Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | >= 758 MPa | >= 110000 psi | |
PSM Industries PolyAlloys WNF-2109 Tungsten Heavy Alloy Mil. T-21014 Class 4, SAE-AMS-T-21014 Class 4, ASTM-B-777-87 Class 4Information Provided by PolyAlloys, a division of PSM Industries |
|||
Tensile Strength, Ultimate | 758 MPa | 110000 psi | |
Hogen HM1000 Tungsten-Based Metal Mil Spec T-21014D Class 1; ASTM B-777-99 Class 1; SAE Aero Material Spec (AMS) 7725C; AMS T-21014 Class 1. Nil magnetic properties.Manufactured by powder metallurgy methods. The tungsten base offe.. |
|||
Tensile Strength, Ultimate | 758 MPa | 110000 psi | |
Hogen HM3000 Tungsten-Based Metal Mil Spec T-21014D Class 3; ASTM B-777-99 Class 3; AMS T-21014 Class 3. Nil magnetic properties.Manufactured by powder metallurgy methods. The tungsten base offers high thermal conductivity and a l.. |
|||
Tensile Strength, Ultimate | 758 MPa | 110000 psi | |
Materion BrushBronze® 630 (AMS 4640) 0.250" - 1.0" Information supplied by Brush Wellman Engineered Materials.BrushBronze™ 630 is an Aluminum-Nickel-Bronze alloy that combines high strength along with resistance to wear under severe loading con.. |
|||
Tensile Strength, Ultimate | 758 MPa | 110000 psi | |
Materion BrushBronze® 630 (AMS 4640) 1.0" - 2.0" Information supplied by Brush Wellman Engineered Materials.BrushBronze™ 630 is an Aluminum-Nickel-Bronze alloy that combines high strength along with resistance to wear under severe loading con.. |
|||
Tensile Strength, Ultimate | >= 758 MPa | >= 110000 psi | |
Materion ToughMet® T3 AT90 (OD≥4") ToughMet® is Brush Wellman's solution for severe service material problems. By applying their EquaCast® process, tailored alloying additions and spinodal hardening technology, they have e.. |
|||
Tensile Strength, Ultimate | 758 MPa | 110000 psi | |
Mi-Tech Metals HD17 Tungsten-Based Metal Mil Spec T-21014D Class 1; ASTM B-777-99 Class 1; ASTM B-777-07 Class 1; SAE Aero Material Spec (AMS) 7725C; AMS T-21014 Class 1. Nil magnetic properties.Manufactured by powder metallurgy methods. .. |
|||
Tensile Strength, Ultimate | 758 MPa | 110000 psi | |
Mi-Tech Metals HD17BB Tungsten-Based Metal ASTM B-777-07 Class 1; Slightly Magnetic (HD17 is non-magnetic).Manufactured by powder metallurgy methods. The tungsten base offers high thermal conductivity and a low CTE which combine to resist t.. |
|||
Tensile Strength, Ultimate | 758 MPa | 110000 psi | |
Mi-Tech Metals HD18 Tungsten-Based Metal Mil Spec T-21014D Class 3; ASTM B-777-99 Class 3; ASTM B-777-07 Class 3; AMS T-21014 Class 3. Nil magnetic properties.Manufactured by powder metallurgy methods. The tungsten base offers high therm.. |
|||
Tensile Strength, Ultimate | 758 MPa | 110000 psi | Annealed |
H.C. Starck MP35N® Nickel/Cobalt/Chromium/Molybdenum Alloy MP35N is a nickel-cobalt based alloy of the Multiphase® alloy system that has ultra high strength, toughness, ductility, biocompatibility, and outstanding corrosion resistance. H.C. Starck offers.. |
|||
Tensile Strength, Ultimate | 758 - 1034 MPa | 110000 - 150000 psi | |
Materion Beryllium Nickel Strip - Alloy 360 1/4 Hard Information supplied by Brush Wellman Engineered Materials.Treatment required for max strength: as suppliedFormability Ratio, 90° Bend, Radius/Thickness (Good Way): 0Formability Ratio (bad Way): .. |
|||
Tensile Strength, Ultimate | 758 MPa | 110000 psi | |
Special Metals INCONEL® 690 Nickel Superalloy, Cold Drawn Tube, 0.50 inch (12.7 mm) o.d. and 0.050 inch (1.27 mm) Thickness Composition adjustments for nuclear applications: 28-31 Cr; 0.04 max C; 0.10 max Co.Tensile strength (ultimate and yield) and elongation values reported here are typical for Cold Drawn Tube, 0.50 in.. |
|||
Tensile Strength, Ultimate | 758 MPa | 110000 psi | |
Universal Wire Works 625 Nickel Alloy Welding Wire Alloy 625 is used for TIG, MIG and submerged-arc welding of Inconel type alloys 601 and 625, Incoloy type alloy 800, as well as overlaying on steel and joining 9% nickel steel. Alloy 625 can be used.. |
|||
Tensile Strength, Ultimate | 758 MPa | 110000 psi | |
Universal Wire Works B2 Nickel Alloy Welding Wire Alloy B2 is a nickel molybdenum alloy designed for severe corrosion applications in hydrochloric acid at all concentrations and temperatures including the boiling point. This alloy is also resistant.. |
