Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 117 MPa | 17000 psi | ASTM D638 |
Nylene® Naxel™ PC506 30% Glass Reinforced Polycarbonate Description: Naxel™ PC506 is a 30% glass fiber reinforced polycarbonate. Information provided by Custom Resins. ALM, Nylene Canada, and Custom Resins are all operting companies of Polymeric Resourc.. |
|||
Tensile Strength, Ultimate | 117 MPa | 17000 psi | ASTM D638 |
Nylene® Vexel™ B12GF30 , 30% Glass Reinforced PBT Description: Vexel™ B12GF30 is a 30% glass fiber reinforced, general purpose PBT. Information provided by Custom Resins. ALM, Nylene Canada, and Custom Resins are all operting companies of Polymeri.. |
|||
Tensile Strength, Ultimate | 117 MPa | 17000 psi | ASTM D638 |
Nylene® Vexel™ B12GF30 FR , 30% Glass Reinforced, Flame Retardant PBT Description: Vexel™ B12GF30 FR is a 30% glass fiber reinforced, flame retardant PBT. B12GF30 FR is UL approved. Information provided by Custom Resins. ALM, Nylene Canada, and Custom Resins are all .. |
|||
Tensile Strength, Ultimate | 117 MPa @Thickness 3.17 mm |
17000 psi @Thickness 0.125 in |
ASTM D638 |
PTS Trimid® N66-G13L 13% Glass Fiber Reinforced Lubed Nylon 6/6 Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Tensile Strength, Ultimate | 117 - 186 MPa | 17000 - 27000 psi | Average value: 158 MPa Grade Count:17 |
Overview of materials for Polyetherimide (PEI), 30% Glass Fiber This property data is a summary of similar materials in the MatWeb database for the category "Polyetherimide, 30% Glass Fiber". Specific grades with glass content between 25% and 34% are included. E.. |
|||
Tensile Strength, Ultimate | 117 MPa | 17000 psi | ASTM D638 |
Solvay Specialty Polymers Radel® R-7120 Polyphenylsulfone, 20% glass fiber
(discontinued **) RADEL R 7120 is a 20% glass fiber reinforced grade of RADEL R polyphenylsulfone developed specifically for aircraft interior applications. The product complies with the FAA regulation 14CFR Part 25 .. |
|||
Tensile Strength, Ultimate | 117 MPa | 17000 psi | Type 1 - Rigids, 0.2 in/min; ASTM D638 |
PolyOne Edgetek® NJ-30GF/000 Nylon 12, Glass Filled
(discontinued **) Description/Features:Glass Fiber ReinforcedInformation provided by PolyOne Corporation. |
|||
Tensile Strength, Ultimate | 117 MPa | 17000 psi | ASTM D638 |
IDI Composites A-207 Thermoset Polyester, Sheet AUTOMOTIVE - Versatile family of compounds specifically designed for automotive structural applications. Low shrink characteristics, heat resistance, long-term dimensional stability, and corrosion r.. |
|||
Tensile Strength, Ultimate | 117 MPa | 17000 psi | |
Haysite HCR-197 Corrosion Resistant Polyester/Glass Sheet A fiber glass reinforced thermoset polyester sheet using ATLAC® 382 Bisphenol-A Fumarate in the resin matrix. Standard color is light yellow. Additional data covering resistance to specific chemi.. |
|||
Tensile Strength, Ultimate | 117 MPa | 17000 psi | ASTM D638 |
Techmer ES Electrafil® J-50/CF/30/TF/13/SI/2 Polycarbonate, 30% Carbon Fiber Reinforced, 13% PTFE, 2% Silicone |
|||
Tensile Strength, Ultimate | 117 MPa | 17000 psi | ISO 527-1, 2 |
Polyplastics Duranex® 7407 Polybutylene Terephthalate (PBT), Super low warpage, GF filled DURANEX® is a crystalline thermoplastic based on polybutylene terephthalate (PBT) that can be readily strengthened, modified, or otherwise performance enhanced through the addition of glass fibers .. |
|||
Tensile Strength, Ultimate | 117 MPa @Temperature 704 °C |
17000 psi @Temperature 1300 °F |
|
Crucible Steel 446 Chromium Steel Crucible 446 is a non-hardenable chromium steel which has the highest corrosion and heat resisting properties of the straight chromium steels. This grade is magnetic at all times. Information provi.. |
|||
Tensile Strength, Ultimate | 117 MPa | 17000 psi | ASTM D638 |
Adell BR-14 Nylon 6, 20% Glass Reinforced Data provided by Adell Plastics, Inc. |
|||
Tensile Strength, Ultimate | 117 MPa | 17000 psi | ASTM D638 |
Adell BR-34 Nylon 6, 20% Glass Reinforced Data provided by Adell Plastics, Inc. |
|||
Tensile Strength, Ultimate | 117 MPa | 17000 psi | ATSM D638 |
Ashley Polymers Ashlene® 630-13G Nylon 6, 13% Glass Reinforced A 13% glass fiber reinforced Nylon 6, designed to provide a high flexural modulus and good dimensional stability, while maintaining the ease of processing associated with Nylon 6 type materials.Data.. |
|||
Tensile Strength, Ultimate | 117 MPa | 17000 psi | ASTM D638 |
A. Schulman ComAlloy Hiloy® 513 Polycarbonate, Glass Reinforced, UL Data provided by the manufacturer, ComAlloy International Company.30% Glass Reinforced.The ComAlloy product line has been integrated into the A Schulman product line. |
|||
Tensile Strength, Ultimate | 117 MPa | 17000 psi | 5mm/min; ISO 527 |
BASF Ultradur B 4406 G4 Q113 20% Glass Filled PBT Ultradur B4406 G4 Q113 is an UL V0 injection molding PBT grade with 20% glass fiber reinforcement. |
|||
Tensile Strength, Ultimate | 117 MPa | 17000 psi | ATSM D638 |
Ashley Polymers Ashlene® 1430 Polycarbonate, 30% Glass Reinforced A 30% glass reinforced polycarbonate for increased mechanical strength and thermal properties. Also available with UV stabilizer. 1433: with UV stabilizer; 1433-H2: with improved UV stabilizer.Dat.. |
|||
Tensile Strength, Ultimate | 117 MPa | 17000 psi | ASTM D638 |
A. Schulman ComAlloy Comtuf® 615 Nylon 6, Glass Reinforced, Impact Modified Data provided by the manufacturer, ComAlloy International Company.45% Glass Reinforced. Superior toughness and impact resistance characterize Comtuf® materialsThe ComAlloy product line has been int.. |
|||
Tensile Strength, Ultimate | 117 MPa | 17000 psi | ASTM D638 |
Techmer ES Plaslube® J-50/30/TF/15 Polycarbonate, 30% Glass Reinforced, PTFE Lubricated 30% Glass Reinforced, PTFE Lubricated |
|||
Tensile Strength, Ultimate | 117 MPa | 17000 psi | ASTM D638 |
PolyOne Edgetek® ES-06CF-09GF/000 RED Polyethersulfone - 6% Carbon - 9% Glass Fiber Reinforced - ESD Applications
& Data provided by PolyOne. |