Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 48.0 MPa | 6960 psi | ASTM D638 |
Proto3000 Duraform® EX Selective Laser Sintering (SLS®) Prototyping Polymer Plastic for use with all Sinterstation® Pro and Sinterstation HiQ™ series SLS® systemsDescription: This impact-resistant plastic offers the toughness of injection-molded polypropylene and ABS and.. |
|||
Tensile Strength, Ultimate | 48.0 - 152 MPa | 6960 - 22000 psi | Average value: 102 MPa Grade Count:73 |
Overview of materials for Acetal Copolymer, Carbon Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer, Carbon Fiber Filled". Each property range of values reported is minimum and maximum va.. |
|||
Tensile Strength, Ultimate | 48.0 MPa | 6960 psi | ASTM D638 |
PolyOne Lubri-Tech™ AT-000/08T Acetal - 8% PTFE
(discontinued **) Data provided by PolyOne. |
|||
Tensile Strength, Ultimate | 48.0 MPa | 6960 psi | ASTM D638 |
PolyOne Lubri-Tech™ ATH-000/20T Homopolymer Acetal - 20% PTFE Lubricated
(discontinued **) Data provided by PolyOne. |
|||
Tensile Strength, Ultimate | 48.0 - 76.0 MPa | 6960 - 11000 psi | Average value: 61.4 MPa Grade Count:5 |
Overview of materials for Polycarbonate/Styrenic Alloy This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate/Styrenic Alloy". Each property range of values reported is minimum and maximum values of a.. |
|||
Tensile Strength, Ultimate | 48.0 - 200 MPa @Temperature -40.0 - 150 °C |
6960 - 29000 psi @Temperature -40.0 - 302 °F |
Average value: 86.6 MPa Grade Count:1 |
Overview of materials for Liquid Crystal Polymer (LCP), Mineral Filled This property data is a summary of similar materials in the MatWeb database for the category "Liquid Crystal Polymer (LCP), Mineral Filled". Each property range of values reported is minimum and max.. |
|||
Tensile Strength, Ultimate | 48.0 MPa | 6960 psi | ASTM D638 |
Plenco 5314 Black (INJ) Impact Grade Phenolic Molding Compound
(discontinued **) Plaslok 5314 is the replacement material for the former Union Carbide BMMA-5314. It is a two-stage, impact grade phenolic molding compound suitable for compression, transfer or injection molding of.. |
|||
Tensile Strength, Ultimate | 48.0 MPa | 6960 psi | ASTM D638 |
IDI Composites M-102 Thermoset Polyester, Molding Mechanical grade materials in a range of strengths with excellent moldability and molded part appearance.Data provided by the manufacturer. |
|||
Tensile Strength, Ultimate | 48.0 MPa | 6960 psi | ASTM D638 |
LG Chemical Lupoy 1080-70 Polycarbonate Resin Description: LUPOY PC 1080-70 resin is designed for optical media discs applications. It exhibits an excellent physical property balance of heat resistance, transparency and impact strength.Main Ch.. |
|||
Tensile Strength, Ultimate | 48.0 MPa | 6960 psi | ASTM D638 |
Hannam Chemical Hanalac H-2938 ABS |
|||
Tensile Strength, Ultimate | 48.0 MPa @Temperature 1149 °C |
6960 psi @Temperature 2100 °F |
|
Haynes Multimet® alloy, 1.6 mm thick sheet, 1177°C heat treatment, rapid air cooled Recommended for use in applications involving high stress at temperatures up to 816°C (1500°F), and moderate stresses up to 1093°C (2000°F). Excellent oxidation resistance, good ductilit.. |
|||
Tensile Strength, Ultimate | 48.0 MPa | 6960 psi | ASTM D638 |
Sumitomo Bakelite North America RX® 448 Cellulose Reinforced Phenolic Novolac RX448 is a cellulose fiber reinforced phenolic novolac molding compound. This material is recommended for large parts requiring moderate toughness. It is designed to meet the requirements of ASTM D.. |
|||
Tensile Strength, Ultimate | 48.0 MPa | 6960 psi | ASTM D638 |
Sumitomo Bakelite Durez® 25378 Phenolic, Injection Grade Durez 25378 Black Phenolic is a two stage heat resistant/electrical grade molding material having an excellent molded finish, low shrinkage and good heat resistance. Durez 25378 has exceptional UL .. |
|||
Tensile Strength, Ultimate | 48.0 MPa | 6960 psi | ASTM D638 |
Sumitomo Bakelite Durez® 32962 Phenolic Molding Compound, Injection Grade Durez 32962 Black Phenolic is a medium impact, molding compound. It is designed for applications where additional mechanical strength is required. Typical applications include appliance housings whe.. |
|||
Tensile Strength, Ultimate | 48.0 MPa | 6960 psi | ASTM D638 |
Lubrizol Isoplast® 101 Engineering Thermoplastic Polyurethane Resin ISOPLAST® 101 is an engineering thermoplastic polyurethane resin.Available in Americas, Europe, Middle East, Africa, India and AsiaData provided by LubrizolLubrizol acquired the Isoplast product li.. |
|||
Tensile Strength, Ultimate | 48.0 MPa | 6960 psi | ISO 527-1, 2 |
