Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Materion BrushBronze® 630 (AMS 4640) 1.0" - 2.0"

Category Metal , Nonferrous Metal , Copper Alloy , Bronze , Copper Casting Alloy
Manufacturer Materion Corporation (former Brush Wellman)
Trade Name BrushBronze®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Materion BrushBronze® 630 (AMS 4640) 1.0" - 2.0".pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information supplied by Brush Wellman Engineered Materials.BrushBronzeâ„¢ 630 is an Aluminum-Nickel-Bronze alloy that combines high strength along with resistance to wear under severe loading conditions. This material, specified as AMS 4640, is frequently used for very demanding aerospace applications, including, but not limited to: bushings, spherical and rod end bearings, rub pads, and wear strips. This material is also commonly used for applications in the oil and gas and other durable goods markets.BrushBronzeâ„¢ 630 (AMS 4640) offers several significant advantages over other materials available in the marketplace due to the EquaCastâ„¢ process:Higher and more consistent mechanical propertiesImproved service lifeEase of useBrush Engineered Materials Inc. changed its name to Materion Corporation in March 2011.
Mechanical Properties Metric English Comments
Hardness, Brinell 201 - 248
201 - 248
Tensile Strength, Ultimate 758 MPa
110000 psi
Tensile Strength, Yield 414 MPa
60000 psi
Elongation at Break 10 %
10 %
Component Elements Properties Metric English Comments
Aluminum, Al 9.0 - 11 %
9.0 - 11 %
Copper, Cu >= 78 %
>= 78 %
Iron, Fe 2.0 - 4.0 %
2.0 - 4.0 %
Manganese, Mn <= 1.5 %
<= 1.5 %
Nickel, Ni 4.0 - 5.5 %
4.0 - 5.5 %
Silicon, Si <= 0.25 %
<= 0.25 %
Tin, Sn <= 0.20 %
<= 0.20 %
Zinc, Zn <= 0.30 %
<= 0.30 %
Copyright © lookpolymers.com All Rights Reserved