Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 41.4 MPa | 6000 psi | |
Mykroy/Mycalex MM 400 Machining Grade Glass-bonded Mica Composite Natural mica filler. Does not burn. Good radiation resistance (3 x 10^10 Rads-Cobalt).This ceramoplastic material is a versatile and efficient insulating material designed to meet the exacting dem.. |
|||
Tensile Strength, Ultimate | 41.4 MPa | 6000 psi | |
Mykroy/Mycalex MM 500 Machining Grade Glass-bonded Mica Composite Synthetic mica filler. Does not burn. Better radiation resistance (3 x 10^10 Rads-Cobalt) than grade 400.This ceramoplastic material is a versatile and efficient insulating material designed to me.. |
|||
Tensile Strength, Ultimate | 41.4 MPa | 6000 psi | ASTM D412 |
5187 Polyurethane-based Biomedical Elastomer |
|||
Tensile Strength, Ultimate | 41.4 MPa | 6000 psi | ASTM D412 |
5265 Polyurethane-based Biomedical Elastomer |
|||
Tensile Strength, Ultimate | 41.4 MPa | 6000 psi | Type 1 - Rigids, 0.2 in/min; ASTM D638 |
PolyOne Lubri-Tech™ PS-15GB/15T Polybutylene Terephthalate (PBT), Glass Bead Filled, PTFE Lubricated
(discont Description/Features:Glass Bead FilledPTFE LubricatedPolyOne First ChoiceInformation provided by PolyOne Corporation. |
|||
Tensile Strength, Ultimate | 41.4 - 79.3 MPa | 6000 - 11500 psi | Average value: 64.1 MPa Grade Count:5 |
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Glass Fiber Filled, Flame Retardant This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), Glass Fiber Filled, Flame Retardant". Each property range of valu.. |
|||
Tensile Strength, Ultimate | 41.4 MPa | 6000 psi | Type 1 - Rigids, 0.2 in/min; ASTM D638 |
PolyOne Edgetek® AS-20GF/000 FR Acrylonitrile Butadiene Styrene (ABS), Glass Filled
(discontinued **) Description/Features:Glass Fiber ReinforcedPolyOne First ChoiceInformation provided by PolyOne Corporation. |
|||
Tensile Strength, Ultimate | 41.4 MPa | 6000 psi | ASTM D638-95 |
Multibase Multi-ABS 3832 Natural Multi-ABS 3832 is specially formulated for ease of processability, controllability, and thin-walled parts where higher than normal temperatures are being used. This product also shows higher than n.. |
|||
Tensile Strength, Ultimate | 41.4 MPa | 6000 psi | ASTM Data |
Styron Magnum™ 341 ABS, Low Gloss MAGNUM® ABS resins are thermoplastic materials which provide an excellent balance of processability, impact resistance and heat resistance as imparted by the various polymer compositions. MAGNUM .. |
|||
Tensile Strength, Ultimate | 41.4 MPa | 6000 psi | ASTM D412 |
Lubrizol Estane® ALR PC85A Thermoplastic Polyurethane Type: Estane® ALR PC85A is a polycarbonate diol based thermoplastic polyurethane (TPU).Features: Hydrolytically stable, very durableAvailable in Americas, Europe, Middle East, Africa, India and Asi.. |
|||
Tensile Strength, Ultimate | 41.4 MPa | 6000 psi | ASTM D638 |
Ecomass® 1080BI64 Filled Polyamide Nontoxic alternative compound for weighting, balancing and radiation shielding applicationsModerate Specific GravityFilled Polyamide (PA) AlloyExcellent ToughnessInformation provided by Technical Po.. |
|||
Tensile Strength, Ultimate | 41.4 MPa | 6000 psi | ASTM D638 |
Ecomass® 1080ZG90 Metal Filled Polyamide Nontoxic alternative to Lead (Pb), weighting, balancing and radiation shielding applications.High Specific GravityMetal Powder Filled Polyamide (PA) AlloyExcellent ToughnessInformation provided by T.. |
|||
Tensile Strength, Ultimate | 41.4 MPa | 6000 psi | ASTM D1708 |
DSM Biomedical BioSpan® SPU Segmented Polyether Polyurethane (SPU) The flex life exhibited by BioSpan® SPU enables good performance in many different types of medical devices. This elastomeric polymer has shown the ability to withstand millions of flex cycles.The .. |
