Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 35.0 - 250 MPa

@Temperature 60.0 - 275 °C
5080 - 36300 psi

@Temperature 140 - 527 °F
Average value: 134 MPa Grade Count:14
Overview of materials for Polyetheretherketone, Carbon Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polyetheretherketone, Carbon Fiber Filled". Each property range of values reported is minimum and maximu..
Tensile Strength, Ultimate 14.0 - 250 MPa

@Temperature -40.0 - 250 °C
2030 - 36300 psi

@Temperature -40.0 - 482 °F
Average value: 83.4 MPa Grade Count:3
Overview of materials for Liquid Crystal Polymer (LCP), 30% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Liquid Crystal Polymer (LCP), 30% Glass Fiber Filled". Specific grades with glass content between 25% an..
Tensile Strength, Ultimate 14.0 - 250 MPa

@Thickness 0.800 - 3.17 mm
2030 - 36300 psi

@Thickness 0.0315 - 0.125 in
Average value: 83.4 MPa Grade Count:3
Overview of materials for Liquid Crystal Polymer (LCP), 30% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Liquid Crystal Polymer (LCP), 30% Glass Fiber Filled". Specific grades with glass content between 25% an..
Tensile Strength, Ultimate 68.0 - 250 MPa
9860 - 36300 psi
Average value: 143 MPa Grade Count:110
Overview of materials for Nylon 66, Glass Fiber/PTFE Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Glass Fiber/PTFE Filled". Each property range of values reported is minimum and maximum values..
Tensile Strength, Ultimate 60.0 - 250 MPa
8700 - 36300 psi
Average value: 131 MPa Grade Count:27
Overview of materials for Nylon 12, Carbon Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 12, Carbon Fiber Filled". Each property range of values reported is minimum and maximum values of ..
Tensile Strength, Ultimate 230 - 250 MPa
33400 - 36300 psi
AMT AM-Lite® Die Casting Magnesium Alloy