Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 480 - 590 MPa
69600 - 85600 psi
Materion Beryllium Copper Alloy 10 Plate & Rolled Bar; H (TD04) Temper; up to 76 mm Thickness (UNS C17500)
Treatment required for max strength: as suppliedTabulated properties apply to products after age hardening. Information supplied by Brush Wellman.Brush Engineered Materials Inc. changed its name to..
Tensile Strength, Ultimate >= 480 MPa
>= 69600 psi
MetalTek MTEK 23-35WCo Heat Resistant Stainless Steel
Information provided by MetalTekCast ASTM A297 MOD.
Tensile Strength, Ultimate 480 - 655 MPa
69600 - 95000 psi
MetalTek MTEK WC 9 Cast UNS J42045 Alloy Steel
Information provided by MetalTek
Tensile Strength, Ultimate 480 - 655 MPa
69600 - 95000 psi
MetalTek WC 6 Cast UNS J24054 Alloy Steel
General structural use.Applications: Cylinders, rolls, hollow shafts.Information provided by MetalTek
Tensile Strength, Ultimate 480 - 655 MPa
69600 - 95000 psi
MetalTek WCB UNS J13345 Cast Alloy Steel
General structural use.Applications: Cylinders, rolls, hollow shafts.Information provided by MetalTek
Tensile Strength, Ultimate >= 480 MPa
>= 69600 psi
H.C. Starck WCu 90/10 Tungsten-Copper Composite Material
Description of Product: Tungsten-copper composite materials are produced by copper infiltration of porous sintered tungsten. They are available with different copper contents (10 - 30 %). A therm..
Tensile Strength, Ultimate 480 - 680 MPa
69600 - 98600 psi
Materion Brush 1915â„¢ Heat Treated Temper Rod, 0.375" - 0.500"
Information supplied by Brush Wellman Engineered Materials.Treatment required for max strength: 3.5 hrs @ 370°C or Mill HardenedBrush 1915™ is Brush Wellman's new heat-treatable leaded coppe..
Tensile Strength, Ultimate 480 - 655 MPa
69600 - 95000 psi
MetalTek WCC Cast 105-85 Alloy Steel
General structural use.Applications: Cylinders, rolls, hollow shafts.Information provided by MetalTek
Tensile Strength, Ultimate 480 MPa

