Mechanical Properties Metric English Comments
Compressive Strength 40.0 MPa

@Strain 2 %
5800 psi

@Strain 2 %
ISO 604
Quadrant EPP Ertacetal® C POM-C, extruded (ISO Data)
Ertacetal C is Quadrant’s copolymer acetal grade. Next to the standard natural and black grades, there is also a series of special colours available all showing an FDA food contact compliant compos..
Compressive Strength 40.0 MPa

@Strain 2 %
5800 psi

@Strain 2 %
ISO 604
Quadrant EPP Quadrant PC 1000 extruded (ISO Data)
Quadrant Engineering Plastic Products is marketing non-UV-stabilized polycarbonate stock shapes under the trade name Quadrant PC 1000. It is a natural, “non-optical” industrial quality (clear, tra..
Compressive Strength 40.0 - 50.0 MPa

@Temperature 100 °C
5800 - 7250 psi

@Temperature 212 °F
Cold Crushing Strength
Gouda Vuurvast CURON 120 HS Dense Refractory Castable
Description: This castable has a very good resistance against thermal shocks because of its low thermal expansion. In addition, it has a high strength. Used in incinerators and for tunnel kiln cars...
Compressive Strength 40.0 - 50.0 MPa

@Temperature 1000 °C
5800 - 7250 psi

@Temperature 1830 °F
Cold Crushing Strength
Gouda Vuurvast CURON 150 RN Dense Refractory Castable
Description: This on sintered bauxite and low-iron alumina cement based castable contains stainless steel fibers, what results in a very good mechanical strength.Remarks: These values apply to cast ..
Compressive Strength 40.0 - 50.0 MPa

@Temperature 1000 °C
5800 - 7250 psi

@Temperature 1830 °F
Cold Crushing Strength
Gouda Vuurvast CURON 160 HC Dense Refractory Castable
Description: Because of the selection of raw materials, this castable has a high volume stability and keeps its strength up to high temperatures. In addition, Curon 160 HC has an excellent thermal s..
Compressive Strength 40.0 - 50.0 MPa

@Temperature 1300 °C
5800 - 7250 psi

@Temperature 2370 °F
Cold Crushing Strength
Gouda Vuurvast CURON 160 HF Dense Refractory Castable
Description: This castable has a high volume stability and keeps its strength up to high temperatures. In addition, Curon 160 HF has an excellent thermal shock resistance. It is largely used in the ..
Compressive Strength 40.0 - 50.0 MPa

@Temperature 1600 °C
5800 - 7250 psi

@Temperature 2910 °F
Cold Crushing Strength
Gouda Vuurvast CURON 180 B Dense Refractory Castable
Description: This high quality castable is marked by a high refractoriness and a good thermal shock resistance. Because it has a high alumina content and a low percentage of Fe2O3, this castable can..
Compressive Strength 40.0 - 50.0 MPa

@Temperature 1600 °C
5800 - 7250 psi

@Temperature 2910 °F
Cold Crushing Strength
Gouda Vuurvast CURON 180 Dense Refractory Castable
Description: This high quality, corundum based castable is marked by a high refractoriness and a good thermal shock resistance. Because it has a high alumina content and a low percentage of SiO2, th..
Compressive Strength 40.0 - 50.0 MPa

@Temperature 1600 °C
5800 - 7250 psi

@Temperature 2910 °F
Cold Crushing Strength
Gouda Vuurvast CURON 180 L Dense Refractory Castable
Description: Curon 180 L is a castable based on fused alumina for use up to 1800°C and shows a good thermal shock resistance.Remarks: These values apply to cast products. Also available in gunnin..
Compressive Strength 40.0 - 50.0 MPa

@Temperature 100 °C
5800 - 7250 psi

@Temperature 212 °F
Cold Crushing Strength
Gouda Vuurvast CURON 180 TF Dense Refractory Castable
Description: Curon 180 TF is a tabular alumina based castable, highly abrasion resistant, especially developed for application in the vacuum ladle treatment installation in the steel refinery.Remark..
Compressive Strength 40.0 - 50.0 MPa

