Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 71.0 MPa | 10300 psi | ASTM D638 |
Plaskolite Optix® CA-75 General Purpose Acrylic Resin Injection Molding and Extrusion Grade Pellets. Highest heat resistance, medium flow. |
|||
Tensile Strength, Ultimate | 71.0 MPa | 10300 psi | ASTM D638 |
Plaskolite West Optix® CA-75 General Purpose Acrylic Resin Injection Molding and Extrusion Grade Pellets. Highest heat resistance, medium flow. |
|||
Tensile Strength, Ultimate | 71.0 MPa | 10300 psi | |
Polycasa Acryl® G 77 E Acrylic, Extrusion Grade Extrusion grade for semi-finished products such as profile, sheet and tubes; TV-, HiFi - and video-windows.Data was collected by ISO methods.Quinn Manufacturing Group rebranded its Plastics Division.. |
|||
Tensile Strength, Ultimate | 71.0 MPa | 10300 psi | ASTM D638 |
LG Chemical Lupoy 1201-15 Polycarbonate Resin Description: LUPOY PC 1201-15 resin is designed for extrusion and injection molding products. It exhibits an excellent physical property balance of heat resistance, transparency and impact strength... |
|||
Tensile Strength, Ultimate | 71.0 MPa | 10300 psi | ASTM D638 |
LG Chemical Lupoy 1300-15 Polycarbonate Resin Description: LUPOY PC 1300-15 resin is designed for extrusion and injection molding products. It exhibits an excellent physical property balance of heat resistance, transparency and impact strength... |
|||
Tensile Strength, Ultimate | 71.0 MPa | 10300 psi | ASTM D638 |
LG Chemical Lupoy 1301-12 Polycarbonate Resin Description: LUPOY PC 1301-12 resin is designed for extrusion and injection molding products. It exhibits an excellent physical property balance of heat resistance, transparency and impact strength... |
|||
Tensile Strength, Ultimate | 71.0 MPa | 10300 psi | ASTM D638 |
LG Chemical Lupoy 1301V-10 Polycarbonate Resin Description: LUPOY PC 1301V-10 resin is designed for extrusion and injection molding products. It exhibits an excellent physical property balance of heat resistance, transparency and impact strength.. |
|||
Tensile Strength, Ultimate | 71.0 MPa | 10300 psi | ASTM D638 |
LG Chemical Lupoy NF1007F 10R Polycarbonate Resin Description: LUPOY NF 1007F10R, eco-friendly UL94 V0/3.0 mm, is designed for extrusion and injection molding products. It combines an excellent physical property balance of heat resistance, transpar.. |
|||
Tensile Strength, Ultimate | 71.0 MPa | 10300 psi | ASTM D638 |
LG Chemical Lupoy NF1009F 15 Polycarbonate Resin Description: LUPOY NF 1009F15, eco-friendly UL94 V0/2.0 mm, is designed for extrusion and injection molding products. It combines an excellent physical property balance of heat resistance, transpare.. |
|||
Tensile Strength, Ultimate | 71.0 MPa | 10300 psi | ASTM D638 |
Lucky IG-840 Acrylic, Injection Grade General purpose injection molding grade. May be UV stabilized. General Lucky PMMA qualities: Transparent/elegant appearance, high heat and weather resistance, excellent chemical resistance and col.. |
|||
Tensile Strength, Ultimate | 71.0 MPa | 10300 psi | ASTM D638 |
LG Chemical Lupoy 1200HP-15 Polycarbonate Resin Description: LUPOY PC 1200HP-15 resin is designed for extrusion and injection molding products. It exhibits an excellent physical property balance of heat resistance, transparency and impact strengt.. |
|||
Tensile Strength, Ultimate | 71.0 MPa | 10300 psi | ASTM D638 |
LG Chemical Lupoy 1300-10 Polycarbonate Resin Description: LUPOY PC 1300-10 resin is designed for extrusion and injection molding products. It exhibits an excellent physical property balance of heat resistance, transparency and impact strength... |
|||
Tensile Strength, Ultimate | 71.0 MPa | 10300 psi | ASTM D638 |
LG Chemical Lupoy 1300-12 Polycarbonate Resin Description: LUPOY PC 1300-12 resin is designed for extrusion and injection molding products. It exhibits an excellent physical property balance of heat resistance, transparency and impact strength... |
|||
Tensile Strength, Ultimate | 71.0 MPa | 10300 psi | ASTM D638 |
LG Chemical Lupoy 1303AH-15 Polycarbonate Resin Description: LUPOY PC 1303AH-15 Tint Polycarbonate Resin is designed for injection molding of auto-headlamps. It exhibits an excellent physical property balance of heat resistance, transparency and .. |
|||
Tensile Strength, Ultimate | 71.0 MPa | 10300 psi | ASTM D638 |
Styron CALIBREâ„¢ 201-10 Polycarbonate Information provided by DowThis product line was spun off from Dow Chemical to Styron in 2010. |
|||
Tensile Strength, Ultimate | 71.0 MPa | 10300 psi | ASTM Data |
Styron CALIBRE™ 2060 10 Polycarbonate, Sterilization Grade CALIBRE® 2060 series resins are designed for those applications which use steam or ethylene oxide for sterilization. This material has excellent retention of physical properties and optical clari.. |