@Temperature 550 °C
69600 psi

@Temperature 1020 °F
Annealed prior to test
Special Metals INCOLOY® Alloy 330
A nickel-iron-chromium alloy with an addition of silicon for enhanced oxidation resistance. It has good strength at high temperatures and excellent resistance to carburizing and oxidizing atmospher..
Tensile Strength, Ultimate 480 - 540 MPa
69600 - 78300 psi
SSAB Tunnplat Aluzink 380A YP High-strength Metal-coated Steel
High-strength Metal-coated SteelComments: Aluzink YP - HSLA steel (aluminum-zinc coated sheet). Property values are for thicknesses 0.4 - 2.0 mm. Iron content is approximate - exact composition is ..
Tensile Strength, Ultimate 480 - 620 MPa
69600 - 89900 psi
SSAB Tunnplat Domex® 420MC HSLA Steel
HSLA SteelCharacteristics: Some thicknesses of these steel grades are available with a maximum of 0.03% Si for thin Zn coating. If the material is to be hot-dip galvanized and steel with a maximum ..
Tensile Strength, Ultimate >= 480 MPa
>= 69600 psi
SSAB Tunnplat Domex® 420YP Cold-forming Steel, HSLA
Cold-forming Steel, HSLACharacteristics: Domex® is the brand name of hot rolled products from SSAB Tunnplat. Domex® cold-forming steels are modern structural steels. General use of Domex®..
Tensile Strength, Ultimate 480 - 550 MPa
69600 - 79800 psi
Wire
CLAL-MSX ARCAP Anticorrosion AP1 H12 1/2 hard, Drawn Copper Alloy
Description: The AP1D grade has been developed especially for being machined by lathe. The very good machineability of the AP1D grade may be summerised by: cutting speed up to 150 m/minute (accordin..
Tensile Strength, Ultimate 480 - 650 MPa
69600 - 94300 psi
CLAL-MSX NICLAL 1800 H12 1/2 Hard Copper Alloy, Free Cutting Nickel-Silver
Main Characteristics: Good corrosion resistanceHigh mechanical propertiesTypical Applications:Parts subject to high stressHigh quality fastenersInformation provided by CLAL-MSX
Tensile Strength, Ultimate >= 480 MPa
>= 69600 psi
AK Steel ASTM A 1011, Class 2 Formable, Grade 55F Hot Rolled Carbon Steel, Medium/High Strength Low Alloy Steel (HSLA-F)
Not listed in the ASTM.Information provided by AK Steel
Tensile Strength, Ultimate >= 480 MPa
>= 69600 psi
AK Steel ASTM A 1011, Grade 55 Hot Rolled Carbon Steel, Structural Steel (SS)
Information provided by AK Steel
Tensile Strength, Ultimate >= 480 MPa
>= 69600 psi
AK Steel ASTM A 607 Class 1 Formable, Grade 55K Hot Rolled Carbon Steel, Medium/High Strength Low Alloy (HSLA)
ASTM A 607 is for Hot Rolled and Cold Rolled grades. AK Steel produces Type 1 (columbium bearing only), Class 1 has limits placed on C, Mn, P and S with a 15 ksi difference between the minimum spec..
Tensile Strength, Ultimate >= 480 MPa
>= 69600 psi
AK Steel ASTM A 715 Class 2 Formable, Grade 60F Hot Rolled Carbon Steel, Medium/High Strength Low Alloy (HSLA)
ASTM A 715 is for Hot Rolled and Cold Rolled grades. AK Steel produces Type 1 (columbium bearing only), Class 2 limits only C and has a 10 ksi difference between the minimum specified YS and UTS. ..
Tensile Strength, Ultimate 480 MPa

@Temperature 371 °C
69600 psi

@Temperature 700 °F
Plate
AK Steel NITRONIC® 30 Austenitic Stainless Steel
AK Steel NITRONIC 30 Stainless Steel offers significantly higher strength than Type 304 and potential for applications requiring good resistance to aqueous and atmospheric corrosion resistance combi..
Tensile Strength, Ultimate >= 480 MPa
>= 69600 psi
AK Steel ASTM A 1011, Class 1 Formable, Grade 55K Hot Rolled Carbon Steel, Medium/High Strength Low Alloy Steel (HSLA)
Information provided by AK Steel
Tensile Strength, Ultimate >= 480 MPa
>= 69600 psi
AK Steel ASTM A 1011, Class 2 Formable, Grade 60K Hot Rolled Carbon Steel, Medium/High Strength Low Alloy Steel (HSLA)
Information provided by AK Steel
Tensile Strength, Ultimate >= 480 MPa
>= 69600 psi
AK Steel SAE J1392, Grade 55F Hot Rolled Carbon Steel, Medium/High Strength Low Alloy (HSLA)
AK Steel Formable Grade - F indicates inclusion controlled low alloy.Information provided by AK Steel
Tensile Strength, Ultimate 480 MPa
69600 psi
As Cast
AFE Technologies Cronite 37Ni/18Cr/Nb No. HR32
High temperature nickel alloy castings. Applications include heat treatment and handling products, furnace products, tubes, power generation, and petrochemical industries.Information provided by AF..
Tensile Strength, Ultimate 480 MPa

@Temperature 870 °C
69600 psi

@Temperature 1600 °F
Haynes 242® alloy, hot rolled plate, annealed and aged
Age-hardenable, high ductility in the aged condition, lower thermal expansion than most alloys, very good oxidation resistance up to 815°C, excellent low cycle fatigue properties, very good thermal..
Tensile Strength, Ultimate 480 MPa

@Temperature 704 °C
69600 psi

@Temperature 1300 °F
Haynes Hastelloy® N, 1.6 mm sheet, heat treated at 1175°C, rapid air cooled
Applications include containers for molten fluoride salts. Good oxidation resistance to hot fluoride salts at 705-870°C (1300-1600°F), good oxidation resistance in air.Data provided by the manufac..
Copyright © lookpolymers.com All Rights Reserved