Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 27.6 - 145 MPa | 4000 - 21000 psi | Average value: 55.7 MPa Grade Count:33 |
Overview of materials for Polybutylene Terephthalate (PBT), Impact Grade This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Impact Grade". Each property range of values reported is minimum and m.. |
|||
Tensile Strength, Ultimate | 100 - 145 MPa @Temperature 130 - 180 °C |
14500 - 21000 psi @Temperature 266 - 356 °F |
Average value: 84.7 MPa Grade Count:13 |
Overview of materials for Polyphthalamide (PPA) This property data is a summary of similar materials in the MatWeb database for the category "Polyphthalamide". Each property range of values reported is minimum and maximum values of appropriate Ma.. |
|||
Tensile Strength, Ultimate | 100 - 145 MPa @Time 1.80e+7 - 7.20e+7 sec |
14500 - 21000 psi @Time 5000 - 20000 hour |
Average value: 84.7 MPa Grade Count:13 |
Overview of materials for Polyphthalamide (PPA) This property data is a summary of similar materials in the MatWeb database for the category "Polyphthalamide". Each property range of values reported is minimum and maximum values of appropriate Ma.. |
|||
Tensile Strength, Ultimate | 135 - 145 MPa @Temperature 130 - 180 °C |
19600 - 21000 psi @Temperature 266 - 356 °F |
Average value: 107 MPa Grade Count:4 |
Overview of materials for Polyphthalamide (PPA), 50% Glass Fiber Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Polyphthalamide, 50% Glass Fiber Reinforced". Each property range of values reported is minimum and maxi.. |
|||
Tensile Strength, Ultimate | 135 - 145 MPa @Time 1.80e+7 - 7.20e+7 sec |
19600 - 21000 psi @Time 5000 - 20000 hour |
Average value: 107 MPa Grade Count:4 |
Overview of materials for Polyphthalamide (PPA), 50% Glass Fiber Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Polyphthalamide, 50% Glass Fiber Reinforced". Each property range of values reported is minimum and maxi.. |
|||
Tensile Strength, Ultimate | 55.0 - 145 MPa | 7980 - 21000 psi | Average value: 117 MPa Grade Count:71 |
Overview of materials for Polycarbonate, 30% Glass Filled This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, 30% Glass Filled". Specific grades with glass content between 25% and 34% are included. E.. |
|||
Tensile Strength, Ultimate | 60.0 - 145 MPa @Temperature 60.0 - 150 °C |
8700 - 21000 psi @Temperature 140 - 302 °F |
Average value: 108 MPa Grade Count:3 |
Overview of materials for Polyphenylene Sulfide (PPS), Mineral/Glass-Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Sulfide (PPS), Mineral/Glass-Fiber Filled". Each property range of values reported is mini.. |
|||
Tensile Strength, Ultimate | 25.0 - 145 MPa @Temperature -30.0 - 120 °C |
3630 - 21000 psi @Temperature -22.0 - 248 °F |
Average value: 66.1 MPa Grade Count:1 |
Overview of materials for Nylon 6, Glass/Mineral Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Glass/Mineral Reinforced". Each property range of values reported is minimum and maximum values.. |
|||
Tensile Strength, Ultimate | 25.0 - 145 MPa @Strain 1.00 - 10.0 % |
3630 - 21000 psi @Strain 1.00 - 10.0 % |
Average value: 66.1 MPa Grade Count:1 |
Overview of materials for Nylon 6, Glass/Mineral Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Glass/Mineral Reinforced". Each property range of values reported is minimum and maximum values.. |
|||
Tensile Strength, Ultimate | 48.3 - 145 MPa | 7000 - 21000 psi | Average value: 84.8 MPa Grade Count:33 |
Overview of materials for Nylon 66, MoS2 Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, MoS2 Filled". Each property range of values reported is minimum and maximum values of appropri.. |
|||
Tensile Strength, Ultimate | 30.0 - 145 MPa @Temperature 60.0 - 150 °C |
4350 - 21000 psi @Temperature 140 - 302 °F |
Average value: 78.6 MPa Grade Count:14 |
Overview of materials for Nylon 66, Glass Fiber Filled, Flame Retardant This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Glass Fiber Filled, Flame Retardant". Each property range of values reported is minimum and ma.. |
|||
Tensile Strength, Ultimate | 114 - 145 MPa | 16500 - 21000 psi | Average value: 131 MPa Grade Count:8 |
Overview of materials for Nylon 12, 40% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 12, 40% Glass Fiber Filled". Specific grades with glass content between 35% and 44% are included. .. |
|||
Tensile Strength, Ultimate | 93.1 - 145 MPa | 13500 - 21000 psi | Average value: 122 MPa Grade Count:4 |
Overview of materials for Acrylic/Polycarbonate Alloy, Carbon Fiber Filler This property data is a summary of similar materials in the MatWeb database for the category "Acrylic/Polycarbonate Alloy, Carbon Fiber Filler". Each property range of values reported is minimum and.. |
|||
Tensile Strength, Ultimate | 66.9 - 145 MPa | 9700 - 21000 psi | Average value: 109 MPa Grade Count:17 |
Overview of materials for Polyethersulfone (PES), 10% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Polyethersulfone (PES), 10% Glass Fiber Filled". Specific grades with glass content between 5% and 14% a.. |
|||
Tensile Strength, Ultimate | 57.0 - 145 MPa | 8270 - 21000 psi | Average value: 104 MPa Grade Count:24 |
Overview of materials for Polybutylene Terephthalate (PBT), Glass Fiber + PTFE Filled This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Glass Fiber + PTFE Filled". Each property range of values reported is .. |
|||
Tensile Strength, Ultimate | 45.0 - 145 MPa @Temperature -40.0 - 120 °C |
6530 - 21000 psi @Temperature -40.0 - 248 °F |
Average value: 83.3 MPa Grade Count:1 |
Overview of materials for Polyethylene Terephthalate (PET), Glass/Mineral Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Polyethylene Terephthalate (PET), Glass/Mineral Reinforced". Each property range of values reported is m.. |