Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 14.0 MPa | 2030 psi | |
3M Dyneon™ Fluorel™ FC-2110Q Fluoroelastomer VF2 + HFP Dipolymer
(discontinued **) Data provided by the manufacturer, Dyneon LLC.Incorporated cure polymer, 65.9%F in polymer with 22% Medium Thermal Carbon Black (N990), 2% MgO, and 4% Ca(OH)2. Excellent processability. Viscosity .. |
|||
Tensile Strength, Ultimate | 14.0 MPa | 2030 psi | |
3M Dyneon™ Fluorel™ FC-2152 Fluoroelastomer VF2 + HFP Dipolymer
(discontinued **) Data provided by the manufacturer, Dyneon LLC.Incorporated cure polymer, 65.9%F in polymer with 22% Medium Thermal Carbon Black (N990), 2% MgO, and 4% Ca(OH)2. Improved hot tear over FC-2176. Sugg.. |
|||
Tensile Strength, Ultimate | 14.0 MPa | 2030 psi | ASTM Data |
Americas Styrenics Styron® 482 High Impact Polystyrene
(discontinued **) STYRON® 482 high impact polystyrene resin is a high flow resin typically used in toys. When used unmodified for the manufacture of food contact articles STYRON 482 complies with the US Food, Drug a.. |
|||
Tensile Strength, Ultimate | 14.0 MPa | 2030 psi | ASTM D638 |
Global D-2024 Low Density Polyethylene, Film Extrusion Grade
(discontinued **) Description-transparency, high toughness, flexibility, high impact strength, good chemical resistanceApplications-bagsMeets FDA requirements as listed in food additives regulation 21 CFR 117.1520 fo.. |
|||
Tensile Strength, Ultimate | 14.0 MPa | 2030 psi | ASTM D638 |
Huntsman PE1031 Film Extrusion Polyethylene
(discontinued **) Homopolymer, and FDA compliant.Features: Superior strength, good machinability, and heat seal characteristics.Applications: Film extrusion: clarity packaging, frozen food, produce bags, shrink, bund.. |
|||
Tensile Strength, Ultimate | 14.0 MPa | 2030 psi | ASTM D638 |
Chevron Phillips HiD® 9706 HDPE Injection Molding Resin
(discontinued **) Resin Type: linear homopolymerCharacteristics: moderate flow, good impact strength, excellent stiffness, good ESCR, moderate shrinkage resistanceApplications: crates and totes, structural foamInform.. |
|||
Tensile Strength, Ultimate | 14.0 MPa | 2030 psi | ASTM D638 |
Huntsman PE 1402 EVA Film Extrusion
(discontinued **) 4% Vinyl Acetate EVA copolymer and FDA compliantFeatures: Excellent balance of optical and strength, toughness and flexibility at low temperatures, and good heat seal characteristic.Applications: Fi.. |
|||
Tensile Strength, Ultimate | 14.0 - 26.0 MPa | 2030 - 3770 psi | Average value: 18.9 MPa Grade Count:11 |
Overview of materials for Polypropylene, Mineral Reinforced, Impact Modified This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Mineral Reinforced, Impact Modified". Each property range of values reported is minimum a.. |
|||
Tensile Strength, Ultimate | 14.0 - 250 MPa @Temperature -40.0 - 250 °C |
2030 - 36300 psi @Temperature -40.0 - 482 °F |
Average value: 83.4 MPa Grade Count:3 |
Overview of materials for Liquid Crystal Polymer (LCP), 30% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Liquid Crystal Polymer (LCP), 30% Glass Fiber Filled". Specific grades with glass content between 25% an.. |
|||
Tensile Strength, Ultimate | 14.0 - 250 MPa @Thickness 0.800 - 3.17 mm |
2030 - 36300 psi @Thickness 0.0315 - 0.125 in |
Average value: 83.4 MPa Grade Count:3 |
Overview of materials for Liquid Crystal Polymer (LCP), 30% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Liquid Crystal Polymer (LCP), 30% Glass Fiber Filled". Specific grades with glass content between 25% an.. |
|||
Tensile Strength, Ultimate | 14.0 MPa | 2030 psi | IV, 2 in/min; ASTM D638 |
LyondellBasell Sequel® 1718 Engineered Polyolefin Data provided by Solvay Engineered Polymers.An engineered polyolefin designed for exterior painted automotive applications requiring dimensional stability over a broad temperature range. This mater.. |
|||
Tensile Strength, Ultimate | 14.0 MPa | 2030 psi | ASTM D638 |
LyondellBasell Astryn SZ021-2 Polypropylene Copolymer, 20% Talc Key Features: medium melt flow, medium modulus, mineral-filled, utility grade polypropylene copolymer, good impact and stiffness balance, versatileApplications: inner door panels and seat supportsDe.. |
|||
Tensile Strength, Ultimate | 14.0 MPa | 2030 psi | ISO R527-1 |
LyondellBasell Hifaxâ„¢ BB222GC Thermoplastic Olefin Resin Key Features: medium melt flow, very high modulus, UV-stabilized thermoplastic elastomeric olefin resin, excellent impact and stiffness balance, excellent weatherability, high stiffness, good dimens.. |
|||
Tensile Strength, Ultimate | 14.0 MPa | 2030 psi | DIN 53504 |
