Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 40.0 - 82.7 MPa | 5800 - 12000 psi | Average value: 57.6 MPa Grade Count:28 |
Overview of materials for Acetal Copolymer, Aramid Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer, Aramid Fiber Filled". Each property range of values reported is minimum and maximum va.. |
|||
Tensile Strength, Ultimate | 25.0 - 82.7 MPa | 3630 - 12000 psi | Average value: 60.5 MPa Grade Count:4 |
Overview of materials for Nylon 6, Stainless Steel Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Stainless Steel Filled". Each property range of values reported is minimum and maximum values o.. |
|||
Tensile Strength, Ultimate | 55.0 - 82.7 MPa | 7980 - 12000 psi | Average value: 65.2 MPa Grade Count:11 |
Overview of materials for Nylon 612, Aramid Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 612, Aramid Fiber Filled". Each property range of values reported is minimum and maximum values of.. |
|||
Tensile Strength, Ultimate | 58.6 - 82.7 MPa | 8500 - 12000 psi | Average value: 66.4 MPa Grade Count:4 |
Overview of materials for Nylon 11 with 10% Glass Fiber Filler This property data is a summary of similar materials in the MatWeb database for the category "Nylon 11 with 10% Glass Fiber Filler". Specific grades with glass content between 5% and 14% are includ.. |
|||
Tensile Strength, Ultimate | 62.1 - 82.7 MPa | 9000 - 12000 psi | |
Bulk Molding Compounds BMC 685 Mineral Filled, Glass Fiber Reinforced Polyester Compound BMC 685 molding compound is a mineral filled, glass fiber-reinforced polyester compound suitable for compression, transfer and stuffer injection molding It is characterized by good moldability, oil .. |
|||
Tensile Strength, Ultimate | 62.1 - 82.7 MPa | 9000 - 12000 psi | |
Bulk Molding Compounds BMC 695 Vinyl Ester Molding Compound BMC 695 vinyl ester molding compound is a mineral filled glass fiber-reinforced vinyl ester compound suitable for compression and injection molding It is characterized by good moldability, oil and s.. |
|||
Tensile Strength, Ultimate | 68.9 - 82.7 MPa | 10000 - 12000 psi | |
Bulk Molding Compounds BMC 810 General Purpose Molding Compound BMC 810 is a general purpose, very high strength compound suitable for compression, transfer and stuffer injection molding. It is characterized by excellent flow and controlled reactivity and is wel.. |
|||
Tensile Strength, Ultimate | 62.0 - 83.0 MPa | 8990 - 12000 psi | Average value: 77.0 MPa Grade Count:10 |
Overview of materials for Acrylic, Cast This property data is a summary of similar materials in the MatWeb database for the category "Acrylic, Cast". Each property range of values reported is minimum and maximum values of appropriate MatW.. |