Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Dart Drop, Total Energy = 64.2 ft-lb Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Dart Drop, Total Energy 87.0 J

@Thickness 3.20 mm
64.2 ft-lb

@Thickness 0.126 in
203m/min; ASTM D3763
LG Chemical Lupoy 1200-10 Polycarbonate Resin
Description: LUPOY PC 1200-10 resin is designed for extrusion and injection molding products. It exhibits an excellent physical property balance of heat resistance, transparency and impact strength...
Dart Drop, Total Energy 87.0 J

@Thickness 3.20 mm
64.2 ft-lb

@Thickness 0.126 in
203m/min; ASTM D3763
LG Chemical Lupoy 1200-15 Polycarbonate Resin
Description: LUPOY PC 1200-15 resin is designed for extrusion and injection molding products. It exhibits an excellent physical property balance of heat resistance, transparency and impact strength...
Dart Drop, Total Energy 87.0 J

@Thickness 3.20 mm
64.2 ft-lb

@Thickness 0.126 in
203m/min; ASTM D3763
LG Chemical Lupoy 1201-10 Polycarbonate Resin
Description: LUPOY PC 1201-10 resin is designed for extrusion and injection molding products. It exhibits an excellent physical property balance of heat resistance, transparency and impact strength...
Dart Drop, Total Energy 87.0 J

@Thickness 3.20 mm
64.2 ft-lb

@Thickness 0.126 in
203m/min; ASTM D3763
LG Chemical Lupoy 1201-15 Polycarbonate Resin
Description: LUPOY PC 1201-15 resin is designed for extrusion and injection molding products. It exhibits an excellent physical property balance of heat resistance, transparency and impact strength...
Dart Drop, Total Energy 87.0 J

@Thickness 3.20 mm
64.2 ft-lb

@Thickness 0.126 in
203m/min; ASTM D3763
LG Chemical Lupoy 1300-15 Polycarbonate Resin
Description: LUPOY PC 1300-15 resin is designed for extrusion and injection molding products. It exhibits an excellent physical property balance of heat resistance, transparency and impact strength...
Dart Drop, Total Energy 87.0 J

@Thickness 3.20 mm
64.2 ft-lb

@Thickness 0.126 in
203m/min; ASTM D3763
LG Chemical Lupoy 1301-12 Polycarbonate Resin
Description: LUPOY PC 1301-12 resin is designed for extrusion and injection molding products. It exhibits an excellent physical property balance of heat resistance, transparency and impact strength...
Dart Drop, Total Energy 87.0 J

@Thickness 3.20 mm
64.2 ft-lb

@Thickness 0.126 in
203m/min; ASTM D3763
LG Chemical Lupoy 1301V-10 Polycarbonate Resin
Description: LUPOY PC 1301V-10 resin is designed for extrusion and injection molding products. It exhibits an excellent physical property balance of heat resistance, transparency and impact strength..
Dart Drop, Total Energy 87.0 J

@Thickness 3.20 mm
64.2 ft-lb

@Thickness 0.126 in
203m/min; ASTM D3763
LG Chemical Lupoy 3010-10 Polycarbonate Resin
Description: LUPOY PC 3010-10 resin is designed for injection molding products. It exhibits an excellent physical property balance of heat resistance, transparency and impact strength.Main Character..
Dart Drop, Total Energy 87.0 J

@Thickness 3.20 mm
64.2 ft-lb

@Thickness 0.126 in
203m/min; ASTM D3763
LG Chemical Lupoy 3010-22 Polycarbonate Resin
Description: LUPOY PC 3010-22 resin is designed for injection molding products. It exhibits an excellent physical property balance of heat resistance, transparency and impact strength.Main Character..
Dart Drop, Total Energy 87.0 J

@Thickness 3.20 mm
64.2 ft-lb

@Thickness 0.126 in
203m/min; ASTM D3763
LG Chemical Lupoy 3030-10 Polycarbonate Resin
Description: LUPOY PC 3030-10 resin is designed for injection molding products. It exhibits an excellent physical property balance of heat resistance, transparency and impact strength.Main Character..
Dart Drop, Total Energy 87.0 J

