Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Elmendorf Tear Strength TD | 100 g | 100 g | ASTM D1922 |
ExxonMobil Escorene® LD-108 LDPE Packaging Film Resin, High Clarity
(discontinued **) Data provided by the manufacturer, Exxon Chemical.A homopolymer high clarity film resin with a good balance of toughness, stiffness, and drawdown capability. This resin has good machinability in ba.. |
|||
Elmendorf Tear Strength TD | 100 g | 100 g | ASTM D1922 |
ExxonMobil Escorene® LD-302 EVA Film Resin, High Clarity, High Impact
(discontinued **) Data provided by the manufacturer, Exxon Chemical.A 3.4% vinyl acetate copolymer, high clarity film resin. The combination of low melt index and comonomer content helps produce films which exhibit .. |
|||
Elmendorf Tear Strength TD | 100 g | 100 g | ASTM D1922 |
ExxonMobil Escorene® LD-303 EVA Film Resin, Clarity, High Impact
(discontinued **) Data provided by the manufacturer, Exxon Chemical.A 3.8% vinyl acetate copolymer, clarity film resin. The low melt index and comonomer context of this resin help produce films with superior impact .. |
|||
Elmendorf Tear Strength TD | 100 g | 100 g | ASTM D1922 |
ExxonMobil Escorene® LD-306 EVA Film Resin, High Clarity, Very High Impact
(discontinued **) Data provided by the manufacturer, Exxon Chemical.A 5.5% vinyl acetate copolymer, high clarity film resin. Film made from this resin exhibits superior impact strength and heat sealability.Applicati.. |
|||
Elmendorf Tear Strength TD | 100 g | 100 g | ASTM D1922 |
ExxonMobil Escorene® LD-307 EVA Film Resin, Clarity, High Impact
(discontinued **) Data provided by the manufacturer, Exxon Chemical.A 5.0% vinyl acetate copolymer, clarity film resin. Film made from this resin has superior impact strength and heat sealability.Applications: Froze.. |
|||
Elmendorf Tear Strength TD | 100 g | 100 g | ASTM D1922 |
ExxonMobil Escorene® LD-312 EVA Film Resin, High Impact
(discontinued **) Data provided by the manufacturer, Exxon Chemical.A 4.6% vinyl acetate copolymer resin for films with good toughness. This resin's low melt index and comonomer content help produce films which exhi.. |
|||
Elmendorf Tear Strength TD | 100 g | 100 g | ASTM D1922 |
ExxonMobil Escorene® LD-314 EVA Packaging Film Resin
(discontinued **) Data provided by the manufacturer, Exxon Chemical.A 3.5% vinyl acetate copolymer resin for higher clarity films. Film made from LD-314 offers good impact strength, heat sealability, and low tempera.. |
|||
Elmendorf Tear Strength TD | 100 g | 100 g | ASTM D1922 |
ExxonMobil Escorene® LD-315 EVA Packaging Film Resin for Frozen Food
(discontinued **) Data provided by the manufacturer, Exxon Chemical.A 5.0% vinyl acetate copolymer clarity film resin. This resin's low melt index and its comonomer contact combine to provide film of special toughne.. |
|||
Elmendorf Tear Strength TD | 100 g | 100 g | ASTM D1922 |
ExxonMobil Escorene® LD-318 EVA Film Resin
(discontinued **) Data provided by the manufacturer, Exxon Chemical.A 9.0% vinyl acetate copolymer film resin. Film made from LD-318 exhibits superior impact strength and heat sealability.Applications: Primal meat b.. |
|||
Elmendorf Tear Strength TD | 100 g | 100 g | ASTM D1922 |
ExxonMobil Escorene® LD-319 EVA Film Resin
(discontinued **) Data provided by the manufacturer, Exxon Chemical.A 9.0% vinyl acetate copolymer film resin. Film made from LD-319 exhibits superior impact strength and heat sealability.Applications: Primal meat b.. |
|||
Elmendorf Tear Strength TD | 100 g | 100 g | ASTM D1922 |
ExxonMobil Escorene® LD-325 EVA Film Resin, High Clarity, High Impact
(discontinued **) Data provided by the manufacturer, Exxon Chemical.A 3.8% vinyl acetate copolymer, high clarity film resin. The combination of low melt index and comonomer content helps produce films which exhibit .. |
|||
Elmendorf Tear Strength TD | 100 g | 100 g | ASTM D1922 |
LyondellBasell Petrothene® NA951000 Low Density Polyethylene ApplicationsPETROTHENE NA 951 is a series of homopolymer resins specially designed for industrial and consumer packaging and liner and bag applications. NA 951 has an excellent balance of processab.. |
|||
Elmendorf Tear Strength TD | 100 g | 100 g | ASTM D1922 |
LyondellBasell Petrothene® NA967000 Low Density Polyethylene, Film Extrusion Grade Petrothene NA967000 is a low density polyethylene resin designed for blown film, general purpose and industrial packaging applications. NA967000 exhibits good processing characteristics and impact s.. |
|||
Elmendorf Tear Strength TD | 100 g | 100 g | |
Kraton® D1102 + HDPE blend (10/90) Blending KRATON D and G polymers with PE significantly improves the toughness at both room and low temperatures. KRATON polymers are block segments of styrene and rubber monomers (A-B, A-B-A, or [A.. |
