Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Lubrizol ESTANE® ETE50DT3 Ester Based Thermoplastic Polyurethane (European Grade)

Category Polymer , Thermoplastic , Elastomer, TPE , Polyurethane, TP , Thermoplastic Polyurethane, Elastomer, Ether Grade
Manufacturer Lubrizol (former Noveon)
Trade Name ESTANE®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Lubrizol ESTANE® ETE50DT3 Ester Based Thermoplastic Polyurethane (European Grade).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: Estane® thermoplastic polyurethanes (TPUs) include elastomeric materials that bridge the gap between flexible rubber and rigid plastics. These materials offer toughness and durability in a flexible thermoplastic elastomer system that is easy to process in a wide range of equipment. The Estane® TPU portfolio of products offers high performance polyester - and polyether - based resins and compounds in a broad range of hardnesses to meet a variety of application needs.Benefits of Estane® TPU: Outstanding Abrasion and Wear ResistanceExcellent Low Temperature FlexibilitySuperior Toughness and DurabilityEase of Processing and Manufacturing FlexibilityColorability and Paintability with no adhesion promoterApplications: Film & SheetFabric coating & melt coatingWire & CableHose, Tube & ProfileCustom moldingCustom compoundingAutomotive interior/chassis and exterior painted trimSpecific Notes for this Material: Excellent extrusion, processability, low temperature flexibility, good clarity, substrate for overmolding Information provided by Noveon, Inc.
Physical Properties Metric English Comments
Specific Gravity 1.15 g/cc
1.15 g/cc
DIN 53479
Mechanical Properties Metric English Comments
Hardness, Shore D 50
50
DIN 53505
Tensile Strength, Ultimate 37.0 MPa
5370 psi
DIN 53504
Elongation at Break 515 %
515 %
DIN 53504
50% Modulus 0.0100 GPa
1.45 ksi
DIN 53504
100% Modulus 0.0118 GPa
1.71 ksi
DIN 53504
300% Modulus 0.0205 GPa
2.97 ksi
DIN 53504
Flexural Stiffness 70.002 MPa
10153 psi
ASTM D747
Tear Strength 105 kN/m
599 pli
DIN 53515
Abrasion 81
81
mm<sup>3</sup>; DIN 53516
Thermal Properties Metric English Comments
Vicat Softening Point 85.0 °C
185 °F
A50; DIN 53460
Descriptive Properties Value Comments
E-Modulus 63 mm/min