@Thickness 3.20 mm
64.2 ft-lb

@Thickness 0.126 in
203m/min; ASTM D3763
LG Chemical Lupoy 3030-15 Polycarbonate Resin
Description: LUPOY PC 3030-15 resin is designed for injection molding products. It exhibits an excellent physical property balance of heat resistance, transparency and impact strength.Main Character..
Dart Drop, Total Energy 87.0 J

@Thickness 3.20 mm
64.2 ft-lb

@Thickness 0.126 in
203m/min; ASTM D3763
LG Chemical Lupoy NF1007F 10R Polycarbonate Resin
Description: LUPOY NF 1007F10R, eco-friendly UL94 V0/3.0 mm, is designed for extrusion and injection molding products. It combines an excellent physical property balance of heat resistance, transpar..
Dart Drop, Total Energy 87.0 J

@Thickness 3.20 mm
64.2 ft-lb

@Thickness 0.126 in
203m/min; ASTM D3763
LG Chemical Lupoy NF1009F 15 Polycarbonate Resin
Description: LUPOY NF 1009F15, eco-friendly UL94 V0/2.0 mm, is designed for extrusion and injection molding products. It combines an excellent physical property balance of heat resistance, transpare..
Dart Drop, Total Energy 87.0 J

@Thickness 3.20 mm
64.2 ft-lb

@Thickness 0.126 in
203m/min; ASTM D3763
LG Chemical Lupoy 1200HP-15 Polycarbonate Resin
Description: LUPOY PC 1200HP-15 resin is designed for extrusion and injection molding products. It exhibits an excellent physical property balance of heat resistance, transparency and impact strengt..
Dart Drop, Total Energy 87.0 J

@Thickness 3.20 mm
64.2 ft-lb

@Thickness 0.126 in
203m/min; ASTM D3763
LG Chemical Lupoy 1300-10 Polycarbonate Resin
Description: LUPOY PC 1300-10 resin is designed for extrusion and injection molding products. It exhibits an excellent physical property balance of heat resistance, transparency and impact strength...
Dart Drop, Total Energy 87.0 J

@Thickness 3.20 mm
64.2 ft-lb

@Thickness 0.126 in
203m/min; ASTM D3763
LG Chemical Lupoy 1300-12 Polycarbonate Resin
Description: LUPOY PC 1300-12 resin is designed for extrusion and injection molding products. It exhibits an excellent physical property balance of heat resistance, transparency and impact strength...
Dart Drop, Total Energy 87.0 J

@Thickness 3.20 mm
64.2 ft-lb

@Thickness 0.126 in
203m/min; ASTM D3763
LG Chemical Lupoy 1302-10 Polycarbonate Resin
Description: LUPOY PC 1302-10 resin is designed for extrusion and injection molding products. It exhibits an excellent physical property balance of heat resistance, transparency and impact strength...
Dart Drop, Total Energy 87.0 J

@Thickness 3.20 mm
64.2 ft-lb

@Thickness 0.126 in
203m/min; ASTM D3763
LG Chemical Lupoy 1303-15 Polycarbonate Resin
Description: LUPOY PC 1303-15 resin is designed for extrusion and injection molding products. It exhibits an excellent physical property balance of heat resistance, transparency and impact strength...
Dart Drop, Total Energy 87.0 J

@Thickness 3.20 mm
64.2 ft-lb

@Thickness 0.126 in
203m/min; ASTM D3763
LG Chemical Lupoy 1303AH-10 Polycarbonate Resin
Description: LUPOY PC 1303AH-10 Tint Polycarbonate Resin is designed for injection molding of auto-headlamps. It exhibits an excellent physical property balance of heat resistance, transparency and ..
Dart Drop, Total Energy 87.0 J

