Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 28.42 - 60.0 MPa

@Temperature 70.0 - 100 °C
4122 - 8700 psi

@Temperature 158 - 212 °F
Average value: 46.5 MPa Grade Count:6
Overview of materials for Thermoplastic Polyurethane, Elastomer, Ether Grade
This property data is a summary of similar materials in the MatWeb database for the category "Thermoplastic Polyurethane, Elastomer, Ether Grade". Each property range of values reported is minimum a..
Tensile Strength, Ultimate 28.42 - 60.0 MPa

@Time 0.000 - 4.84e+6 sec
4122 - 8700 psi

@Time 0.000 - 1340 hour
Average value: 46.5 MPa Grade Count:6
Overview of materials for Thermoplastic Polyurethane, Elastomer, Ether Grade
This property data is a summary of similar materials in the MatWeb database for the category "Thermoplastic Polyurethane, Elastomer, Ether Grade". Each property range of values reported is minimum a..
Tensile Strength, Ultimate 15.0 - 60.0 MPa

@Temperature 60.0 - 120 °C
2180 - 8700 psi

@Temperature 140 - 248 °F
Average value: 36.7 MPa Grade Count:1
Overview of materials for Polyphenylene Ether, 10% Glass Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Ether, 10% Glass Filled". Specific grades with glass content between 5% and 14% are includ..
Tensile Strength, Ultimate 8.00 - 60.0 MPa

@Temperature 60.0 - 90.0 °C
1160 - 8700 psi

@Temperature 140 - 194 °F
Average value: 29.6 MPa Grade Count:3
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), 20% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), 20% Glass Fiber Filled". Specific grades with glass content betwe..
Tensile Strength, Ultimate 40.0 - 60.0 MPa
5800 - 8700 psi
50 mm/min; ASTM D638
Solvay Specialty Polymers Solef® 3108/0903 Anti-static PVDF Compound  (discontinued **)
Key features of this grade: Anti-static, Formulated. Recommended processing is injection. Available as granules.General information about SOLEF® PVDF: SOLEF® PVDF is a fluorinated semi-crystall..
Tensile Strength, Ultimate 40.0 - 60.0 MPa
5800 - 8700 psi
50 mm/min; ASTM D638
Solvay Specialty Polymers Solef® 3208/0150 Anti-friction PVDF Compound  (discontinued **)
Key features of this grade: Anti-friction, Formulated. Recommended processing is injection. Available as granules.General information about SOLEF® PVDF: SOLEF® PVDF is a fluorinated semi-crysta..
Tensile Strength, Ultimate 37.0 - 60.0 MPa
5370 - 8700 psi
Average value: 51.9 MPa Grade Count:21
Overview of materials for Phenolic, Novolac, Mineral/Flock Filled
This property data is a summary of similar materials in the MatWeb database for the category "Phenolic, Novolac, Mineral/Flock Filled". Each property range of values reported is minimum and maximum ..
Tensile Strength, Ultimate 39.3 - 60.0 MPa
5700 - 8700 psi
Average value: 53.1 MPa Grade Count:3
Overview of materials for Nylon 6/69
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6/69". Each property range of values reported is minimum and maximum values of appropriate MatWeb ..
Tensile Strength, Ultimate 50.0 - 60.0 MPa
7250 - 8700 psi
ASTM D638
Chang Chun Plastic PBT1100L General Purpose PBT
Information provided by Dowell Trading Company Ltd.
Tensile Strength, Ultimate 50.0 - 60.0 MPa
7250 - 8700 psi
ASTM D638
Chang Chun Plastic PBT1200M General Purpose PBT
Information provided by Dowell Trading Company Ltd.
Tensile Strength, Ultimate 1.32 - 60.0 MPa
191 - 8700 psi
Average value: 19.0 MPa Grade Count:22
Overview of materials for Silicone Polyurethane, Ether Based
This property data is a summary of similar materials in the MatWeb database for the category "Silicone Polyurethane, Ether Based". Each property range of values reported is minimum and maximum value..
Tensile Strength, Ultimate 9.00 - 60.0 MPa

@Temperature 60.0 - 120 °C
1310 - 8700 psi

@Temperature 140 - 248 °F
Average value: 36.3 MPa Grade Count:4
Overview of materials for Polypropylene with 20% Glass Fiber Filler
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 20% Glass Fiber Filler". Specific grades with glass content between 15% and 24% are i..
Copyright © lookpolymers.com All Rights Reserved