Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | >= 480 MPa | >= 69600 psi | |
MetalTek MTEK 23-35WCo Heat Resistant Stainless Steel Information provided by MetalTekCast ASTM A297 MOD. |
|||
Tensile Strength, Ultimate | 480 - 655 MPa | 69600 - 95000 psi | |
MetalTek WC 6 Cast UNS J24054 Alloy Steel General structural use.Applications: Cylinders, rolls, hollow shafts.Information provided by MetalTek |
|||
Tensile Strength, Ultimate | 480 - 655 MPa | 69600 - 95000 psi | |
MetalTek WCB UNS J13345 Cast Alloy Steel General structural use.Applications: Cylinders, rolls, hollow shafts.Information provided by MetalTek |
|||
Tensile Strength, Ultimate | 480 - 680 MPa | 69600 - 98600 psi | |
Materion Brush 1915™ Heat Treated Temper Rod, 0.375" - 0.500" Information supplied by Brush Wellman Engineered Materials.Treatment required for max strength: 3.5 hrs @ 370°C or Mill HardenedBrush 1915™ is Brush Wellman's new heat-treatable leaded coppe.. |
|||
Tensile Strength, Ultimate | >= 480 MPa | >= 69600 psi | |
MetalTek MTEK 29-17 Cast UNS J94003 Heat Resistant Stainless Steel Good strength, ductility, and corrosion resistance.Applications: Billet skids, rails, tube spacers.Information provided by MetalTek |
|||
Tensile Strength, Ultimate | 480 MPa @Temperature 550 °C |
69600 psi @Temperature 1020 °F |
Annealed prior to test |
Special Metals INCOLOY® Alloy 330 A nickel-iron-chromium alloy with an addition of silicon for enhanced oxidation resistance. It has good strength at high temperatures and excellent resistance to carburizing and oxidizing atmospher.. |
|||
Tensile Strength, Ultimate | 480 MPa @Temperature 550 °C |
69600 psi @Temperature 1020 °F |
Annealed prior to test |
Special Metals INCOLOY® Alloy 800HT™ A nickel-iron-chromium alloy having the same basic composition as INCOLOY alloy 800 but with significantly higher creep-rupture strength. The higher strength results from close control of the carbo.. |
|||
Tensile Strength, Ultimate | 480 - 540 MPa | 69600 - 78300 psi | |
SSAB Tunnplat Aluzink 380A YP High-strength Metal-coated Steel High-strength Metal-coated SteelComments: Aluzink YP - HSLA steel (aluminum-zinc coated sheet). Property values are for thicknesses 0.4 - 2.0 mm. Iron content is approximate - exact composition is .. |
|||
Tensile Strength, Ultimate | >= 480 MPa | >= 69600 psi | |
SSAB Tunnplat Domex® 420XP Extra High-strength Cold-forming Steel Extra High-strength Cold-forming Steel, HSLACharacteristics: Domex® is the brand name of hot rolled products from SSAB Tunnplat. Domex® cold-forming steels are modern structural steels. Gene.. |
|||
Tensile Strength, Ultimate | >= 480 MPa | >= 69600 psi | |
SSAB Tunnplat Domex® 420YP Cold-forming Steel, HSLA Cold-forming Steel, HSLACharacteristics: Domex® is the brand name of hot rolled products from SSAB Tunnplat. Domex® cold-forming steels are modern structural steels. General use of Domex®.. |
|||
Tensile Strength, Ultimate | 480 - 650 MPa | 69600 - 94300 psi | |
CLAL-MSX NICLAL 1800 H12 1/2 Hard Copper Alloy, Free Cutting Nickel-Silver Main Characteristics: Good corrosion resistanceHigh mechanical propertiesTypical Applications:Parts subject to high stressHigh quality fastenersInformation provided by CLAL-MSX |
|||
Tensile Strength, Ultimate | >= 480 MPa | >= 69600 psi | |
AK Steel ASTM A 1011, Grade 55 Hot Rolled Carbon Steel, Structural Steel (SS) Information provided by AK Steel |
|||
Tensile Strength, Ultimate | >= 480 MPa | >= 69600 psi | |
AK Steel ASTM A 570, Grade 55 Hot Rolled Carbon Steel, Structural Quality (SQ) For gauges up to 0.229", ASTM A 570 must be specified, gauges >0.230", ASTM A 907 must be used. Items 0.180 to 0.230" gauge which are >48" wide may be ordered to either A 570 or A 907.Information p.. |
|||
Tensile Strength, Ultimate | >= 480 MPa | >= 69600 psi | |
AK Steel ASTM A 607 Class 1 Formable, Grade 55K Hot Rolled Carbon Steel, Medium/High Strength Low Alloy (HSLA) ASTM A 607 is for Hot Rolled and Cold Rolled grades. AK Steel produces Type 1 (columbium bearing only), Class 1 has limits placed on C, Mn, P and S with a 15 ksi difference between the minimum spec.. |