@Temperature 1000 °C
5800 - 7250 psi

@Temperature 1830 °F
Cold Crushing Strength
Gouda Vuurvast CURON 120 S Dense Refractory Castable
Description: A very strong castable with a high abrasion resistance of which both aggregate and cement attribute to hydraulic binding.Remarks: These values apply to cast products. Also available in ..
Compressive Strength 40.0 - 50.0 MPa

@Temperature 1000 °C
5800 - 7250 psi

@Temperature 1830 °F
Cold Crushing Strength
Gouda Vuurvast CURON 13 SC Dense Refractory Castable
Description: Curon 13 SC is a spinel based castable with a very low silica content and therefore it is suitable for direct contact with all kinds of aluminum/alloys and fluxes in aluminum melting/ho..
Compressive Strength 40.0 - 50.0 MPa

@Temperature 100 °C
5800 - 7250 psi

@Temperature 212 °F
Cold Crushing Strength
Gouda Vuurvast CURON 130 HRC Dense Refractory Castable
Description: A coarse, low iron castable for use up to 1300°C under normal operation conditions, also usable under reducing circumstances. Curon 130 HRC has a good thermal shock resistance becaus..
Compressive Strength 40.0 - 50.0 MPa

@Temperature 100 °C
5800 - 7250 psi

@Temperature 212 °F
Cold Crushing Strength
Gouda Vuurvast CURON 130 HRCC RAPID Dense Refractory Castable
Description: An extra coarse, low iron castable for use to 1300°C under normal operation conditions, also usable under reducing circumstances. Curon 130 HRCC RAPID has good thermal shock resistan..
Compressive Strength 40.0 - 50.0 MPa

@Temperature 1300 °C
5800 - 7250 psi

@Temperature 2370 °F
Cold Crushing Strength
Gouda Vuurvast CURON 145 CC Dense Refractory Castable
Description: This castable is especially developed for strong, large constructions.Remarks: These values apply to cast products.Information provided by Gouda Vuurvast.
Compressive Strength 40.0 - 50.0 MPa

@Temperature 100 °C
5800 - 7250 psi

@Temperature 212 °F
Cold Crushing Strength
Gouda Vuurvast CURON 150 H Dense Refractory Castable
Description: Curon 150 H is composed of a very pure grog combined with a high quality high alumina cement. It is characterized by a good resistance against thermal shock and against reducing operati..
Compressive Strength 40.0 - 50.0 MPa

@Temperature 1300 °C
5800 - 7250 psi

@Temperature 2370 °F
Cold Crushing Strength
Gouda Vuurvast CURON 160 H Dense Refractory Castable
Description: Because of the selection of raw materials this castable has a high volume stability and keeps its strength up to high temperatures. In addition Curon 160 H has an excellent thermal shoc..
Compressive Strength 40.0 - 50.0 MPa

@Temperature 1200 °C
5800 - 7250 psi

@Temperature 2190 °F
Cold Crushing Strength
Gouda Vuurvast CURON 160 HSC Dense Refractory Castable
Description: Curon 160 HSC is a coarse abrasion resistant castable to be used up to 1600°C in reducing conditions.Remarks: These values apply to cast products.Information provided by Gouda Vuurva..
Compressive Strength 40.0 - 50.0 MPa

@Temperature 100 °C
5800 - 7250 psi

@Temperature 212 °F
Cold Crushing Strength
Gouda Vuurvast CURON 165 Dense Refractory Castable
Description: Curon 165 is based on bauxite and very pure chamotte grog. In has very good thermal shock resistance and a low firing shrinkage.Remarks: These values apply to cast products. Also availa..
Compressive Strength 40.0 MPa

@Temperature 200 °C
5800 psi

@Temperature 392 °F
ISO 604
Victrex® PEEK 450GL15 Polyetheretherketone, 15% Glass Fibre Reinforced
Product Description:High performance thermoplastic material, 15% glass fibre reinforced Polyetheretherketone (PEEK), semi crystalline, granules for injection moulding and extrusion, standard flow, F..