Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 65.5 MPa | 9500 psi | ASTM D638 |
PTS Trimid® N66-1010L Lubed, Utility Nylon 6/6 Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Tensile Strength, Ultimate | 65.5 MPa | 9500 psi | TM R050-36 |
Resinlab® EP950G Gray Aluminum Filled Rubber Modified Epoxy EP950G Gray is an aluminum filled one part rubber modified epoxy designed for bonding metal and other structural material subject to stress at elevated temperature. It is a medium paste-like viscosi.. |
|||
Tensile Strength, Ultimate | 65.5 MPa | 9500 psi | ASTM D638 |
Plaskolite West Optix® CA-81 UVA-7 UV-Absorbing Acrylic Resin Special UV-absorption grade, extrusion and injection moldingApplications: A special UV-absorption acrylic resin for extrusion and injection molding. It is slightly lubricated for ease of processing.. |
|||
Tensile Strength, Ultimate | 65.5 - 175 MPa | 9500 - 25400 psi | Average value: 114 MPa Grade Count:60 |
Overview of materials for Syndiotactic Polystyrene (SPS) with Glass or Carbon Fiber This property data is a summary of similar materials in the MatWeb database for the category "Syndiotactic Polystyrene (SPS) with Glass or Carbon Fiber". Each property range of values reported is mi.. |
|||
Tensile Strength, Ultimate | 65.5 MPa | 9500 psi | ASTM D638 |
Rostone Rosite® 3950ES SMC Thermoset Polyester, 25% Glass Reinforced
(discontinued **) Key Features: High Strength; High DielectricElectrical grade material that provides higher flexural and impact strength than Rosite 3550 composites with comparable glass fiber content. 3950ES is fo.. |
|||
Tensile Strength, Ultimate | 65.5 MPa | 9500 psi | |
Inchem Phenoxy PKFE Phenoxy PKFE - polyhydroxy ether of Bisphenol A. Originally developed by Union Carbide. Produced by InChem Corporation. |
|||
Tensile Strength, Ultimate | 65.5 MPa | 9500 psi | ASTM D638 |
Styron CALIBREâ„¢ 201-22 Polycarbonate Information provided by DowThis product line was spun off from Dow Chemical to Styron in 2010. |
|||
Tensile Strength, Ultimate | 65.5 MPa | 9500 psi | 50 mm/min; ASTM D638 |
Styron CALIBREâ„¢ 2061-22 Polycarbonate CALIBREâ„¢ 2061-22 resin is used in applications involving steam or ethylene oxide for sterilization - though suitability for use in these applications is dependent upon autoclave cycle times and.. |
|||
Tensile Strength, Ultimate | 65.5 MPa | 9500 psi | ASTM Data |
Styron CALIBRE™ 701 15 Polycarbonate, General Purpose CALIBRE® 701 series polycarbonate resins are a general purpose, transparent, ignition resistant grades equipped with a mold release package. The CALIBRE 701 series resins exhibit a high heat resi.. |
|||
Tensile Strength, Ultimate | 65.5 MPa | 9500 psi | 0.125 in, injection molded, unannealed; ASTM D638 |
Styron EMERGEâ„¢ 4310-22 Polycarbonate EMERGEâ„¢ PC 4310-22 advanced resin is high-performance polycarbonate resin offering high heat resistance, toughness, and superior flow. Applications: Consumer Electronics and Information Techn.. |
|||
Tensile Strength, Ultimate | 65.5 MPa | 9500 psi | 0.125 in, injection molded, unannealed; ASTM D638 |
Styron EMERGEâ„¢ 4330-22 Polycarbonate EMERGEâ„¢ PC 4330-22 advanced resin is high-performance polycarbonate resin offering ultraviolet light stability, high heat resistance, toughness, and superior flow. Applications: Consumer Elec.. |
|||
Tensile Strength, Ultimate | 65.5 MPa | 9500 psi | ASTM D638 |
Styron EMERGEâ„¢ 4610-10 Polycarbonate EMERGEâ„¢ PC 4610-10 advanced resin is formulated to deliver both outstanding clarity and enhanced ignition resistance while maintaining excellent physical properties and processability. Applica.. |
|||
Tensile Strength, Ultimate | 65.5 MPa | 9500 psi | ASTM D638 |
Styron EMERGEâ„¢ 4630-10 Polycarbonate EMERGEâ„¢ PC 4630-10 advanced resin is formulated to supply both excellent ultraviolet stability and enhanced ignition resistance while maintaining excellent physical properties and processabilit.. |
|||
Tensile Strength, Ultimate | 65.5 MPa | 9500 psi | ASTM D638 |
Styron CALIBREâ„¢ 301 EP Polycarbonate Information provided by DowThis product line was spun off from Dow Chemical to Styron in 2010. |
|||
Tensile Strength, Ultimate | 65.5 MPa | 9500 psi | ASTM D638 |
Styron CALIBREâ„¢ 303 EP Polycarbonate Information provided by DowThis product line was spun off from Dow Chemical to Styron in 2010. |
|||
Tensile Strength, Ultimate | 65.5 MPa | 9500 psi | ASTM D638 |
Styron EMERGEâ„¢ 4600-10 Polycarbonate EMERGEâ„¢ PC 4600-10 advanced resin is formulated to supply both clarity and enhanced ignition resistance while maintaining excellent physical properties. Applications: Information Technology E.. |
|||
Tensile Strength, Ultimate | 65.5 MPa | 9500 psi | |
Cotronics Duralco™ 4461 Electrically Resistant, Low Viscosity Epoxy Adhesive, Coating, and Sealant |
|||
Tensile Strength, Ultimate | 65.5 MPa | 9500 psi | |
Abatron AboCast/AboCure 8109-3 Low viscosity, RT cure. Easy processing.Processing: 100/10 pbw; Potlife: 2.5 h/20°C (68°F), 30 min/40°C (105°F), 15 min/60°C (140°F); mix at RT; cures in: 24 h/20°C (68°F), 2-3 h/60°C (140.. |
|||
Tensile Strength, Ultimate | 65.5 MPa | 9500 psi | ATSM D638 |
Ashley Polymers Ashlene® P1503 Polycarbonate A rigid flame retardant polycarbonate, UV stabilized for applications requiring superior dimensional stability and overall toughness. Also available as 1500 without UV stabilizer.Data provided by t.. |
|||
Tensile Strength, Ultimate | 65.5 MPa | 9500 psi | ASTM D638 |
Applied Composites 150 Polyester SMC Industry Application: TransportationProduct Application: Engine CoversDistinct Features: Grey Pigments Only, Low DensityInformation provided by Applied Composites Corporation. |
|||
Tensile Strength, Ultimate | 65.5 MPa | 9500 psi | ASTM D638 |
Technetics Group Amicon™ Acetal Copolymer
(Unverified Data**) Information provided by Technetics Group (formerly Plastomer Technologies) |