylene, Film Grade DOW LDPE 682I barefoot resin is used for shrink, frozen food, and heavy duty film applications. This material complies with U.S.FDA regulation 21 CFR 177.1520(c) 2.1 for food contact applications. T.. |
|||
Dart Drop | 3.50 g/micron | 88.9 g/mil | |
Dow LDPE 494A Low Density Polyethylene, Film Grade DOW LDPE 494A resin, is a high strength, general purpose resin used for shipping sack, industrial liner and produce film applications. DOW LDPE 494A resin can be blended with most linear low density.. |