Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 82.9 MPa | 12000 psi | ASTM D638 |
Plenco 50015 PET, Pellet, Injection Molded, Black
(discontinued **) PLENCO 50015 is an engineering grade glass reinforced polyethylene terephthalate resin designed for increased flexibility and good physical strength. It is UL recognized and available in white, natu.. |
|||
Tensile Strength, Ultimate | 82.7 MPa | 12000 psi | Type 1 - Rigids, 0.2 in/min; ASTM D638 |
PolyOne Lubri-Tech™ AS-15CF/15T Acrylonitrile Butadiene Styrene (ABS), Carbon Fiber Reinforced, PTFE Lubricated
&nb Description/Features:Carbon Fiber ReinforcedPTFE LubricatedPolyOne First ChoiceInformation provided by PolyOne Corporation. |
|||
Tensile Strength, Ultimate | 83.0 - 97.0 MPa | 12000 - 14100 psi | Average value: 90.0 MPa Grade Count:7 |
Overview of materials for Epoxy, Molded, Mineral Filled This property data is a summary of similar materials in the MatWeb database for the category "Epoxy, Molded, Mineral Filled". Each property range of values reported is minimum and maximum values of .. |
|||
Tensile Strength, Ultimate | 83.0 MPa | 12000 psi | |
Cookson Group Plaskon® 3300SGH Mineral Filled Epoxy Molding Compound
(discontinued **) Test specimens were transfer molded and post cured 4 hours at 175°C.Exhibits exceptional reliability, excellent moldability, good release characteristics, low flash and rapid cure. This compound i.. |
|||
Tensile Strength, Ultimate | 83.0 MPa | 12000 psi | ASTM D638 |
Aardvark Polymers Aarlon® 2000 Rotational Molding Resin, DAM Aarlon® 2000 PA 6/6 is a high performance nylon for rotational molding applications. Aarlon® 2000 offers high heat capabilities with exceptional mechanical properties.Information provided by G.. |
|||
Tensile Strength, Ultimate | 83.0 MPa | 12000 psi | |
Haysite 46000 Polyester SMC, 30% Glass Reinforced The 46000 series sheet molding compound is designed for "automotive type" applications requiring good mechanical properties and low shrink characteristics. |
|||
Tensile Strength, Ultimate | 83.0 MPa | 12000 psi | DIN 53455; ASTM D638 |
Kolon Kopa® KN138R Nylon 6 Resin KOPA is widely used in the automobile and industrial parts.General KOPA N-6 Features: Good mechanical properties, Extreme toughness, Outstanding self-lubrication and abrasion resistance, Excellent c.. |
|||
Tensile Strength, Ultimate | 82.7 MPa | 12000 psi | ASTM Data |
Styron Pulse® 759 ABS + Polycarbonate, 15% Glass Reinforced PULSE® 759 Engineering resin is a 15% glass reinforced resin designed to provide excellent processability, high heat resistance, and practical toughness. PULSE 759 Engineering resin has been used.. |
|||
Tensile Strength, Ultimate | 83.0 MPa | 12000 psi | |
Cosmic Plastics E487 lass Filled Epoxy Molding Compound, Electrical Grade Data provided by the manufacturer. |
|||
Tensile Strength, Ultimate | 83.0 MPa | 12000 psi | |
Cosmic Plastics E4920 Mineral Filled Epoxy Molding Compound, Encapsulated Grade Data provided by the manufacturer. |
|||
Tensile Strength, Ultimate | 83.0 MPa | 12000 psi | ATSM D638 |
Ashley Polymers Ashlene® 520MS/520SMS Nylon 66, MoS2 Filled A general purpose Molybdenum-disulfide filled nylon resin.Data provided by the manufacturer |
|||
Tensile Strength, Ultimate | 83.0 MPa | 12000 psi | ATSM D638 |
Ashley Polymers Ashlene® 62M Nylon 66, 40% Mineral reinforced A 40% mineral reinforced Nylon 66 resin modified for reduced shrinkage.Data provided by the manufacturer |
|||
Tensile Strength, Ultimate | 83.0 MPa | 12000 psi | Static |
Channel Industries 5800 Lead Zirconate Titanate Piezoelectric Characterized by high coupling factors and high piezoelectric and dielectric constants over extended temperature ranges and stress amplitudes, lead zirconate titanates are the most extensively used .. |
|||
Tensile Strength, Ultimate | 83.0 MPa | 12000 psi | ASTM D638 |
A. Schulman ComAlloy Hiloy® 431 Glass Reinforced, PBT Alloy Data provided by the manufacturer, ComAlloy International Company.15% Glass Reinforced.The ComAlloy product line has been integrated into the A Schulman product line. |
|||
Tensile Strength, Ultimate | 83.0 MPa | 12000 psi | ATSM D638 |
Ashley Polymers Ashlene® 830 Nylon 6 Basic Nylon 6, medium viscosity, unlubricated.Data provided by the manufacturer |
|||
Tensile Strength, Ultimate | 83.0 MPa | 12000 psi | Static |
Channel Industries 5804 Lead Zirconate Titanate Piezoelectric Navy Type IIICharacterized by high coupling factors and high piezoelectric and dielectric constants over extended temperature ranges and stress amplitudes, lead zirconate titanates are the most exte.. |
|||
Tensile Strength, Ultimate | 82.7 MPa | 12000 psi | Type 1 - Rigids, 0.2 in/min; ASTM D638 |
PolyOne Lubri-Tech™ PI-000/15T Polyetherimide (PEI), PTFE Lubricated
(discontinued **) Description/Features:PTFE LubricatedPolyOne First ChoiceInformation provided by PolyOne Corporation. |