Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Strength | 40.0 MPa @Strain 2 % |
5800 psi @Strain 2 % |
ISO 604 |
Quadrant EPP Ertacetal® C POM-C, extruded (ISO Data) Ertacetal C is Quadrant’s copolymer acetal grade. Next to the standard natural and black grades, there is also a series of special colours available all showing an FDA food contact compliant compos.. |
|||
Compressive Strength | 40.0 MPa @Strain 2 % |
5800 psi @Strain 2 % |
ISO 604 |
Quadrant EPP Quadrant PC 1000 extruded (ISO Data) Quadrant Engineering Plastic Products is marketing non-UV-stabilized polycarbonate stock shapes under the trade name Quadrant PC 1000. It is a natural, “non-optical” industrial quality (clear, tra.. |
|||
Compressive Strength | 40.0 - 50.0 MPa @Temperature 100 °C |
5800 - 7250 psi @Temperature 212 °F |
Cold Crushing Strength |
Gouda Vuurvast CURON 120 HS Dense Refractory Castable Description: This castable has a very good resistance against thermal shocks because of its low thermal expansion. In addition, it has a high strength. Used in incinerators and for tunnel kiln cars... |
|||
Compressive Strength | 40.0 - 50.0 MPa @Temperature 1000 °C |
5800 - 7250 psi @Temperature 1830 °F |
Cold Crushing Strength |
Gouda Vuurvast CURON 150 RN Dense Refractory Castable Description: This on sintered bauxite and low-iron alumina cement based castable contains stainless steel fibers, what results in a very good mechanical strength.Remarks: These values apply to cast .. |
|||
Compressive Strength | 40.0 - 50.0 MPa @Temperature 1000 °C |
5800 - 7250 psi @Temperature 1830 °F |
Cold Crushing Strength |
Gouda Vuurvast CURON 160 HC Dense Refractory Castable Description: Because of the selection of raw materials, this castable has a high volume stability and keeps its strength up to high temperatures. In addition, Curon 160 HC has an excellent thermal s.. |
|||
Compressive Strength | 40.0 - 50.0 MPa @Temperature 1300 °C |
5800 - 7250 psi @Temperature 2370 °F |
Cold Crushing Strength |
Gouda Vuurvast CURON 160 HF Dense Refractory Castable Description: This castable has a high volume stability and keeps its strength up to high temperatures. In addition, Curon 160 HF has an excellent thermal shock resistance. It is largely used in the .. |
|||
Compressive Strength | 40.0 - 50.0 MPa @Temperature 1600 °C |
5800 - 7250 psi @Temperature 2910 °F |
Cold Crushing Strength |
Gouda Vuurvast CURON 180 B Dense Refractory Castable Description: This high quality castable is marked by a high refractoriness and a good thermal shock resistance. Because it has a high alumina content and a low percentage of Fe2O3, this castable can.. |
|||
Compressive Strength | 40.0 - 50.0 MPa @Temperature 1600 °C |
5800 - 7250 psi @Temperature 2910 °F |
Cold Crushing Strength |
Gouda Vuurvast CURON 180 Dense Refractory Castable Description: This high quality, corundum based castable is marked by a high refractoriness and a good thermal shock resistance. Because it has a high alumina content and a low percentage of SiO2, th.. |
|||
Compressive Strength | 40.0 - 50.0 MPa @Temperature 1600 °C |
5800 - 7250 psi @Temperature 2910 °F |
Cold Crushing Strength |
Gouda Vuurvast CURON 180 L Dense Refractory Castable Description: Curon 180 L is a castable based on fused alumina for use up to 1800°C and shows a good thermal shock resistance.Remarks: These values apply to cast products. Also available in gunnin.. |
|||
Compressive Strength | 40.0 - 50.0 MPa @Temperature 100 °C |
5800 - 7250 psi @Temperature 212 °F |
Cold Crushing Strength |
Gouda Vuurvast CURON 180 TF Dense Refractory Castable Description: Curon 180 TF is a tabular alumina based castable, highly abrasion resistant, especially developed for application in the vacuum ladle treatment installation in the steel refinery.Remark.. |
|||