@Thickness 3.20 mm
64.2 ft-lb

@Thickness 0.126 in
203m/min; ASTM D3763
LG Chemical Lupoy 1303AH-15 Polycarbonate Resin
Description: LUPOY PC 1303AH-15 Tint Polycarbonate Resin is designed for injection molding of auto-headlamps. It exhibits an excellent physical property balance of heat resistance, transparency and ..
Dart Drop, Total Energy 87.0 J
64.2 ft-lb
3.39 m/sec; ASTM D3763
Styron CALIBREâ„¢ 201-15 Polycarbonate Resin
Overview: CALIBREâ„¢ 201-15 polycarbonate resins are produced in compliance with the US Food and Drug Administration (FDA) and EU food contact regulations. They provide excellent impact resistanc..
Dart Drop, Total Energy 87.0 J
64.2 ft-lb
8000 ipm; ASTM D3763
Styron CALIBREâ„¢ 2061-15 Polycarbonate
CALIBREâ„¢ 2061-15 resin is used in applications involving steam or ethylene oxide for sterilization - though suitability for use in these applications is dependent upon autoclave cycle times and..
Dart Drop, Total Energy 87.0 J

@Thickness 3.20 mm
64.2 ft-lb

@Thickness 0.126 in
203 m/min; ASTM D1822
Styron CALIBREâ„¢ 301-10 Polycarbonate
Information provided by DowThis product line was spun off from Dow Chemical to Styron in 2010.
Dart Drop, Total Energy 87.0 J

@Thickness 3.20 mm
64.2 ft-lb

@Thickness 0.126 in
203 m/min; ASTM D1822
Styron CALIBREâ„¢ 301-15 Polycarbonate
Information provided by DowThis product line was spun off from Dow Chemical to Styron in 2010.
Dart Drop, Total Energy 87.0 J
64.2 ft-lb
8000 ipm; ASTM D3763
Styron EMERGEâ„¢ 4310-10 Polycarbonate
EMERGEâ„¢ PC 4310-10 advanced resin is high-performance polycarbonate resin offering high heat resistance and maximum toughness. Applications: Consumer Electronics and Information Technology Eq..
Dart Drop, Total Energy 87.0 J
64.2 ft-lb
8000 ipm; ASTM D3763
Styron EMERGEâ„¢ 4330-10 Polycarbonate
EMERGEâ„¢ PC 4330-10 advanced resin is a polycarbonate resin offering ultraviolet light stability, high heat resistance and maximum toughness. Applications: Consumer Electronics and Information..
Dart Drop, Total Energy 87.0 J

@Thickness 3.20 mm
64.2 ft-lb

@Thickness 0.126 in
203 m/min; ASTM D1822
Styron CALIBREâ„¢ 201-15 Polycarbonate
Information provided by DowThis product line was spun off from Dow Chemical to Styron in 2010.
Dart Drop, Total Energy 87.0 J
64.2 ft-lb
3.39 m/sec; ASTM D3763
Styron CALIBREâ„¢ 300-10 Polycarbonate Resin
Overview: CALIBREâ„¢ 300-10 polycarbonate resin offer exceptional impact resistance, heat distortion resistance, and optical clarity. The CALIBREâ„¢ 300-10 series products are available in 4 a..
Dart Drop, Total Energy 87.0 J
64.2 ft-lb
3.39 m/sec; ASTM D3763
Styron CALIBREâ„¢ 302-10 Polycarbonate Resin
Overview: CALIBREâ„¢ 300-10 polycarbonate resins offer exceptional impact resistance, heat distortion resistance and optical clarity as well as high melt strength for blow molding and sheet appli..
Dart Drop, Total Energy 87.0 J
64.2 ft-lb
8000 ipm; ASTM D3763
Styron EMERGEâ„¢ 4310-15 Polycarbonate
EMERGEâ„¢ PC 4310-15 advanced resin is high-performance polycarbonate resin offering high heat resistance and maximum toughness. Applications: Consumer Electronics and Information Technology Eq..
Copyright © lookpolymers.com All Rights Reserved