|||
Tensile Strength, Ultimate | 41.4 MPa | 6000 psi | ETFE film property; ASTM D638 |
Arlon 25188T010 Silicone Rubber/Laminated ETFE Film Liner: 3 mil PTFE coated fiberglass; Side 1: uncured silicone rubber; Substrate: laminated ETFE film, treated for adhesion |
|||
Tensile Strength, Ultimate | 41.4 MPa | 6000 psi | ASTM D638 |
Buckeye Polymers BP ABS 4332 ABS Low GlossABS is a copolymer of acrylonitrile and styrene, modified with butadiene rubber. ABS is primarily used for their combination of toughness, rigidity, chemical resistance, ease of processing.. |
|||
Tensile Strength, Ultimate | 41.4 - 55.2 MPa | 6000 - 8000 psi | |
Bulk Molding Compounds BMC 5209 Mineral Filled, Glass Reinforced Polyester BMC 5209 molding compound is a mineral filled, glass fiber-reinforced polyester compound suitable for compression, transfer and stuffer injection molding. It is a high impact material produced in ex.. |
|||
Tensile Strength, Ultimate | 41.4 - 55.2 MPa | 6000 - 8000 psi | |
Bulk Molding Compounds BMC 605L Mineral Filled, Glass Fiber Reinforced Polyester Compound BMC 605L molding compound is a low cost, mineral filled, glass-fiber-reinforced polyester compound suitable for compression, transfer and stuffer injection molding. It is characterized by good molda.. |
|||
Tensile Strength, Ultimate | 41.4 - 55.2 MPa | 6000 - 8000 psi | |
Bulk Molding Compounds BMC 605LS Mineral Filled, Glass Fiber Reinforced Polyester Compound BMC 605LS molding compound is a low-shrink, mineral filled, glass-fiber-reinforced polyester compound suitable for compression, transfer and stuffer injection molding It is characterized by good mol.. |
|||
Tensile Strength, Ultimate | 41.4 - 55.2 MPa | 6000 - 8000 psi | |
Bulk Molding Compounds BMC 615 Mineral Filled, Glass Fiber Reinforced Polyester Compound BMC 615 molding compound is a mineral filled, glass fiber-reinforced polyester compound suitable for compression, transfer and stuffer injection molding. It is a high impact material produced in ext.. |
|||
Tensile Strength, Ultimate | 41.4 - 51.7 MPa | 6000 - 7500 psi | Conditioned 7 days at RT/50% RH; ASTM D638 |
AdvanSource Biomaterials ChronoFlex® C 55D Biodurable Medical Grade Polyurethane ChronoFlex® C is a family of premium polycarbonate aromatic biodurable thermoplastic polyurethane elastomers developed by AdvanSource Biomaterials Corporation. ChronoFlex® C medical-grade elastome.. |
|||
Tensile Strength, Ultimate | 41.4 - 48.3 MPa | 6000 - 7000 psi | |
Bulk Molding Compounds BMC 1412 Flame and Track Resistant BMC 1412 is an extremely versatile material. Flame and track resistant, low shrink for close dimensional control and surface smoothness, high physical properties. Developed for injection molding, bu.. |
|||
Tensile Strength, Ultimate | 41.4 MPa | 6000 psi | |
Dymax 3086 Solvent-Free Plastic Adhesive Solvent-Free Adhesives for Plastic Assembly in SecondsDymax® Light-Weld® and Ultra 3000 Series UV and UV/Visible Curing Adhesives for plastic assembly provide instant durable bonds to cure a wide .. |
|||
Tensile Strength, Ultimate | 41.4 - 64.0 MPa | 6000 - 9280 psi | Average value: 53.1 MPa Grade Count:22 |
Overview of materials for Acetal Homopolymer, PTFE-Filled This property data is a summary of similar materials in the MatWeb database for the category "Acetal Homopolymer, PTFE-Filled". Each property range of values reported is minimum and maximum values o.. |
|||
Tensile Strength, Ultimate | 41.4 MPa | 6000 psi | TM R050-36 |
Resinlab® EP1285HD-14 Highly Filled, Medium Viscosity Casting Resin Resinlab™ EP1285 (Formerly Lab Product W021901 series) is a highly filled, medium viscosity black casting resin designed for applications requiring a high degree of thermal conductivity and a low C.. |