Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 37.0 MPa | 5370 psi | ISO 527 |
Premix Thermoplastics PRE-ELEC® PBT 1455 PRE-ELEC PBT 1455 is a conductive thermoplastic compound based on PBT. Conductivity is achieved by using special conductive carbon black. PRE-ELEC PBT 1455 has excellent mechanical properties as wel.. |
|||
Tensile Strength, Ultimate | 37.0 MPa | 5370 psi | ISO 527 |
LATI LATAN 13 S/30 30% Glass Sphere Reinforced Polyoxymethylene Copolymer (POM)
(Unverified Data**) Description: Latan series thermoplastics are polyoxymethylene copolymer (POM) products. The main applications for Latan feature good wear resistance, chemical inertness and low water absorption (gea.. |
|||
Tensile Strength, Ultimate | 37.0 MPa | 5370 psi | ASTM D638 |
Global GA-3245 High Density Polyethylene, Film Extrusion Grade
(discontinued **) Description-opacity, medium high stiffness, good impact strength, good chemical resistanceApplications- shopping bags, packing bagsInformation provided by Global Polymers Corporation. |
|||
Tensile Strength, Ultimate | 37.0 MPa | 5370 psi | ASTM D638 |
Solvay Specialty Polymers Algoflon® S 111 PTFE (Polytetrafluoroethylene)
(discontinued **) Data provided by the manufacturer.Type IV.G.1 Classification. Suspension polymer powder grade recommended for compression molding and extrusion. PTFE possesses high inertness, excellent dielectric p.. |
|||
Tensile Strength, Ultimate | 37.0 - 74.0 MPa | 5370 - 10700 psi | Average value: 58.8 MPa Grade Count:4 |
Overview of materials for Ethylene Vinyl Alcohol (EVOH) This property data is a summary of similar materials in the MatWeb database for the category "Ethylene Vinyl Alcohol". Each property range of values reported is minimum and maximum values of appropr.. |
|||
Tensile Strength, Ultimate | 37.0 MPa | 5370 psi | |
Kuraray HYBRAR® PH5 Polypropylene Blend Description: HYBRAR® is another in the series of new high performance thermoplastic rubbers developed by KURARAY using their unique isoprene technology. HYBRAR® is a special thermoplastic rubb.. |
|||
Tensile Strength, Ultimate | 37.0 MPa @Temperature 22.0 °C |
5370 psi @Temperature 71.6 °F |
25mm flat samples, compression moulded; ISO 527-4 |
Menzolit Menzolit® BMC 1400 Unsaturated Polyester UP BMC 1400 is a special BMC for the use on an engine. The glass content is set to a level that combines good mouldability with good strength and stiffness properties. The product has been developped f.. |
|||
Tensile Strength, Ultimate | 37.0 MPa | 5370 psi | ASTM D638 |
Stratasys® ABSi Stratasys is the only company that gives engineers the ability to manufacture real ABSi industrial thermoplastic parts direct from digital files. ABSi parts can be used from conceptual prototyping t.. |
|||
Tensile Strength, Ultimate | 37.0 MPa | 5370 psi | 2 in/min, at max load; ASTM D638 |
A. Schulman POLYPUR™ CB 1110 Thermoplastic Polyurethane Compound Information provided by A. Schulman. |
|||
Tensile Strength, Ultimate | 37.0 - 50.0 MPa | 5370 - 7250 psi | ASTM D638 |
Zeus ETFE Tubing ETFE (Ethylenetetrafluoroethylene), a copolymer of ethylene and tetrafluoroethylene, is used in applications requiring excellent impact, abrasion and stress cracking resistance. This polymer possess.. |
|||
Tensile Strength, Ultimate | 37.0 MPa | 5370 psi | 2 in/min, at max load; ASTM D638 |
A. Schulman POLYPUR™ CB 1110 Thermoplastic Polyurethane Compound Information provided by A. Schulman. |
|||
Tensile Strength, Ultimate | 37.0 MPa | 5370 psi | DIN 53504 |
Lubrizol ESTANE® 58610 Ester Based Thermoplastic Polyurethane (European Grade) Description: Estane® thermoplastic polyurethanes (TPUs) include elastomeric materials that bridge the gap between flexible rubber and rigid plastics. These materials offer toughness and durability .. |
|||
Tensile Strength, Ultimate | 37.0 MPa | 5370 psi | DIN 53504 |
Lubrizol ESTANE® ETE50DT3 Ester Based Thermoplastic Polyurethane (European Grade) Description: Estane® thermoplastic polyurethanes (TPUs) include elastomeric materials that bridge the gap between flexible rubber and rigid plastics. These materials offer toughness and durability .. |
