Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 73.8 MPa | 10700 psi | ASTM D638 |
Nylene® Norpex® AX10GF , 10% Glass Reinforced Polyphenylene Ether Description: Norpex® AX10GF is a 10% glass fiber reinforced Polyphenylene Ether. Information provided by Custom Resins. ALM, Nylene Canada, and Custom Resins are all operting companies of Polymeric.. |
|||
Tensile Strength, Ultimate | 73.8 MPa | 10700 psi | ASTM D638 |
Nylene® Norpex® AX20MR , 20% Mineral Reinforced Polyphenylene Ether Description: Norpex® AX20MR is a 20% mineral reinforced Polyphenylene Ether. Information provided by Custom Resins. ALM, Nylene Canada, and Custom Resins are all operting companies of Polymeric Res.. |
|||
Tensile Strength, Ultimate | 73.5 MPa | 10700 psi | ISO 527 |
Polikim KESTOIL® Polyamide 6 + Lubricant Kestoil® is a self-lubricated, strong, wear resistant engineering plastic with a low coefficient of friction. Implicit in its nature, it has many properties that no other material has in combinatio.. |
|||
Tensile Strength, Ultimate | 74.0 MPa | 10700 psi | ISO 527-2 |
NOVA Chemicals DYLARK® 480P16 Glass Reinforced Engineering Resin Features:Very high modulus High heat resistance Excellent flow characteristics Excellent adhesion to urethaneApplications:Instrument panel substrates Consoles Cluster housings Interior trimInformati.. |
|||
Tensile Strength, Ultimate | 73.5 MPa | 10700 psi | ISO 527 |
Polikim KESTAMID® GRF Polyamide 6, Graphite Filled Graphite and special lubricants are evenly dispersed in its entirety in this type of Polikim's cast polyamide. The material is dark grey colored. Kestamid®-GRF has a high degree of crystallinity an.. |
|||
Tensile Strength, Ultimate | 73.5 MPa | 10700 psi | ASTM D638 |
Kolon Kocetal® WH702 Reinforced Grade Acetal Copolymer
(discontinued **) Thermal properties: Kocetal has excellent heat stability; heat degradation is little under long term and high temperature application, compared to other POM. Maximum applicable temperature of produ.. |
|||
Tensile Strength, Ultimate | 74.0 MPa | 10700 psi | 10%/min; ASTM D638 |
EVALCA EVAL® F100 Ethylene Vinyl Alcohol Copolymer Resin
(discontinued **) 32 mol % Ethylene.Data provided by EVALCA. Applications: Melt phase forming. EVOH is used in packaging applications because of its outstanding gas barrier properties.EVAL™ is now produced as a pa.. |
|||
Tensile Strength, Ultimate | 73.77 MPa | 10700 psi | |
Abatron AboCast 8-12/Abocure 8-12 Epoxy
(discontinued **) 2-part solvent-free dielectric epoxy casting compound.Processing: 100/13.2 ratio (pbw); Gel time, 100 g (3.5 oz.): 49 minutes; cures in 16 hours at 25°C (77°F); postcure: 2 hours at 100°C (212°F.. |
|||
Tensile Strength, Ultimate | 73.5 MPa | 10700 psi | DIN 53455; ASTM D638 |
Kolon KOPA® KN177N Nylon Extrusion Resin Excellent transparent & flexible copolyamide, typical applications are fishing nets & fishing linesInformation provided by US distributor, API-Kolon. |
|||
Tensile Strength, Ultimate | 74.0 MPa | 10700 psi | ASTM D638 |
Lucky IH-830 Acrylic, Injection Grade Similar to grade EH-910, but with higher flow for injection molding. May be UV stabilized. General Lucky PMMA qualities: Transparent/elegant appearance, high heat and weather resistance, excellent.. |
|||
Tensile Strength, Ultimate | 74.0 MPa @Temperature 1093 °C |
10700 psi @Temperature 1999 °F |
|
Haynes HR-160® alloy, hot rolled and solution annealed plate Outstanding resistance to various forms of high-temperature corrosion attack, excellent resistance to sulfidation and chloride attack in both reducing and oxidizing atmospheres. Excellent forming an.. |
|||
Tensile Strength, Ultimate | 73.5 MPa | 10700 psi | DIN 53455; ASTM D638 |
Kolon KOPA® KN133G8ST Multi Reinforced Nylon 6 KOPA® is a thermoplastic resin with excellent mechanical, thermal and electrical properties and is widely used in automobile and industrial parts.Good mechanical properties, outstanding self-lubr.. |
|||
Tensile Strength, Ultimate | 74.0 MPa | 10700 psi | ASTM D638 |
