Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Kraton® D1102 + HDPE blend (10/90)

Category Polymer , Film , Thermoplastic , Elastomer, TPE , Polyethylene (PE) , HDPE
Manufacturer Kraton
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Kraton® D1102 + HDPE blend (10/90).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Blending KRATON D and G polymers with PE significantly improves the toughness at both room and low temperatures. KRATON polymers are block segments of styrene and rubber monomers (A-B, A-B-A, or [A-B]n). The KRATON D series consists of an unsaturated polymer, either butadiene or isoprene, as the rubber monomer. The high softening point of the HDPE and the low glass transition temperatures of the D1102 elastomeric midblock give the films a broad range of service temperatures, from below freezing to above boiling. All properties listed below are measured on blown film, 1 mil (25 microns) thick. Information provided by the manufacturer, Kraton® Polymers.
Physical Properties Metric English Comments
Melt Flow 0.54 g/10 min
0.54 g/10 min
Mechanical Properties Metric English Comments
Tensile Impact Strength 16.0 kJ/m²
7.61 ft-lb/in²
Machine direction
128 kJ/m²
60.9 ft-lb/in²
Transverse
Elmendorf Tear Strength MD 680 g
680 g
Elmendorf Tear Strength TD 100 g
100 g
Dart Drop Test 133 g
0.293 lb
Using 2 in. (0.508 cm) dia dart, 60 in. (774 cm) drop height.
Copyright © lookpolymers.com All Rights Reserved