Polyplastics Duracon® TD-10 Acetal Co-polymer (POM), High impact, Flexible DURACON® is a crystalline thermoplastic acetal copolymer. The primary raw material trioxane, a trimer of formaldehyde.The thermoplastic adopts a copolymer structure in which polyoxymethylene (-C-O).. |
|||
Tensile Strength, Ultimate | 48.0 MPa | 6960 psi | ASTM D638/D412 |
Covestro Prism® CM-200 Polyurethane Solid RIM, MDI-based 2-Component Liquid System 0.125 in. thickness. RIM = Reaction Injection MoldingInformation provided by Bayer Corporation, Polyurethanes DivisionAs of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and o.. |
|||
Tensile Strength, Ultimate | 48.0 MPa | 6960 psi | ASTM D638 |
3D Systems DuraForm® EX Impact-Resistant Plastic for SLS® Systems This impact-resistant plastic offers the toughness of injection-molded polypropylene and ABS and is suitable for Rapid Manufacturing. For use with all Sinterstation® Pro and Sinterstation HiQ™ ser.. |
|||
Tensile Strength, Ultimate | 48.0 MPa | 6960 psi | ATSM D638 |
Ashley Polymers Ashlene® P260WO PPO A general purpose V-0 rated resin with good impact strength.Data provided by the manufacturer |
|||
Tensile Strength, Ultimate | 48.0 MPa | 6960 psi | ATSM D638 |
Ashley Polymers Ashlene® PB261WO PPO A general purpose flame retardant resin for injection molding.Data provided by the manufacturer |
|||
Tensile Strength, Ultimate | 48.0 MPa | 6960 psi | Dynamic tensile strength |
Channel Industries 5800 Lead Zirconate Titanate Piezoelectric Characterized by high coupling factors and high piezoelectric and dielectric constants over extended temperature ranges and stress amplitudes, lead zirconate titanates are the most extensively used .. |
|||
Tensile Strength, Ultimate | 48.0 MPa | 6960 psi | ASTM D638 |
A. Schulman ComAlloy Comtuf® 604 Nylon 6/6, Impact Modified, Flow Enhanced Data provided by the manufacturer, ComAlloy International Company. Superior toughness and impact resistance characterize Comtuf® materialsThe ComAlloy product line has been integrated into the A Sc.. |
|||
Tensile Strength, Ultimate | 48.0 MPa | 6960 psi | ATSM D638 |
Ashley Polymers Ashlene® 847 Nylon 6, Film Grade A very high impact, low flexural modulus Nylon 6 resin for molding or extrusion. Outstanding low temperature properties.Data provided by the manufacturer |
|||
Tensile Strength, Ultimate | 48.0 MPa | 6960 psi | Dynamic tensile strength |
Channel Industries 5804 Lead Zirconate Titanate Piezoelectric Navy Type IIICharacterized by high coupling factors and high piezoelectric and dielectric constants over extended temperature ranges and stress amplitudes, lead zirconate titanates are the most exte.. |
|||
Tensile Strength, Ultimate | 48.0 MPa | 6960 psi | ISO 527B |
Ineos Nova 202 Crystal Polystyrene High Heat Extrusion Grade
(discontinued **) Excellent heat resistance, Fast cyclingApplications: XPS food packaging, Foam insulation, CD boxes, medical and food disposables, Sheet and profile extrusionProperties were determined on injection m.. |
|||
Tensile Strength, Ultimate | 48.0 MPa | 6960 psi | ASTM D651 |
Resinoid 1312 Phenolic Molding, Glass Reinforced Data provided by the manufacturer.The Resinoid 1300 and 7000 glass fiber reinforced series compounds feature mechanical strength, dimensional stability, electrical insulation, and heat resistance |
|||
Tensile Strength, Ultimate | 48.0 MPa | 6960 psi | ASTM D638 |
Kleerdex Kydex® 107 Acrylic/PVC Thermoplastic Sheet
(discontinued **) High performance sheet for NSFApplications: Ice makers, vending machines, beverage dispensers, and other equipment requiring NSF approval, as a replacement for stainless steel parts where cost, weig.. |
|||
Tensile Strength, Ultimate | 48.0 MPa | 6960 psi | ASTM D638 |
Plaslok 5314 Black (INJ) Impact Grade Phenolic Molding Compound
(discontinued **) Plaslok Corporation was purchased by Plastics Engineering Company (maker of Plenco brand materials) in March 2000. The Plaslok name is no longer in use.Plaslok 5314 is the replacement material for .. |
|||
Tensile Strength, Ultimate | 48.0 MPa | 6960 psi | ATSM D638 |
Ashley Polymers Ashlene® P258 PPO A high flow grade for applications requiring good impact strength and a high heat deflection temperature.Data provided by the manufacturer |
|||
Tensile Strength, Ultimate | 48.0 MPa | 6960 psi | ASTM D651 |
Resinoid 2020 Phenolic Molding, Fabric Reinforced Data provided by the manufacturer.The Resinoid 2000 organic fiber reinforced series compounds feature mechanical strength, dimensional stability, and shock resistance |