|||
Tensile Strength, Ultimate | 37.0 MPa | 5370 psi | DIN 53504 |
Lubrizol ESTANE® 54610 Ester Based Thermoplastic Polyurethane (European Grade) Description: Estane® thermoplastic polyurethanes (TPUs) include elastomeric materials that bridge the gap between flexible rubber and rigid plastics. These materials offer toughness and durability .. |
|||
Tensile Strength, Ultimate | 37.0 MPa | 5370 psi | DIN 53504 |
Lubrizol ESTANE® 5702F2 Ester Based Thermoplastic Polyurethane (European Grade) Description: Estane® thermoplastic polyurethanes (TPUs) include elastomeric materials that bridge the gap between flexible rubber and rigid plastics. These materials offer toughness and durability .. |
|||
Tensile Strength, Ultimate | 37.0 MPa | 5370 psi | ISO 527 |
DSM Fibre Intermediates Nyrim® 3000 (Dry) Nyrim is a Block Copolymer of Nylon 6 and an elastomer with exceptional properties in impact resistance, fatigue and abrasion resistance. Nyrim is processed via Reaction Injection Moulding (RIM) tec.. |
|||
Tensile Strength, Ultimate | 37.0 MPa | 5370 psi | ASTM D638 |
DuPont™ Surlyn® 8140 Ionomer Resin, Sodium Surlyn® 8140 thermoplastic resin is an advanced ethylene/methacrylic acid (E/MAA) copolymer, in which the MAA acid groups have been partially neutralized with sodium ions. The amount of MAA and neu.. |
|||
Tensile Strength, Ultimate | 37.0 MPa | 5370 psi | ISO R527 |
Arkema Group ORGASOL® 2002 D Nat 1 Polyamide 12, Food Contact Approved Information provided by Arkema Group |
|||
Tensile Strength, Ultimate | 37.0 MPa | 5370 psi | ASTM D412 |
BASF Elastollan® C-78A Polyester Type Polyurethane Elastomer Processed by extrusion or injection molding. Elastollan C series of products are polyester-based thermoplastic polyurethanes that exhibit very good hydrolytic stability. They also exhibit excellen.. |
|||
Tensile Strength, Ultimate | 37.0 MPa | 5370 psi | |
Alliance BCN-13 Bonded (Composite) Magnetic Material |
|||
Tensile Strength, Ultimate | 37.0 MPa | 5370 psi | Z; ASTM D638 |
ALM PA 605-A Filled Nylon 12 Prototyping Polymer 50% Aluminum filled nylon 12 that can produce accurate parts with excellent part strength and surface detail.Drop in replacement for other commercially available 50% aluminum filled materials with a.. |
|||
Tensile Strength, Ultimate | 37.0 MPa | 5370 psi | Z; ASTM D638 |
ALM PA-840-GSL Filled Nylon 12 Prototyping Polymer Engineered for excellent mechanical properties, part definition and surface finish.Stabilized against thermal degradation resulting in little or no scrap material, with typical virgin refresh rates .. |
|||
Tensile Strength, Ultimate | 37.0 MPa @Temperature 1204 °C |
5370 psi @Temperature 2199 °F |
|
ATI Allegheny Ludlum Altemp® HX Nickel-Based superalloy Characteristics: outstanding resistance to oxidation at high temperatures, exceptional strength at elevated temperatures, good fabricability, good machinability in annealed condition, work hardening.. |
|||
Tensile Strength, Ultimate | 37.0 MPa | 5370 psi | |
Alliance BCN-10 Bonded (Composite) Magnetic Material |
|||
Tensile Strength, Ultimate | 37.0 MPa | 5370 psi | |
Alliance BCN-14 Bonded (Composite) Magnetic Material |
|||
Tensile Strength, Ultimate | 37.0 MPa | 5370 psi | |
Alliance BCN-15 Bonded (Composite) Magnetic Material |
|||
Tensile Strength, Ultimate | 37.0 MPa | 5370 psi | |
Alliance BCN-17 Bonded (Composite) Magnetic Material |
|||
Tensile Strength, Ultimate | 37.0 MPa | 5370 psi | 2 in/min, at max load; ASTM D638 |
A. Schulman POLYPUR™ CB 1110 Thermoplastic Polyurethane Compound Information provided by A. Schulman. |
|||
Tensile Strength, Ultimate | 37.0 MPa | 5370 psi | ASTM D638 |
Plenco 7591 Phenolic, Pellet, Transfer Molded PLENCO 07591 is a mineral and flock cotton filled novolac phenolic molding compound. UL recognized under component file E40654.Information supplied by Plenco. |