|||
Elmendorf Tear Strength TD | 100 g | 100 g | ASTM D1922 |
ExxonMobil LD 144.50 Packaging Film Resin Film made from LD 144.50 offers improved impact strength and heat sealability compared to homopolymer clarity film resins. Typically applications include food packaging, frozen food packaging, and .. |
|||
Elmendorf Tear Strength TD | 100 g | 100 g | ASTM D1922 |
ExxonMobil LDPE LD 136.MN Low Density Polyethylene Resin Product Description: LD 136.MN is a homopolymer film resin with good clarity. The resin is suitable for processing on blown film equipmentAvailability: Latin America, North America and South America.. |
|||
Elmendorf Tear Strength TD | 100 g | 100 g | ASTM D1922 |
ExxonMobil LDPE LD 317.09 Low Density Polyethylene Resin Product Description: LD 317.09 resin is a fractional melt index, 6% vinyl acetate copolymer film resin. Film made from LD 317.09 offers excellent impact strength, tensile properties and heat sealabi.. |
|||
Elmendorf Tear Strength TD | 100 g | 100 g | ASTM D1922 |
ExxonMobil LDPE LD 319.92 Low Density Polyethylene Resin Product Description: LD 319.92 resin is an 8.7% vinyl acetate copolymer film resin. Film made from LD 319.92 exhibits superior impact strength and heat sealability.Availability: Latin America, North.. |
|||
Elmendorf Tear Strength TD | 100 g | 100 g | ASTM D1922 |
ExxonMobil LDPE LD 331.08 Low Density Polyethylene Resin Product Description: LD 331.08 is a 5.9% vinyl acetate copolymer, higher clarity film resin. Film made from this resin exhibits superior impact strength and heat sealability.Availability: Latin Amer.. |
|||
Elmendorf Tear Strength TD | 100 g | 100 g | |
Dow LDPE 494A Low Density Polyethylene, Film Grade DOW LDPE 494A resin, is a high strength, general purpose resin used for shipping sack, industrial liner and produce film applications. DOW LDPE 494A resin can be blended with most linear low density.. |
|||
Elmendorf Tear Strength TD | 100 g | 100 g | gF; ASTM D1922 |
Braskem EB853/72 Blown Film Extrusion Low Density Polyethylene Automatic packaging for several products; High transparency films.Additives: Antiblock, DInformation provided by Braskem. |
|||
Elmendorf Tear Strength TD | 100 g | 100 g | gF; ASTM D1922 |
Braskem EB861 Blown Film Extrusion Low Density Polyethylene Medium-resistance films for general use; Mulching films; Shrink films; Coextrusion.Information provided by Braskem. |
|||
Elmendorf Tear Strength TD | 100 g | 100 g | gF; ASTM D1922 |
Braskem EB861/51 Blown Film Extrusion Low Density Polyethylene Film for general use; Shrink films; Coextrusion.Additives: Antiblock, DInformation provided by Braskem. |
|||
Elmendorf Tear Strength TD | 100 g | 100 g | ASTM-D1922 |
Braskem PB681 LDPE Cast and Blown Film Extrusion, Injection Molding Polyethylene PB681 is a resin produced under high pressure in a tubular reactor. This resin presents excellent 'draw down' (stability to form fine films). The films produced with this resin have excellent optica.. |
|||
Elmendorf Tear Strength TD | 100 g | 100 g | gF; ASTM D1922 |
Braskem PB681/59 Blown Film Extrusion Low Density Polyethylene Description: PB681/59 is a grade produced under high pressure in a tubular reactor. This resin is used for laminating films mainly on paper substrate. It is also used in the extrusion coating proces.. |
|||
Elmendorf Tear Strength TD | 100 g | 100 g | gF; ASTM D1922 |
Braskem BF2021 Cast Film Extrusion Low Density Polyethylene Films for diapers and absorbent articles; Medium resistance films or for general use.Information provided by Braskem. |
|||
Elmendorf Tear Strength TD | 100 g | 100 g | gF; ASTM D1922 |
Braskem EB853 Cast Film Extrusion Low Density Polyethylene LLDPE and HDPE blends.Information provided by Braskem. |
|||
Elmendorf Tear Strength TD | 100 - 170 g | 100 - 170 g | Average value: 152 g Grade Count:3 |
Overview of materials for Low Density Polyethylene (LDPE), Blow Molding Grade This property data is a summary of similar materials in the MatWeb database for the category "Low Density Polyethylene (LDPE), Blow Molding Grade". Each property range of values reported is minimum .. |
|||
Elmendorf Tear Strength TD | 100 g | 100 g | ASTM D1922 |
ExxonMobil Escorene® LD-316 EVA Film Resin, High Clarity, High Impact
(discontinued **) Data provided by the manufacturer, Exxon Chemical.A 1.9% vinyl acetate copolymer, high clarity film resin. Film made from LD-316 offers improved impact strength and heat sealability versus homopoly.. |
|||
Elmendorf Tear Strength TD | 100 g | 100 g | gF; ASTM D1922 |
Braskem BF0323/12HC Blown Film Extrusion Low Density Polyethylene Shrink films; Automatic packaging of liquid products (FFS).Additives: Antiblock, DInformation provided by Braskem. |