Lucky CH-910 Acrylic, Coextrusion Grade Coextrusion grade. May be UV stabilized. General Lucky PMMA qualities: Transparent/elegant appearance, high heat and weather resistance, excellent chemical resistance and coloring capability. |
|||
Tensile Strength, Ultimate | 74.0 MPa | 10700 psi | ASTM D638 |
Plenco 1510 Polyester, Pellet, Injection Molded PLENCO 01510 is a mineral filled, pelletized polyester molding compound, which offers an excellent combination of electrical properties and dimensional stability. UL recognized under component file .. |
|||
Tensile Strength, Ultimate | 74.0 MPa | 10700 psi | ASTM D638 |
Plenco 6582 Phenolic, Briquette, Transfer Molded PLENCO 06582 is a rubber modified phenolic molding compound, offering excellent heat resistant properties, along with improved mechanical strength at elevated temperatures. UL recognized under compo.. |
|||
Tensile Strength, Ultimate | 74.0 MPa | 10700 psi | ASTM D638 |
Toyobo Vylopet® EMC317R Glass Reinforced Polyester, Standard Grade Key Feature: UL-94 classApplications: Glossy surface componentsGeneral features of Vylopet® include heat resistance, good mechanical properties, high dielectric strength and tracking resistance, ch.. |
|||
Tensile Strength, Ultimate | 74.0 MPa | 10700 psi | ISO 527-2/1A/5 |
Lubrizol ESTALOC® 59200 Ester-Type, Reinforced Engineering Thermoplastic (European Grade) Description: Estaloc® RETP (Reinforced Engineering Thermoplastic) is a tough, dimensionally stable, abrasion-resistant thermoplastic that withstands demanding environments. Developed as an extensio.. |
|||
Tensile Strength, Ultimate | 74.0 MPa @Temperature 982 °C |
10700 psi @Temperature 1800 °F |
ASTM E8 |
ATI Allegheny Ludlum 309S Austenitic Stainless Steel Characteristics: comparable corrosion resistance, superior resistance to oxidation, and the retention of a larger fraction of room temperature strength than common austenitic alloys. Good creep defo.. |
|||
Tensile Strength, Ultimate | 74.0 MPa | 10700 psi | ASTM D638 |
A. Schulman ComAlloy Hiloy® 104 Polypropylene, Glass Reinforced Data provided by the manufacturer, ComAlloy International Company.40% Glass Reinforced.The ComAlloy product line has been integrated into the A Schulman product line. |
|||
Tensile Strength, Ultimate | 74.0 MPa | 10700 psi | ASTM D638 |
A. Schulman ComAlloy Hiloy® 222 ABS, Glass Reinforced, UL Data provided by the manufacturer, ComAlloy International Company.20% Glass Reinforced.The ComAlloy product line has been integrated into the A Schulman product line. |
|||
Tensile Strength, Ultimate | 74.0 MPa | 10700 psi | ASTM D638 |
A. Schulman ComAlloy Hiloy® 246 SAN, Glass/Mineral Reinforced Data provided by the manufacturer, ComAlloy International Company.30% Glass/Mineral Reinforced.The ComAlloy product line has been integrated into the A Schulman product line. |
|||
Tensile Strength, Ultimate | 74.0 MPa | 10700 psi | ASTM D638 |
A. Schulman ComAlloy Hiloy® 421 Polyester - PBT, Glass/Mineral Reinforced Data provided by the manufacturer, ComAlloy International Company.45% Glass/Mineral Reinforced.The ComAlloy product line has been integrated into the A Schulman product line. |
|||
Tensile Strength, Ultimate | 74.0 MPa | 10700 psi | ASTM D638 |
Cast Nylons Nycast® Nyloil®-MDX Lubricated Nylon, MoS2 Filled NYCAST® NYLOIL® was developed to extend the wear-resistant properties of unlubricated or dry lubricated materials such as MoS2 filled nylons. NYCAST® NYLOIL® will last 5 to 7 times longer than .. |
|||
Tensile Strength, Ultimate | 74.0 MPa | 10700 psi | ATSM D638 |
Ashley Polymers Ashlene® P291WO PPO A reinforced, flame retardant resin with outstanding structural strength. Good appearance and high impact.Data provided by the manufacturer |
|||
Tensile Strength, Ultimate | 74.0 MPa | 10700 psi | ASTM D638 |
Lucky EH-910 Acrylic, Extrusion Grade Highest heat and stress cracking resistance of Lucky PMMA grades. Recommended for extrusion of sheets, pipes, and profiles. Can also be used for injection molding of small parts. May be UV stabil.. |