Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 33.0 MPa | 4790 psi | ASTM D638-61T |
Rotuba 855, Slow Burning Ethyl Cellulose Data provided by the manufacturer. |
|||
Tensile Strength, Ultimate | 33.0 MPa | 4790 psi | ASTM D638-61T |
Rotuba 890 Ethyl Cellulose Data provided by the manufacturer. |
|||
Tensile Strength, Ultimate | 33.0 MPa | 4790 psi | 4.0 mm thick, 10.0 mm wide molded rod; ISO 527 |
Premix Thermoplastics PRE-ELEC® ESD 7200 PRE-ELEC ESD 7200 is a static dissipative thermoplastic compound based on PC/ABS. The dissipative property is permanent and built into the polymer chain. PRE-ELEC ESD 7200 has been developed for inj.. |
|||
Tensile Strength, Ultimate | 33.0 MPa | 4790 psi | ASTM D638 |
NOVA Chemicals Novapol® HE-D250A HDPE Extrusion Resin
(discontinued **) Features: Excellent ESCR and toughness, good processability.Applications: conduit, corrugated pipe.Data provided by the manufacturer. |
|||
Tensile Strength, Ultimate | 33.0 MPa | 4790 psi | ASTM D638 Type IV |
Chevron Phillips Marlex® HHM TR-418N/M358Y Natural medium density ethylene hexene copolymer/yellow concrete
( Benefits: environmentally-friendly pigment system, yellow color for easy identification, outstanding pipe rind ESCR, UV stabilizer in natural resin, concentrate base resinCharacteristics: Pipe Ring .. |
|||
Tensile Strength, Ultimate | 33.0 MPa | 4790 psi | ASTM D638 |
Kleerdex Kydex® GND Acrylic/PVC Thermoplastic Sheet
(discontinued **) Conductive fire-rated sheetApplications: Electronic equipment where protection against electro-static damage is essential, conductive floor mats, IC containers like trays, storage bins, boxes, chip .. |
|||
Tensile Strength, Ultimate | 33.0 - 39.0 MPa | 4790 - 5660 psi | Average value: 37.0 MPa Grade Count:3 |
Overview of materials for Medium Density Polyethylene (MDPE), Film Grade This property data is a summary of similar materials in the MatWeb database for the category "Medium Density Polyethylene (MDPE), Film Grade". Each property range of values reported is minimum and m.. |
|||
Tensile Strength, Ultimate | 33.0 MPa | 4790 psi | ASTM D638 |
ExxonMobil Iotek® 8000 Sodium Ionomer Molding/Extrusion Resin
(discontinued **) Data provided by the manufacturer, Exxon Chemical.A sodium ionomer with excellent abrasion resistance, impact strength, hardness and tensile strength. IOTEK ionomers provide superb low temperature .. |
|||
Tensile Strength, Ultimate | 33.0 MPa @Temperature 1204 °C |
4790 psi @Temperature 2199 °F |
|
Haynes HR-160® alloy, solution annealed sheet Outstanding resistance to various forms of high-temperature corrosion attack, excellent resistance to sulfidation and chloride attack in both reducing and oxidizing atmospheres. Excellent forming an.. |
|||
Tensile Strength, Ultimate | 33.0 MPa @Temperature 1204 °C |
4790 psi @Temperature 2199 °F |
|
Haynes Multimet® alloy, 1.6 mm thick sheet, 1177°C heat treatment, rapid air cooled Recommended for use in applications involving high stress at temperatures up to 816°C (1500°F), and moderate stresses up to 1093°C (2000°F). Excellent oxidation resistance, good ductilit.. |
|||
Tensile Strength, Ultimate | 33.0 MPa @Temperature -20.0 °C |
4790 psi @Temperature -4.00 °F |
Type IV, crosshead speed 2 in/min, at -20°C; ASTM D638 |
DuPont Elvax® 260 Ethylene-Vinyl Acetate Copolymer Resin Elvax resins offer a unique combination of processing and performance characteristics. They provide outstanding toughness and resilience and maintain flexibility over a broad temperature range with.. |
|||
Tensile Strength, Ultimate | 33.0 MPa @Temperature -20.0 °C |
4790 psi @Temperature -4.00 °F |
Type IV, crosshead speed 2 in/min, at -20°C; ASTM D638 |
DuPont Elvax® 460 Ethylene-Vinyl Acetate Copolymer Resin Elvax resins offer a unique combination of processing and performance characteristics. They provide outstanding toughness and resilience and maintain flexibility over a broad temperature range with.. |
|||
Tensile Strength, Ultimate | 33.0 MPa | 4790 psi | DIN 53504 |
Lubrizol ESTANE® ETE55DT3 Ester Based Thermoplastic Polyurethane (European Grade) Description: Estane® thermoplastic polyurethanes (TPUs) include elastomeric materials that bridge the gap between flexible rubber and rigid plastics. These materials offer toughness and durability .. |
|||
Tensile Strength, Ultimate | 33.0 MPa | 4790 psi | ISO 527-1, 2 |
Polyplastics Duracon® SF-20 Acetal Co-polymer (POM), High impact, Flexible DURACON® is a crystalline thermoplastic acetal copolymer. The primary raw material trioxane, a trimer of formaldehyde.The thermoplastic adopts a copolymer structure in which polyoxymethylene (-C-O).. |
|||
Tensile Strength, Ultimate | 33.0 MPa | 4790 psi | ISO 527-1, 2 |
Polyplastics Duranex® CE7300 Polybutylene Terephthalate (PBT), Higher impact resistant DURANEX® is a crystalline thermoplastic based on polybutylene terephthalate (PBT) that can be readily strengthened, modified, or otherwise performance enhanced through the addition of glass fibers .. |
|||
Tensile Strength, Ultimate | 33.0 MPa | 4790 psi | DIN 53504 |