|||
Tensile Strength, Ultimate | >= 480 MPa | >= 69600 psi | |
AK Steel ASTM A 607 Class 2 Formable, Grade 60K Hot Rolled Carbon Steel, Medium/High Strength Low Alloy (HSLA) ASTM A 607 is for Hot Rolled and Cold Rolled grades. AK Steel produces Type 1 (columbium bearing only), Class 2 limits only C and has a 10 ksi difference between the minimum specified YS and UTS. .. |
|||
Tensile Strength, Ultimate | >= 480 MPa | >= 69600 psi | |
AK Steel ASTM A 715 Class 2 Formable, Grade 60F Hot Rolled Carbon Steel, Medium/High Strength Low Alloy (HSLA) ASTM A 715 is for Hot Rolled and Cold Rolled grades. AK Steel produces Type 1 (columbium bearing only), Class 2 limits only C and has a 10 ksi difference between the minimum specified YS and UTS. .. |
|||
Tensile Strength, Ultimate | 480 MPa @Temperature 371 °C |
69600 psi @Temperature 700 °F |
Plate |
AK Steel NITRONIC® 30 Austenitic Stainless Steel AK Steel NITRONIC 30 Stainless Steel offers significantly higher strength than Type 304 and potential for applications requiring good resistance to aqueous and atmospheric corrosion resistance combi.. |
|||
Tensile Strength, Ultimate | 480 MPa | 69600 psi | |
ATI Allegheny Ludlum AL 409 Cb™ Brazeable Ferritic Stainless Steel, 8.5% Cold Work AL 409 Cb™ is normally 12.5% chromium ferritic stainless steel with columbium stabilization and with restricted titanium and aluminum contents. As a result of these alloying adjustments, the braze.. |
|||
Tensile Strength, Ultimate | >= 480 MPa | >= 69600 psi | |
AK Steel ASTM A 1011, Class 1 Formable, Grade 55K Hot Rolled Carbon Steel, Medium/High Strength Low Alloy Steel (HSLA) Information provided by AK Steel |
|||
Tensile Strength, Ultimate | >= 480 MPa | >= 69600 psi | |
AK Steel ASTM A 1011, Class 2 Formable, Grade 60K Hot Rolled Carbon Steel, Medium/High Strength Low Alloy Steel (HSLA) Information provided by AK Steel |
|||
Tensile Strength, Ultimate | >= 480 MPa | >= 69600 psi | |
AK Steel SAE J1392, Grade 55F Hot Rolled Carbon Steel, Medium/High Strength Low Alloy (HSLA) AK Steel Formable Grade - F indicates inclusion controlled low alloy.Information provided by AK Steel |
|||
Tensile Strength, Ultimate | 480 MPa | 69600 psi | As Cast |
AFE Technologies Cronite 37Ni/18Cr/Nb No. HR32 High temperature nickel alloy castings. Applications include heat treatment and handling products, furnace products, tubes, power generation, and petrochemical industries.Information provided by AF.. |
|||
Tensile Strength, Ultimate | 480 MPa @Temperature 870 °C |
69600 psi @Temperature 1600 °F |
|
Haynes 242® alloy, hot rolled plate, annealed and aged Age-hardenable, high ductility in the aged condition, lower thermal expansion than most alloys, very good oxidation resistance up to 815°C, excellent low cycle fatigue properties, very good thermal.. |
|||
Tensile Strength, Ultimate | 480 MPa @Temperature 704 °C |
69600 psi @Temperature 1300 °F |
|
Haynes Hastelloy® N, 1.6 mm sheet, heat treated at 1175°C, rapid air cooled Applications include containers for molten fluoride salts. Good oxidation resistance to hot fluoride salts at 705-870°C (1300-1600°F), good oxidation resistance in air.Data provided by the manufac.. |
|||
Tensile Strength, Ultimate | 480 MPa @Temperature 649 °C |
69600 psi @Temperature 1200 °F |
|
Haynes 230® alloy, as cast vacuum investment casting Excellent high-temperature strength, outstanding resistance to oxidizing environments up to 1149°C, premier resistance to nitriding environments, and excellent long-term thermal stability. Applicat.. |
|||
Tensile Strength, Ultimate | 480 - 590 MPa | 69600 - 85600 psi | |
Materion Beryllium Copper Alloy 3 Plate & Rolled Bar; H (TD04) Temper; up to 76 mm Thickness (UNS C17510) Treatment required for max strength: as suppliedTabulated properties apply to products after age hardening. Information supplied by Brush Wellman.Brush Engineered Materials Inc. changed its name to.. |