Polymer Property : Dart Drop, Total Energy = 25.8 ft-lb Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Dart Drop, Total Energy 35.0 J

@Temperature 23.0 °C
25.8 ft-lb

@Temperature 73.4 °F
ASTM D3763
SABIC Innovative Plastics Cycolac® EX75 ABS
Multi-purpose, extrusion ABS providing a favorable balance of engineering properties.
Dart Drop, Total Energy 35.0 J

@Temperature 23.0 °C
25.8 ft-lb

@Temperature 73.4 °F
ASTM D3763
SABIC Innovative Plastics Cycolac® MG34LG ABS
Automotive: Low gloss ABS for unpainted interior applications.
Dart Drop, Total Energy 35.0 J

@Temperature 23.0 °C
25.8 ft-lb

@Temperature 73.4 °F
ASTM D3763
SABIC Innovative Plastics Cycolac® MG37EPX ABS
ABS plating grade optimized for a broad processing window for both painted and plated applications. NSF standard 61 compliant (80 sq in/L)
Dart Drop, Total Energy 35.0 J

@Temperature 23.0 °C
25.8 ft-lb

@Temperature 73.4 °F
ASTM D3763
SABIC Innovative Plastics GELOY XTWE265 ASA (Asia Pacific)
Highly weatherable Geloy ASA profile extrusion grade for processes with simple or no calibration hardware.
Dart Drop, Total Energy 35.0 J
25.8 ft-lb
ASTM D3029
SABIC Innovative Plastics Cycolac® BDT5510 ABS
Automotive. High heat resistance, low gloss, color concentratable for interior applications. Natural only.
Dart Drop, Total Energy 35.0 J

@Temperature 23.0 °C
25.8 ft-lb

@Temperature 73.4 °F
ASTM D3763
SABIC Innovative Plastics LNP LUBRICOMP DP001E PC
LNP* LUBRICOMP* DP001E is a Polycarbonate base resin containing 5% PTFE/Silicone. Added features are: Internally Lubricated, Easy Molding.
Dart Drop, Total Energy 35.0 J
25.8 ft-lb
Instrumented Impact Energy @ peak; ASTM D3763
SABIC Innovative Plastics PREVEX VGAX PPE+PS
Improved productivity and reliability. Nonchlorinated, nonbrominated flame retardant. 180F HDT.
Dart Drop, Total Energy 35.0 J

@Temperature 23.0 °C
25.8 ft-lb

@Temperature 73.4 °F
ASTM D3763
SABIC Innovative Plastics Valox® 357 PBT (Asia Pacific)
PBT + PC, Unreinforced, impact modified, UL94V-0 rated. Applications like bobbins, switches and enclosures.
Dart Drop, Total Energy 35.0 J

@Temperature 23.0 °C
25.8 ft-lb

@Temperature 73.4 °F
ASTM D3763
SABIC Innovative Plastics Valox® 357 PBT+PC
PC/PBT, Unreinforced, impact modified, UL94V-0 rated. Applications like bobbins, switches and enclosures.
Dart Drop, Total Energy 35.0 J

@Temperature 23.0 °C
25.8 ft-lb

@Temperature 73.4 °F
ASTM D3763
SABIC Innovative Plastics Valox® 357X PBT (Europe-Africa-Middle East)
VALOX 357X is an impact modified, flame retarted PBT+PC blend. Applications like bobbins, switches and enclosures.
Dart Drop, Total Energy 35.0 J

@Temperature 23.0 °C
25.8 ft-lb

@Temperature 73.4 °F
ASTM D3763
SABIC Innovative Plastics Valox® HX3091HP PBT
PBT for compounding/fibers only. Not intended for injection molding. Biocompatible. Melt viscosity at 250C and 21.6kgf is 3500-4500 poise. Available in Natural color (1001) only.
Dart Drop, Total Energy 35.0 J

@Temperature 23.0 °C
25.8 ft-lb

@Temperature 73.4 °F
ASTM D3763
SABIC Innovative Plastics LNP STAT-KON 9X02785 PC
LNP STAT-KON* 9X02785 is a compound based on Polycarbonate resin containing Proprietary Filler(s). Added feature of this material is: Electrically Conductive.
Dart Drop, Total Energy 35.0 J

@Temperature 23.0 °C
25.8 ft-lb

@Temperature 73.4 °F
ASTM D3763
SABIC Innovative Plastics LNP THERMOCOMP NF001XXX PC+ABS
LNP* THERMOCOMP* PCA-F-1001 is a compound based on PC+ABS resin containing 5% Glass Fiber.