Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 48.3 MPa | 7000 psi | TM R050-36 |
Resinlab® EP1330 Heat Cure Epoxy Polymer System Resinlab™ EP1330 and EP1330LV are one part heat cure epoxy polymer systems. They can also be used as a small mass potting or staking compounds, or a dam adhesive in and “dam and fill” application.. |
|||
Tensile Strength, Ultimate | 48.3 MPa | 7000 psi | ASTM D412 |
1085A Polyurethane-based Biomedical Elastomer |
|||
Tensile Strength, Ultimate | 48.3 - 103 MPa | 7000 - 15000 psi | Average value: 79.0 MPa Grade Count:10 |
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), 10% Carbon Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), 10% Carbon Fiber Filled". Specific grades with carbon fiber conte.. |
|||
Tensile Strength, Ultimate | 48.3 - 138 MPa | 7000 - 20000 psi | Average value: 88.2 MPa Grade Count:45 |
Overview of materials for Nylon 66, Aramid Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Aramid Fiber Filled". Each property range of values reported is minimum and maximum values of .. |
|||
Tensile Strength, Ultimate | 48.3 MPa | 7000 psi | 50 mm/min; ASTM D638 |
Styron CALIBREâ„¢ 1080 DVD Polycarbonate CALIBREâ„¢ 1080 DVD resin has been developed to meet the high demands of the modern Optical Media Industry and is suitable for standard CD molding (audio or ROM) as well as for recordable optical.. |
|||
Tensile Strength, Ultimate | 48.3 MPa | 7000 psi | |
Elastomer Engineering E50D Polyurethane A polyester-based urethane with excellent strength, resilience, and abrasion resistance. Excellent in heavy-duty applications and where oils and solvents are present. Information provided by Elasto.. |
|||
Tensile Strength, Ultimate | 48.3 MPa | 7000 psi | ASTM D412 |
Lubrizol Estane® AG 8451 Thermoplastic Polyurethane Type: Estane® AG 8451 is a polyether based aliphatic (TPU) specifically formulated to be used as an adhesive interlayer film. AG-8451 is an excellent general purpose polymer for all optical allpha.. |
|||
Tensile Strength, Ultimate | 48.3 MPa | 7000 psi | ASTM D638 |
Ecomass® 1850ZD88 Tungsten Filled Polyamide Nontoxic alternative to Lead (Pb), weighting and balancing applicationsHigh Specific GravityTungsten Powder Filled Polyamide (PA6)Information provided by Technical Polymers |
|||
Tensile Strength, Ultimate | 48.3 MPa | 7000 psi | at 0.2"/min; ASTM D638 |
CPC - Vycom FLAMETEC™ CLEANROOM PVC-C Sheet Material Cleanroom PVC-C sheet material is designed to be the most economical choice in FM 4910 materials. Compression Polymers Corp's Cleanroom PVC-C has been audited and tested in accordance with the FM 49.. |
|||
Tensile Strength, Ultimate | 48.3 MPa @Temperature 760 °C |
7000 psi @Temperature 1400 °F |
|
Crucible Steel 430F Stainless Steel Crucible 430F is a low carbon, high chromium ferritic stainless steel, specially developed for solenoid core applications in corrosive environments. The chemistry is closely controlled to develop o.. |
|||
Tensile Strength, Ultimate | 48.3 MPa | 7000 psi | ASTM D-638 |
CMT Materials REN Shape® 472 Machinable Board for Prototype Tooling & Assembly Fixtures RenShape 472 is a polyurethane-based board designed for CNC machining of production grade checking and assembly fixtures. It may also be used in prototype thermoforming and vacuum forming tooling a.. |
|||
Tensile Strength, Ultimate | 48.3 MPa | 7000 psi | |
Cotronics 4420 One-Part Epoxy |
|||
Tensile Strength, Ultimate | 48.3 MPa | 7000 psi | Crosswise; ASTM D638 |
Bedford Plastics Glass Reinforced Vinylester Structural Fiberglass Profiles Flame retardant grade; see details in the property table.Pultrusion results in the production and supply of one of the worlds strongest and most durable products available today. The pultruded prod.. |
|||
Tensile Strength, Ultimate | 48.3 MPa | 7000 psi | ASTM D638 |
Applied Composites 8033 Polyester SMC Industry Application: RecreationProduct Application: Sports EquipmentDistinct Features: Pigmentable, Low Cost, Good Weatherability, High Molding EfficiencyInformation provided by Applied Composites .. |
|||
Tensile Strength, Ultimate | 48.3 MPa | 7000 psi | ASTM D638 |
Applied Composites 8092 Polyester SMC Industry Application: ConstructionProduct Application: Building ProductsDistinct Features: Pigmentable, High Molding Efficiency, Low Thermal ExpansionInformation provided by Applied Composites Corpo.. |
|||
Tensile Strength, Ultimate | 48.3 - 58.6 MPa | 7000 - 8500 psi | |
Bulk Molding Compounds BMC 1605 Low Shrink, Medium Strength BMC 1605 is an excellent low-cost HB material with low shrink and medium strength. Has excellent surface finish and gloss. Can be injection, compression or transfer molded. UL® recognized. This mat.. |
|||
Tensile Strength, Ultimate | 48.3 - 62.1 MPa | 7000 - 9000 psi | |
Bulk Molding Compounds BMC 620X Mineral Filled, Glass Fiber Reinforced Polyester Compound BMC 620X molding compound is a mineral filled, glass fiber-reinforced polyester compound suitable for compression, transfer and stuffer injection molding. It is a high impact material produced in ex.. |
|||
Tensile Strength, Ultimate | 48.3 - 62.1 MPa | 7000 - 9000 psi | |
Bulk Molding Compounds BMC 850 Corrosion Resistant, Flame Retardant Molding Compound BMC 850 is a high strength, corrosion resistant and flame retardant molding compound. As with all other BMCI compounds, this Series can be supplied in logs, slugs or bulk form.Typical applications a.. |
|||
Tensile Strength, Ultimate | 48.3 - 68.9 MPa | 7000 - 10000 psi | |
Bulk Molding Compounds BMC 5209-12940 Mineral Filled, Glass Reinforced Polyester BMC 5209-12940 molding compound is a mineral filled, glass fiber-reinforced polyester compound suitable for compression, transfer and stuffer injection molding. It is a high impact material produced.. |
|||
Tensile Strength, Ultimate | 48.3 - 62.1 MPa | 7000 - 9000 psi | |
Bulk Molding Compounds BMC 6605A Polyester Molding Compound |
|||
Tensile Strength, Ultimate | 48.3 - 62.1 MPa | 7000 - 9000 psi | |
Bulk Molding Compounds BMC 8005 Polyester Molding Compound |
|||
Tensile Strength, Ultimate | 48.3 - 62.1 MPa | 7000 - 9000 psi | |
Bulk Molding Compounds BMC 851 Corrosion Resistant, Flame Retardant Molding Compound BMC 851is a high strength, corrosion resistant and flame retardant molding compound. As with all other BMCI compounds, this Series can be supplied in logs, slugs or bulk form.Typical applications ar.. |
|||
Tensile Strength, Ultimate | 48.3 MPa | 7000 psi | TM R050-36 |
Resinlab® EP11HTFS Gray Filled Epoxy Adhesive Resinlab™ EP11HTFS Gray is a two part filled epoxy adhesive designed for bonding metals and plastics. It cures at room temperature to a tough, semi-rigid material. It has good wetting to most surfa.. |