|||
Tensile Strength, Ultimate | 71.0 MPa | 10300 psi | 50 mm/min; ASTM D638 |
Styron CALIBREâ„¢ 2061-15 Polycarbonate CALIBREâ„¢ 2061-15 resin is used in applications involving steam or ethylene oxide for sterilization - though suitability for use in these applications is dependent upon autoclave cycle times and.. |
|||
Tensile Strength, Ultimate | 71.0 MPa | 10300 psi | ASTM Data |
Styron CALIBRE™ 2071 15 Polycarbonate, Sterilization Grade CALIBRE® 2071 resins are designed for those applications which use steam or ethylene oxide for sterilization while providing enhanced mold release characteristics. This material has excellent ret.. |
|||
Tensile Strength, Ultimate | 71.0 MPa | 10300 psi | ASTM Data |
Styron CALIBRE™ 300 10 Polycarbonate, General Purpose CALIBRE® 300 series are general purpose, UL listed polycarbonate resins. CALIBRE 300 series resins exhibit an excellent physical property balance of heat resistance, transparency and impact stren.. |
|||
Tensile Strength, Ultimate | 71.0 MPa | 10300 psi | 0.125 in, injection molded, unannealed; ASTM D638 |
Styron EMERGEâ„¢ 4310-10 Polycarbonate EMERGEâ„¢ PC 4310-10 advanced resin is high-performance polycarbonate resin offering high heat resistance and maximum toughness. Applications: Consumer Electronics and Information Technology Eq.. |
|||
Tensile Strength, Ultimate | 71.0 MPa | 10300 psi | 0.125 in, injection molded, unannealed; ASTM D638 |
Styron EMERGEâ„¢ 4330-10 Polycarbonate EMERGEâ„¢ PC 4330-10 advanced resin is a polycarbonate resin offering ultraviolet light stability, high heat resistance and maximum toughness. Applications: Consumer Electronics and Information.. |
|||
Tensile Strength, Ultimate | 71.0 MPa | 10300 psi | 0.125 in, injection molded, unannealed; ASTM D638 |
Styron EMERGEâ„¢ 4330-15 Polycarbonate EMERGEâ„¢ PC 4330-15 advanced resin is a polycarbonate resin offering ultraviolet light stability, high heat resistance and maximum toughness. Applications: Consumer Electronics and Information.. |
|||
Tensile Strength, Ultimate | 71.0 MPa | 10300 psi | ASTM D638 |
Styron CALIBREâ„¢ 201-15 Polycarbonate Information provided by DowThis product line was spun off from Dow Chemical to Styron in 2010. |
|||
Tensile Strength, Ultimate | 71.0 MPa | 10300 psi | 0.125 in, injection molded, unannealed; ASTM D638 |
Styron EMERGEâ„¢ 4310-15 Polycarbonate EMERGEâ„¢ PC 4310-15 advanced resin is high-performance polycarbonate resin offering high heat resistance and maximum toughness. Applications: Consumer Electronics and Information Technology Eq.. |
|||
Tensile Strength, Ultimate | 71.0 MPa | 10300 psi | 0.125 in, injection molded, unannealed; ASTM D638 |
Styron EMERGEâ„¢ 4510-10 Polycarbonate EMERGEâ„¢ PC 4510-10 advanced resin is a general purpose polycarbonate resin offering ignition resistance, heat resistance and excellent toughness. Applications: Consumer Electronics and Inform.. |
|||
Tensile Strength, Ultimate | 71.0 MPa | 10300 psi | 0.125 in, injection molded, unannealed; ASTM D638 |
Styron EMERGEâ„¢ 4530-15 Polycarbonate EMERGEâ„¢ PC 4530-15 advanced resin is a general purpose polycarbonate resin offering ultraviolet light stability, ignition resistance, heat resistance and excellent toughness. Applications: Co.. |
|||
Tensile Strength, Ultimate | 71.0 MPa | 10300 psi | DIN 53504 |
Lubrizol ESTANE® 5719 Ester Based Thermoplastic Polyurethane (European Grade) Description: Estane® thermoplastic polyurethanes (TPUs) include elastomeric materials that bridge the gap between flexible rubber and rigid plastics. These materials offer toughness and durability .. |
|||
Tensile Strength, Ultimate | 71.0 MPa | 10300 psi | |
Cotronics Duralco™ 4460 Electrically Resistant, Low Viscosity Epoxy Adhesive, Coating, and Sealant Excellent adhesion to metals, plastics, ceramics and glass. High bond strength, low moisture absorption, high thermal stability, low shrinkage and excellent chemical, electrical, and radiation resi.. |
|||
Tensile Strength, Ultimate | 71.0 MPa | 10300 psi | ASTM D638 |
Cast Nylons Nycast® 6MPB Plasticized Nylon 6 A plasticized Type 6 material, NYCAST® 6MPB is formulated for use as pile driver caps or cushion pads. Data provided by the manufacturer, Cast Nylons Limited.The data below are average values prese.. |
|||
Tensile Strength, Ultimate | 71.0 MPa | 10300 psi | ASTM D638 |
Asahi Kasei Delpet® 60N Acrylic Molding Compound 60N is a medium grade of heat resistance and mechanical strength, allowing injection molding through relatively small gates and runners. General Delpet® qualities include attractive transparency, .. |