3M Scotch-Weld™ 847-L Nitrile High Performance Rubber & Gasket Adhesive

Category Polymer , Adhesive
Manufacturer 3M
Trade Name Scotch-Weld™
Port Shanghai port,China
Trade Terms EXW, FOB, CFR, CIF
Payment Terms L/C, T/T, PayPal
Download PDF 3M Scotch-Weld™ 847-L Nitrile High Performance Rubber & Gasket Adhesive.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Features: Strong flexible bondsMedium viscosity grade adhesive for many brush or flow applicationsQuick dryingExcellent resistance to many fuels and oilsBond leather, nitrile rubber, most plastics, gasketing materials to a variety of substratesMay be heat cured to obtain improved physical properties.Information provided by 3M
Physical Properties Metric English Comments
Solids Content 22 - 26 %
22 - 26 %
pH 4.1 - 4.5
4.1 - 4.5
Brookfield Viscosity 175 - 350 cP
175 - 350 cP
RVF #2 sp @ 20 rpm
Mechanical Properties Metric English Comments
Shear Strength 0.0621 MPa
<br>@Temperature 82.0 °C
9.00 psi
<br>@Temperature 180 °F
Overlap, 1/8&quot; Birch/Birch
0.138 MPa
<br>@Temperature 66.0 °C
20.0 psi
<br>@Temperature 151 °F
Overlap, 1/8&quot; Birch/Birch
1.05 MPa
<br>@Temperature 1.00 °C
152 psi
<br>@Temperature 33.8 °F
Overlap, 1/8&quot; Birch/Birch
1.38 MPa
<br>@Temperature 14.0 °C
200 psi
<br>@Temperature 57.2 °F
Overlap, 1/8&quot; Birch/Birch
Peel Strength 0.701 kN/m
<br>@Temperature 14.0 °C,<br> Time 1.81e+6 sec
4.00 pli
<br>@Temperature 57.2 °F,<br> Time 504 hour
180°, Canvas/Steel
1.58 kN/m
<br>@Temperature 82.0 °C,<br> Time 1.81e+6 sec
9.00 pli
<br>@Temperature 180 °F,<br> Time 504 hour
180°, Canvas/Steel
2.28 kN/m
<br>@Temperature 14.0 °C,<br> Time 86400 sec
13.0 pli
<br>@Temperature 57.2 °F,<br> Time 24.0 hour
180°, Canvas/Steel
2.80 kN/m
<br>@Temperature 66.0 °C,<br> Time 1.81e+6 sec
16.0 pli
<br>@Temperature 151 °F,<br> Time 504 hour
180°, Canvas/Steel
3.51 kN/m
<br>@Temperature 1.00 °C,<br> Time 1.81e+6 sec
20.0 pli
<br>@Temperature 33.8 °F,<br> Time 504 hour
180°, Canvas/Steel
4.12 kN/m
<br>@Temperature 14.0 °C,<br> Time 259000 sec
23.5 pli
<br>@Temperature 57.2 °F,<br> Time 72.0 hour
180°, Canvas/Steel
4.82 kN/m
<br>@Temperature 14.0 °C,<br> Time 432000 sec
27.5 pli
<br>@Temperature 57.2 °F,<br> Time 120 hour
180°, Canvas/Steel
5.43 kN/m
<br>@Temperature 14.0 °C,<br> Time 605000 sec
31.0 pli
<br>@Temperature 57.2 °F,<br> Time 168 hour
180°, Canvas/Steel
6.14 kN/m
<br>@Temperature 14.0 °C,<br> Time 1.21e+6 sec
35.0 pli
<br>@Temperature 57.2 °F,<br> Time 336 hour
180°, Canvas/Steel
Thermal Properties Metric English Comments
Flash Point -18.0 °C
-0.400 °F
CC
Descriptive Properties Value Comments
Appearance Brown
Base Nitrile Rubber