Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Peel Strength | 3.51 kN/m @Temperature 24.0 °C, Time 605000 sec |
20.0 pli @Temperature 75.2 °F, Time 168 hour |
canvas/canvas |
3M Fastbond™ 30-NF Contact Adhesive 3M Fastbond™ Contact Adhesive 30-NF and 30H-NF are water-dispersed, sprayable contact adhesives for high immediate bond strength n long bonding range.Information provided by 3M |
|||
Peel Strength | 3.51 kN/m @Temperature 24.0 °C, Time 1.21e+6 sec |
20.0 pli @Temperature 75.2 °F, Time 336 hour |
canvas/canvas |
3M Fastbond™ 30-NF Contact Adhesive 3M Fastbond™ Contact Adhesive 30-NF and 30H-NF are water-dispersed, sprayable contact adhesives for high immediate bond strength n long bonding range.Information provided by 3M |
|||
Peel Strength | 3.51 kN/m @Temperature 1.00 °C, Time 1.81e+6 sec |
20.0 pli @Temperature 33.8 °F, Time 504 hour |
180°, Canvas/Steel |
3M Scotch-Weld™ 847 Nitrile High Performance Rubber & Gasket Adhesive Features: Strong flexible bondsMedium viscosity grade adhesive for many brush or flow applicationsQuick dryingExcellent resistance to many fuels and oilsBond leather, nitrile rubber, most plastics, .. |
|||
Peel Strength | 3.51 kN/m @Temperature 1.00 °C, Time 1.81e+6 sec |
20.0 pli @Temperature 33.8 °F, Time 504 hour |
180°, Canvas/Steel |
3M Scotch-Weld™ 847-H Nitrile High Performance Rubber & Gasket Adhesive Features: Strong flexible bondsHigh viscosity grade adhesive for many brush or spray applications.Quick dryingExcellent resistance to many fuels and oilsBond leather, nitrile rubber, most plastics, .. |
|||
Peel Strength | 3.51 kN/m @Temperature 21.0 °C |
20.0 pli @Temperature 69.8 °F |
180° |
3M Scotch-Weld™ DP190 Gray Epoxy Adhesive 3M™ Scotch-Weld™ Epoxy Adhesive DP190 Gray is a 1:1 mix ratio similar to Scotch-Weld™ Epoxy Adhesive 2216 B/A Gray and exhibits good peel, shear and environmental aging properties.Information pro.. |
|||
Peel Strength | 3.51 kN/m @Temperature 82.0 °C |
20.0 pli @Temperature 180 °F |
Aluminum, T-Peel |
3M Scotch-Weld™ DP460 NS Epoxy Adhesive 3M™ Scotch-Weld™ Epoxy Adhesive DP460 Off-White and DP460 NS are high performance, two-part epoxy adhesives offering outstanding shear and peel adhesion and very high levels of durability.Informat.. |
|||
Peel Strength | 3.51 kN/m @Temperature -55.0 °C |
20.0 pli @Temperature -67.0 °F |
180° T-Peel, Etched Al/Etched Al |
3M Scotch-Weld™ DP805 Acrylic Adhesives 3M™ Scotch-Weld™ Acrylic Adhesive DP805 is a two-part, 1:1 mix ratio, toughened acrylic structural adhesives. They exhibit excellent shear and peel strengths along with good impact and durability .. |
|||
Peel Strength | 3.51 kN/m @Temperature 24.0 °C, Time 605000 sec |
20.0 pli @Temperature 75.2 °F, Time 168 hour |
canvas/canvas |
3M Fastbond™ 30H-NF Contact Adhesive 3M Fastbond™ Contact Adhesive 30-NF and 30H-NF are water-dispersed, sprayable contact adhesives for high immediate bond strength n long bonding range.Information provided by 3M |
|||
Peel Strength | 3.51 kN/m @Temperature 24.0 °C, Time 1.21e+6 sec |
20.0 pli @Temperature 75.2 °F, Time 336 hour |
canvas/canvas |
3M Fastbond™ 30H-NF Contact Adhesive 3M Fastbond™ Contact Adhesive 30-NF and 30H-NF are water-dispersed, sprayable contact adhesives for high immediate bond strength n long bonding range.Information provided by 3M |
|||
Peel Strength | 3.51 kN/m @Temperature 66.0 °C, Time 1.81e+6 sec |
20.0 pli @Temperature 151 °F, Time 504 hour |
180°, Canvas/Steel |
3M Fastbond™ 4213-NF Industrial Adhesive 3M™ Fastbond™ Industrial Adhesive 4213-NF is a white, water dispersed adhesive for bonding many fabrics, supported vinyl, wood, leather and most porous materials. Exhibits outstanding clarity when.. |
|||
Peel Strength | 3.51 kN/m @Temperature 1.00 °C, Time 1.81e+6 sec |
20.0 pli @Temperature 33.8 °F, Time 504 hour |
180°, Canvas/Steel |
3M Scotch-Weld™ 847-L Nitrile High Performance Rubber & Gasket Adhesive Features: Strong flexible bondsMedium viscosity grade adhesive for many brush or flow applicationsQuick dryingExcellent resistance to many fuels and oilsBond leather, nitrile rubber, most plastics, .. |
|||
Peel Strength | 3.51 kN/m @Temperature 21.0 °C |
20.0 pli @Temperature 69.8 °F |
180° |
3M Scotch-Weld™ DP190 Translucent Epoxy Adhesive 3M™ Scotch-Weld™ Epoxy Adhesive DP190 Translucent is a 1:1 mix ratio similar to Scotch-Weld™ Epoxy Adhesive 2216 B/A Translucent but faster curing.Information provided by 3M |