Lubrizol ESTANE® T4086 Ester Based Thermoplastic Polyurethane (European Grade) Description: Estane® thermoplastic polyurethanes (TPUs) include elastomeric materials that bridge the gap between flexible rubber and rigid plastics. These materials offer toughness and durability .. |
|||
Tensile Strength, Ultimate | 14.0 MPa | 2030 psi | Type IV, crosshead speed 2 in/min; ASTM D638 |
DuPont Elvax® 260 Ethylene-Vinyl Acetate Copolymer Resin Elvax resins offer a unique combination of processing and performance characteristics. They provide outstanding toughness and resilience and maintain flexibility over a broad temperature range with.. |
|||
Tensile Strength, Ultimate | 14.0 MPa | 2030 psi | butt tensile strength per ASTM D426 on brass |
Von Roll Isola IMI E-Solder® 3021 Electrically Conductive Adhesive Data provided by Von Roll Isola USA.E-SOLDER® epoxy based resin systems can be used at room temperature on heat sensitive materials, can bond dissimilar materials, and do not have flux or residue t.. |
|||
Tensile Strength, Ultimate | 14.0 MPa | 2030 psi | ASTM D638 |
Toyobo Pelprene™ P-150M Polyester TPE Key Feature: Pelprene P typePelprene™ can be processed into a wide variety of articles from ultra-small precision parts to sheets by injection, extrusion, and blow molding. The 'P' type is a block.. |
|||
Tensile Strength, Ultimate | 14.0 MPa | 2030 psi | ISO 527-1 |
Chengdu Polyster H3030 Thermoplastic Polyether-ester Elastomer (TPEE) Information provided by Chengdu Polyster Co., Ltd. |
|||
Tensile Strength, Ultimate | 14.0 MPa | 2030 psi | ISO 527-1/-2 |
DSM Arnitel® PL381-H TPC-ET Injection Molding |
|||
Tensile Strength, Ultimate | 14.0 MPa | 2030 psi | |
BASF Lucalen® A 2710 H Ethylene/Acrylate Copolymer Product with properties which are typical of flexible PVC and of low density polyethylene. Suitable for flexible pipes, profiles and seals.Data was collected by ISO methods and provided by BASF. |
|||
Tensile Strength, Ultimate | 14.0 MPa | 2030 psi | ASTM D638 |
Huntsman PE1061 Film Extrusion Polyethylene
(discontinued **) Homopolymer and FDA compliant.Features: Exceptional strength, good machinability and heat seal characteristics.Applications: Film extrusion: high clarity packaging, frozen food, produce bags, shrink.. |
|||
Tensile Strength, Ultimate | 14.0 MPa | 2030 psi | ASTM D638 |
Huntsman PE6010 Blow Molding Polyethylene
(discontinued **) Homopolymer, Drug Master File listed product, complies with USP Classification VI, and FDA compliant.Features: Meets exacting requirements of blow molded containers and processes well with parison s.. |
|||
Tensile Strength, Ultimate | 14.0 MPa | 2030 psi | ASTM D638 |
Huntsman PE7011 Profile Extrusion Polyethylene
(discontinued **) Homopolymer and FDA compliant.Features: Excellent strength, good machinability, and foaming characteristics.Applications: Extrusion: profile extrusion.FDA Notes: Conforms to FDA regulation 21 CFR 17.. |
|||
Tensile Strength, Ultimate | 14.0 - 280 MPa | 2030 - 40600 psi | Average value: 237 MPa Grade Count:18 |
Overview of materials for Polyvinyl Dichloride (PVDC) This property data is a summary of similar materials in the MatWeb database for the category "Polyvinyl Dichloride (PVDC)". Each property range of values reported is minimum and maximum values of ap.. |
|||
Tensile Strength, Ultimate | 14.0 MPa | 2030 psi | ASTM D638 |
Huntsman PE1203 EVA Film Extrusion
(discontinued **) 2% Vinyl Acetate EVA copolymer and FDA compliantFeatures: High clarity film with good stiffness and low temperature toughness.Applications: Film extrusion: food packaging, general purpose packaging .. |
|||
Tensile Strength, Ultimate | 14.0 MPa | 2030 psi | ASTM D638 |
Huntsman PE 1253 EVA Film Extrusion
(discontinued **) 2.5% Vinyl Acetate EVA copolymer and FDA compliantFeatures: Excellent balance of optical and strength, good heat seal characteristics.Applications: Film extrusion: general purpose packaging where to.. |
|||
Tensile Strength, Ultimate | 14.0 MPa | 2030 psi | ASTM D412-80 |
DuPont Performance Polymers Hypalon® 30 Chlorosulfonated Polyethylene Rubber, Mineral Filled Compound
(discon Mineral filled compound with 100 parts Hypalon; 80 parts hard clay; 4 parts magnesia; 30 parts aromatic process oil; 3 parts pentaerythritol; and 2 parts Tetrone® A rubber accelerator (from DuPont .. |
|||
Tensile Strength, Ultimate | 14.0 MPa | 2030 psi | ASTM D638 |
Huntsman PE1353 EVA Film Extrusion
(discontinued **) 3.5% Vinyl Acetate EVA copolymer and FDA compliantFeatures: Excellent balance of optical and strength, toughness and flexibility at low temperatures, and good heat seal characteristic.Applications: .. |