Material Notes:
Mil Spec T-21014D Class 1; ASTM B-777-99 Class 1; SAE Aero Material Spec (AMS) 7725C; AMS T-21014 Class 1. Nil magnetic properties.Manufactured by powder metallurgy methods. The tungsten base offers high thermal conductivity and a low CTE which combine to resist thermal fatigue. The high melting point reduces soldering or erosion problems. To increase the machinability of this brittle metal, alloying elements are added and practical use of tungsten is possible for die casting tools.Used in resistance brazing and high temp applications. Used as counter weights and counter balances, radiation shielding components, tool shanks for boring bars and other tools for chatter-free machining.Data provided by Hogen Industries.
Physical Properties Metric English Comments
Density 17.0 g/cc
0.614 lb/in³
Mechanical Properties Metric English Comments
Hardness, Rockwell C 32
32
Tensile Strength, Ultimate 758 MPa
110000 psi
Tensile Strength, Yield 550 MPa

@Strain 0.200 %
79800 psi

@Strain 0.200 %
Elongation at Break 6.0 %
6.0 %
in 50 mm
Modulus of Elasticity 276 GPa
40000 ksi
Thermal Properties Metric English Comments
CTE, linear 5.40 µm/m-°C

@Temperature 20.0 - 400 °C
3.00 µin/in-°F

@Temperature 68.0 - 752 °F
Thermal Conductivity 96.0 W/m-K
666 BTU-in/hr-ft²-°F
Component Elements Properties Metric English Comments
Copper, Cu 4.0 %
4.0 %
Nickel, Ni 6.0 %
6.0 %
Tungsten, W 90 %
90 %
Electrical Properties Metric English Comments
Electrical Resistivity 0.0000120 ohm-cm