Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 155 - 280 MPa | 22500 - 40600 psi | Average value: 230 MPa Grade Count:13 |
Overview of materials for Nylon 66/6, 60% Glass Fiber Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66/6, 60% Glass Fiber Reinforced". Specific grades with glass content between 55% and 64% are incl.. |
|||
Tensile Strength, Ultimate | 14.0 - 280 MPa | 2030 - 40600 psi | Average value: 237 MPa Grade Count:18 |
Overview of materials for Polyvinyl Dichloride (PVDC) This property data is a summary of similar materials in the MatWeb database for the category "Polyvinyl Dichloride (PVDC)". Each property range of values reported is minimum and maximum values of ap.. |
|||
Tensile Strength, Ultimate | 117 - 280 MPa | 17000 - 40600 psi | Average value: 151 MPa Grade Count:11 |
Overview of materials for Polypropylene with 60% Glass Fiber Filler This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 60% Glass Fiber Filler". Specific grades with glass content between 55% and 64% are i.. |