Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 15.0 GPa @Temperature 90.0 °C |
2180 ksi @Temperature 194 °F |
|
LATI Larton G/40 PPS, 40% Glass Fiber Reinforced Polyphenylene Sulfide (PPS) based compound. Glass fibers. Very good chemical resistance. Very good thermal properties. Low smoke density and low toxicity index.Availability: Africa & Middle East; As.. |
|||
Tensile Modulus | 15.0 GPa @Temperature 150 °C |
2180 ksi @Temperature 302 °F |
|
LATI Larton K/40 HM PPS, 40% Carbon Fiber Reinforced Polyphenylene Sulfide (PPS) based compound. Carbon fiber. High tensile modulus. Very good chemical resistance. Very good thermal properties. Low smoke density and low toxicity index.Availability: Af.. |
|||
Tensile Modulus | 15.0 GPa @Temperature 90.0 °C |
2180 ksi @Temperature 194 °F |
|
LATI Latamid 66 H2 K/30 PA 66, 30% Carbon Fiber Reinforced, Heat Stabilized Polyamide 66 (PA66) based compound. Heat stabilized. Carbon fiber.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria Termopl.. |
|||
Tensile Modulus | 15.0 GPa @Temperature 120 °C |
2180 ksi @Temperature 248 °F |
|
LATI Laramid G/60 PPA, 60% Glass Fiber Reinforced Semi-aromatic polyamide (PPA) based compound. Glass fibers. Very good thermal properties. Good chemical resistance. Low moisture absorption.Availability: Africa & Middle East; Asia Pacific; Europe; .. |
|||
Tensile Modulus | 15.0 GPa @Temperature 23.0 °C |
2180 ksi @Temperature 73.4 °F |
|
LATI Larton G/40 I6 PPS, 40% Glass Fiber Reinforced Polyphenylene Sulfide (PPS) based compound. Glass fibers. Good elongation. Very good chemical resistance. Very good thermal properties. Low smoke density and low toxicity index.Availability: Africa .. |
|||
Tensile Modulus | 15.0 GPa @Temperature 120 °C |
2180 ksi @Temperature 248 °F |
|
LATI Larton K/30 PPS, 30% Carbon Fiber Reinforced Polyphenylene Sulfide (PPS) based compound. Carbon fiber. Very good chemical resistance. Very good thermal properties. Low smoke density and low toxicity index.Availability: Africa & Middle East; As.. |
|||
Tensile Modulus | 15.0 GPa @Temperature 23.0 °C |
2180 ksi @Temperature 73.4 °F |
|
LATI Latene® AG7H K/30 PP Homopolymer, 30% Carbon Fiber Reinforced, Heat Stabilized Polypropylene homopolymer (PPh) based compound. Chemical grafting Heat stabilized. Carbon fiber. Good thermal properties.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; Nort.. |
|||
Tensile Modulus | 15.0 GPa @Temperature 23.0 °C |
2180 ksi @Temperature 73.4 °F |
DAM; ISO 527 |
DuPont Performance Polymers Zytel® HTN 51G45HSL BK083 Polyphthalamide (PPA)
(Unverified Data**) Zytel® HTN51G45HSL BK083 is a 45% glass reinforced, heat stabilized, lubricated high performance polyamide resin. It is also a PPA resin.Information provided by DuPont Performance Polymers |