Compressive Strength | 40.0 - 50.0 MPa @Temperature 1000 °C |
5800 - 7250 psi @Temperature 1830 °F |
Cold Crushing Strength |
Gouda Vuurvast CURON 120 S Dense Refractory Castable Description: A very strong castable with a high abrasion resistance of which both aggregate and cement attribute to hydraulic binding.Remarks: These values apply to cast products. Also available in .. |
|||
Compressive Strength | 40.0 - 50.0 MPa @Temperature 1000 °C |
5800 - 7250 psi @Temperature 1830 °F |
Cold Crushing Strength |
Gouda Vuurvast CURON 13 SC Dense Refractory Castable Description: Curon 13 SC is a spinel based castable with a very low silica content and therefore it is suitable for direct contact with all kinds of aluminum/alloys and fluxes in aluminum melting/ho.. |
|||
Compressive Strength | 40.0 - 50.0 MPa @Temperature 100 °C |
5800 - 7250 psi @Temperature 212 °F |
Cold Crushing Strength |
Gouda Vuurvast CURON 130 HRC Dense Refractory Castable Description: A coarse, low iron castable for use up to 1300°C under normal operation conditions, also usable under reducing circumstances. Curon 130 HRC has a good thermal shock resistance becaus.. |
|||
Compressive Strength | 40.0 - 50.0 MPa @Temperature 100 °C |
5800 - 7250 psi @Temperature 212 °F |
Cold Crushing Strength |
Gouda Vuurvast CURON 130 HRCC RAPID Dense Refractory Castable Description: An extra coarse, low iron castable for use to 1300°C under normal operation conditions, also usable under reducing circumstances. Curon 130 HRCC RAPID has good thermal shock resistan.. |
|||
Compressive Strength | 40.0 - 50.0 MPa @Temperature 1300 °C |
5800 - 7250 psi @Temperature 2370 °F |
Cold Crushing Strength |
Gouda Vuurvast CURON 145 CC Dense Refractory Castable Description: This castable is especially developed for strong, large constructions.Remarks: These values apply to cast products.Information provided by Gouda Vuurvast. |
|||
Compressive Strength | 40.0 - 50.0 MPa @Temperature 100 °C |
5800 - 7250 psi @Temperature 212 °F |
Cold Crushing Strength |
Gouda Vuurvast CURON 150 H Dense Refractory Castable Description: Curon 150 H is composed of a very pure grog combined with a high quality high alumina cement. It is characterized by a good resistance against thermal shock and against reducing operati.. |
|||
Compressive Strength | 40.0 - 50.0 MPa @Temperature 1300 °C |
5800 - 7250 psi @Temperature 2370 °F |
Cold Crushing Strength |
Gouda Vuurvast CURON 160 H Dense Refractory Castable Description: Because of the selection of raw materials this castable has a high volume stability and keeps its strength up to high temperatures. In addition Curon 160 H has an excellent thermal shoc.. |
|||
Compressive Strength | 40.0 - 50.0 MPa @Temperature 1200 °C |
5800 - 7250 psi @Temperature 2190 °F |
Cold Crushing Strength |
Gouda Vuurvast CURON 160 HSC Dense Refractory Castable Description: Curon 160 HSC is a coarse abrasion resistant castable to be used up to 1600°C in reducing conditions.Remarks: These values apply to cast products.Information provided by Gouda Vuurva.. |
|||
Compressive Strength | 40.0 - 50.0 MPa @Temperature 100 °C |
5800 - 7250 psi @Temperature 212 °F |
Cold Crushing Strength |
Gouda Vuurvast CURON 165 Dense Refractory Castable Description: Curon 165 is based on bauxite and very pure chamotte grog. In has very good thermal shock resistance and a low firing shrinkage.Remarks: These values apply to cast products. Also availa.. |
|||
Compressive Strength | 40.0 MPa @Temperature 200 °C |
5800 psi @Temperature 392 °F |
ISO 604 |
Victrex® PEEK 450GL15 Polyetheretherketone, 15% Glass Fibre Reinforced Product Description:High performance thermoplastic material, 15% glass fibre reinforced Polyetheretherketone (PEEK), semi crystalline, granules for injection moulding and extrusion, standard flow, F.. |