Lubrizol ESTANE® 58360 Ester Based Thermoplastic Polyurethane (European Grade) Description: Estane® thermoplastic polyurethanes (TPUs) include elastomeric materials that bridge the gap between flexible rubber and rigid plastics. These materials offer toughness and durability .. |
|||
Tensile Strength, Ultimate | 33.0 MPa | 4790 psi | ASTM D638/D412 |
Covestro Baydur® 726 IBS Polyurethane Structural Foam RIM, Density 55 pcf, MDI-based 2-Component Liquid System 0.25 in. thickness. IBS = Interactive Blowing System RIM = Reaction Injection MoldingInformation provided by Bayer Corporation, Polyurethanes DivisionAs of 1 September 2015, Bayer MaterialScience .. |
|||
Tensile Strength, Ultimate | 33.0 MPa | 4790 psi | ASTM D638 |
DuPont™ Surlyn® 8940 Ionomer Resin, Sodium Surlyn® 8940 thermoplastic resin is an advanced ethylene/methacrylic acid (E/MAA) copolymer, in which the MAA acid groups have been partially neutralized with sodium ions. The amount of MAA and neu.. |
|||
Tensile Strength, Ultimate | 33.0 MPa | 4790 psi | Z; ASTM D638 |
ALM PA-640-GSL Filled Nylon 12 Prototyping Polymer This carbon fiber/glass sphere filled composite is an easy to process, extremely light weight filled PA 12 material.Improved dimensional stability, recyclability, and increased stiffness.Good Z dire.. |
|||
Tensile Strength, Ultimate | 33.0 MPa @Temperature 871 °C |
4790 psi @Temperature 1600 °F |
|
ATI Allegheny Ludlum AL 453™ Stainless Steel Single phase iron-chromium ferritic stainless steel alloy. Should be annealed between 1450 and 1600°F and quickly cooled. Information provided by Allegheny Ludlum |
|||
Tensile Strength, Ultimate | 33.0 MPa | 4790 psi | ASTM D638 |
A. Schulman ComAlloy Comtuf® 608 Nylon 6/12, Impact Modified Data provided by the manufacturer, ComAlloy International Company. Superior toughness and impact resistance characterize Comtuf® materialsThe ComAlloy product line has been integrated into the A Sc.. |
|||
Tensile Strength, Ultimate | 33.0 MPa | 4790 psi | ASTM D412 |
BASF Elastollan® M88A55 Polyester Type Polyurethane Elastomer The Elastollan M Series of products listed are part of a new series of polyester-based thermoplastic polyurethanes (TPU). They are specifically formulated for fast cycling in Injection Molding appl.. |
|||
Tensile Strength, Ultimate | 33.0 MPa | 4790 psi | ASTM D638 |
Solvay Specialty Polymers Algoflon® A.27 PTFE (Polytetrafluoroethylene)
(discontinued **) Data provided by the manufacturer.Type IV.G.2 (except elongation at break) Classification. Suspension polymer powder grade recommended for compression molding and extrusion. PTFE possesses high iner.. |
|||
Tensile Strength, Ultimate | 33.0 MPa | 4790 psi | ISO 527 |
LATI LARTON CE/60 60% Special Mineral Filled Polyphenylene sulfide (PPS)
(Unverified Data**) Description: Larton thermoplastics are polyphenylene sulfide (PPS) products. They are distinguished by a group of very interesting properties combined with easy moldability. Larton parts feature: ex.. |
|||
Tensile Strength, Ultimate | 33.0 MPa | 4790 psi | ASTM D412 |
BASF Elastollan® 1185A Polyether Type Polyurethane Elastomer Processed by extrusion or injection molding. Elastollan ® 1100 series products are FDA Sec. 177.2600 compliant. Elastollan 1100 series of products are polyether-based thermoplastic polyurethanes... |
|||
Tensile Strength, Ultimate | 33.0 MPa | 4790 psi | ASTM D412 |
BASF Elastollan® M88A15 Polyester Type Polyurethane Elastomer The Elastollan M Series of products listed are part of a new series of polyester-based thermoplastic polyurethanes (TPU). They are specifically formulated for fast cycling in Injection Molding appl.. |
|||
Tensile Strength, Ultimate | 33.0 MPa @Temperature 90.0 °C |
4790 psi @Temperature 194 °F |
ISO 527 |
LATI LARIL 13 Light Brown Polyphenylene Oxide (PPOm)
(discontinued **) Description: Laril thermoplastics are polyphenylene oxide (PPOm) products. They exhibit excellent toughness, even at low temperatures, good thermal resistance and dimensional stability are the most .. |
|||
Tensile Strength, Ultimate | 33.0 - 100 MPa | 4790 - 14500 psi | Average value: 47.4 MPa Grade Count:29 |
Overview of materials for Polybutylene Terephthalate (PBT), PTFE Filled This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), PTFE Filled". Each property range of values reported is minimum and ma.. |
|||
Tensile Strength, Ultimate | 33.0 - 50.0 MPa @Temperature 60.0 - 120 °C |
4790 - 7250 psi @Temperature 140 - 248 °F |
Average value: 41.0 MPa Grade Count:1 |
Overview of materials for Nylon 6, MoS2 Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, MoS2 Filled". Each property range of values reported is minimum and maximum values of appropria.. |
|||
Tensile Strength, Ultimate | 33.0 MPa | 4790 psi | DIN 53504 |
Lubrizol ESTANE® 54620 Ester Based Thermoplastic Polyurethane (European Grade) Description: Estane® thermoplastic polyurethanes (TPUs) include elastomeric materials that bridge the gap between flexible rubber and rigid plastics. These materials offer toughness and durability .. |