|||
Tensile Strength, Ultimate | 758 MPa | 110000 psi | |
Universal Wire Works X Nickel Alloy Welding Wire Universal Alloy X is a nickel chromium molybdenum alloy that possesses exceptional strength and oxidation resistance up to 2200 degrees F. Alloy X has been found to be highly resistant to stress-cor.. |
|||
Tensile Strength, Ultimate | 758 - 841 MPa | 110000 - 122000 psi | |
Eagle Brass 521 Phosphor Bronzes 8% C, Extra Spring Alloy C521 is a high tin alloy of the phosphor bronze family. The additional tin relative to the more commonly used C510 results in higher mechanical properties with a modest reduction in electrical.. |
|||
Tensile Strength, Ultimate | 758 - 862 MPa | 110000 - 125000 psi | |
Eagle Brass 70265 XP175, Hard Information provided by Eagle Brass Company |
|||
Tensile Strength, Ultimate | 758 MPa | 110000 psi | |
Crucible Steel 440C Chromium Steel Crucible 440C is a hardenable chromium steel. It has one of the highest attainable hardnesses of the corrosion and heat resisting grades. This grade is magnetic at all times.Information provided b.. |
|||
Tensile Strength, Ultimate | 758 MPa | 110000 psi | |
CMW® 2000 AMS-T-21014 ASTM B777 High Density Machinable Tungsten Uses: Radiation Shielding, High Mass, Gyro, Ordnance. Machinability is similar to gray iron.Information provided by CMW Inc. |
|||
Tensile Strength, Ultimate | 758 MPa | 110000 psi | Castings |
CMW® 73 Copper Alloy CMW® 73 material is a heat treatable copper base alloy having extremely high hardness and strength coupled with fair electrical and thermal conductivity. The extremely high hardness, strength and w.. |
|||
Tensile Strength, Ultimate | 758 MPa | 110000 psi | Typical |
Dura-Bar 100-70-03 Continuously Cast Ductile Iron Bar Stock ASTM A536 Continuously cast ductile iron bar stock is produced in a wide variety of sizes and shapes, including rounds, rectangles and special shape cross sections.It often is used as a direct replacement for.. |
|||
Tensile Strength, Ultimate | 758 MPa | 110000 psi | Annealed |
AK Steel 201LN Austenitic Stainless steel AK Steel 210 was developed originally to conserve nickel. It provides properties similar to Type 301 and can be used in most applications for Type 301. This alloy is non-magnetic in the annealed c.. |
|||
Tensile Strength, Ultimate | >= 758 MPa | >= 110000 psi | |
ATI Allegheny Ludlum Alloy 255 Stainless Steel, UNS S32550 Alloy 255 is a 25% chromium duplex ferritic-austenitic stainless steel designed to provide a superior combination of high strength and excellent corrosion resistance for a wide variety of applicatio.. |
|||
Tensile Strength, Ultimate | 758 MPa | 110000 psi | |
Universal Wire Works 112 Nickel Alloy Welding Wire Alloy 112 is used for arc welding Incoloy types 800 and 801, Inconel types 601 and 625, for overlaying on carbon steel, and for joining 9% nickel steel. Alloy 112 dissimilar welding applications are.. |
|||
Tensile Strength, Ultimate | 758 MPa | 110000 psi | |
Haynes Hastelloy® C-22® alloy, all-weld metal, SMAW HASTELLOY® C-22® alloy is a nickel-chromium-molybdenum-tungsten alloy with excellent overall corrosion resistance compared to other Ni-Cr-Mo alloys, including HASTELLOY C-276 and C-4 alloys and al.. |
|||
Tensile Strength, Ultimate | >= 758 MPa | >= 110000 psi | |
Materion ToughMet® T3 CX105 (OD ToughMet® is Brush Wellman's solution for severe service material problems. By applying their EquaCast® process, tailored alloying additions and spinodal hardening technology, they have engin.. |
|||
Tensile Strength, Ultimate | 758 MPa | 110000 psi | |
Haynes Hastelloy® C-22® alloy, SMAW weld, 904L base metal, C-22 weld metal HASTELLOY® C-22® alloy is a nickel-chromium-molybdenum-tungsten alloy with excellent overall corrosion resistance compared to other Ni-Cr-Mo alloys, including HASTELLOY C-276 and C-4 alloys and al.. |
|||
Tensile Strength, Ultimate | 758 MPa | 110000 psi | |
Latrobe Nitralloy® 135 Modified VAC-ARC, 3 to 5 in Premium Nitriding Steel NITRALLOY 135 MODIFIED VAC-ARC steel is a low alloy nitriding grade with moderate hardenability. It has been designed to provide a high case hardness and to maintain its core strength during the nit.. |