Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Fatigue Strength | 280 - 310 MPa @# of Cycles 1.00e+8 |
40600 - 45000 psi @# of Cycles 1.00e+8 |
Reverse Bending (R=1) |
Materion Beryllium Copper Alloy 174 Strip; 1/2HT (TH02) Temper (UNS C17410) Treatment required for max strength: Mill HardenedStress Relaxation-% Stress Remaining after 1000 hrs @ 100°C: 95%Stress Relaxation after 1000 hrs @ 200°C: 67%Formability Ratio, 90° Bend, R.. |
|||
Fatigue Strength | 280 - 310 MPa @# of Cycles 1.00e+8 |
40600 - 45000 psi @# of Cycles 1.00e+8 |
Reverse Bending (R=1) |
Materion Beryllium Copper Alloy 174 Strip; HT (TH04) Temper (UNS C17410) Treatment required for max strength: Mill HardenedStress Relaxation-% Stress Remaining after 1000 hrs @ 100°C: 95%Stress Relaxation after 1000 hrs @ 200°C: 76%Formability Ratio, 90° Bend, R.. |
|||
Fatigue Strength | 280 - 310 MPa @# of Cycles 1.00e+8 |
40600 - 45000 psi @# of Cycles 1.00e+8 |
Reverse Bending (R=1) |
Materion Beryllium Copper Alloy 190 Strip; AM (TM00) Temper (UNS C17200) Treatment required for max strength: Mill HardenedStress Relaxation-% Stress Remaining after 1000 hrs @ 100°C: 97%Stress Relaxation after 1000 hrs @ 200°C: 67%Formability Ratio, 90° Bend, R.. |
|||
Fatigue Strength | 280 - 310 MPa @# of Cycles 1.00e+8 |
40600 - 45000 psi @# of Cycles 1.00e+8 |
Reverse Bending (R=1) |
Materion Beryllium Copper Alloy 25 Strip; AT (TF00) Temper (UNS C17200) Treatment required for max strength: 3 hrs @ 315ºCStress Relaxation-% Stress Remaining after 1000 hrs @ 100°C: 96%Stress Relaxation after 1000 hrs @ 200°C: 70%Superficial Hardness: 30N 56-6.. |
|||
Fatigue Strength | 280 - 310 MPa @# of Cycles 1.00e+8 |
40600 - 45000 psi @# of Cycles 1.00e+8 |
Reverse Bending (R=1) |
Materion Brushform® 290 Beryllium Copper Alloy Strip; TM00 Temper (UNS C17200) Treatment required for max strength: Mill HardenedStress Relaxation-% Stress Remaining after 1000 hrs @ 100°C: 97%Stress Relaxation after 1000 hrs @ 200°C: 76%Formability Ratio, 90° Bend, R.. |
|||
Fatigue Strength | 280 - 310 MPa @# of Cycles 1.00e+8 |
40600 - 45000 psi @# of Cycles 1.00e+8 |
Reverse Bending (R=1) |
Materion Beryllium Copper Alloy 25 Strip; 1/4HT (TH01) Temper (UNS C17200) Treatment required for max strength: 2 hrs @ 315ºCStress Relaxation-% Stress Remaining after 1000 hrs @ 100°C: 96%Stress Relaxation after 1000 hrs @ 200°C: 70%Superficial Hardness: 30N 56-6.. |