Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 1.40 GPa @Temperature 23.0 °C |
203 ksi @Temperature 73.4 °F |
50%RH; ISO 527 |
DuPont Performance Polymers Zytel® 101 NC010 Nylon 66
(Unverified Data**) Zytel® 101 NC010 is a general purpose polyamide 66 resin for injection molding and extrusion.Information provided by DuPont Performance Polymers |
|||
Tensile Modulus | 1.40 GPa @Temperature 23.0 °C |
203 ksi @Temperature 73.4 °F |
50%RH; ISO 527 |
DuPont Performance Polymers Zytel® 101L BKB080 Nylon 66
(Unverified Data**) Zytel® 101L BKB080 is a lubricated polyamide 66 resin for injection molding.Information provided by DuPont Performance Polymers |
|||
Tensile Modulus | 1.40 GPa @Temperature 23.0 °C |
203 ksi @Temperature 73.4 °F |
50%RH; ISO 527 |
DuPont Performance Polymers Zytel® 103HSL BKB080 Nylon 66
(Unverified Data**) Zytel® 103HSL BKB080 is a heat stabilized, lubricated polyamide 66 resin for injection molding.Information provided by DuPont Performance Polymers |
|||
Tensile Modulus | 1.40 GPa @Temperature 23.0 °C |
203 ksi @Temperature 73.4 °F |
50%RH; ISO 527 |
DuPont Performance Polymers Zytel® 7335F NC010 Nylon 6
(Unverified Data**) Zytel® 7335F NC010 is a nucleated, lubricated polyamide 6 resin for injection molding.Information provided by DuPont Performance Polymers |
|||
Tensile Modulus | 1.40 GPa @Temperature 120 °C |
203 ksi @Temperature 248 °F |
|
Hybrid Plastics Nanoreinforced® Cellulose Propionate Acetate Nanoreinforced® Cellulose Propionate Acetate is an optically clear nanocomposite with POSS® dispersed at the nanometer level. Compared to virgin cellulose propionate acetate, it enhances mecha.. |
|||
Tensile Modulus | 1.40 GPa @Temperature 60.0 °C |
203 ksi @Temperature 140 °F |
|
LATI Latamid 6 H-V0 PA 6, Heat Stabilized, Flame Retardant Polyamide 6 (PA6) based compound. Heat stabilized. UL94 V-0 classified, halogens-based flame retardants and red phosphorous free. Very good surface appearance.Availability: Africa & Middle East; Asi.. |
|||
Tensile Modulus | 1.40 GPa @Temperature 60.0 °C |
203 ksi @Temperature 140 °F |
|
LATI Latamid 66 H2PX-V0 PA 66, Heat Stabilized, Flame Retardant Polyamide 66 (PA66) based compound. Heat stabilized. Toughened. UL94 V-0 classified, with brominated flame retardants, PBB/PBDE free. Availability: Africa & Middle East; Asia Pacific; Europe; Latin .. |
|||
Tensile Modulus | 1.40 GPa @Temperature 23.0 °C |
203 ksi @Temperature 73.4 °F |
|
LATI Latene® 7-V2 PP Homopolymer, Flame Retardant Polypropylene homopolymer (PPh) based compound. UL94 V-2 classified, with brominated flame retardants, PBB/PBDE free. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North A.. |
|||
Tensile Modulus | 1.40 GPa @Temperature 60.0 °C |
203 ksi @Temperature 140 °F |
|
LATI Latan 23UVE71 POM Polyoxymethylene (POM). UV stabilized. Toughened. Low viscosity. Good elongation and impact resistance.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformati.. |
|||
Tensile Modulus | 1.40 GPa @Temperature 60.0 °C |
203 ksi @Temperature 140 °F |
|
LATI Latan 9 POM Polyoxymethylene (POM). Unfilled. Medium viscosity. Very good tribological properties.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by La.. |
|||
Tensile Modulus | 1.40 GPa @Temperature 50.0 °C |
203 ksi @Temperature 122 °F |
|
Arkema Group KYNAR® 710, 710 HDP Polyvinylidene Fluoride Homopolymer- Injection Molding Characteristics: Natural resin - translucent, off-white hemispheres. HDP indicates higher color stability. High stability in harsh thermal, chemical and ultraviolet environments. High toughness .. |
|||
Tensile Modulus | 1.40 GPa @Temperature 23.0 °C |
203 ksi @Temperature 73.4 °F |
50%RH; ISO 527 |
DuPont Performance Polymers Zytel® FG101L NC010 Nylon 66
(Unverified Data**) Zytel® FG101L NC010 is a lubricated polyamide 66 resin for injection molding. It has been developed for consideration into applications such as parts for the food industry.Information provided by D.. |
|||
Tensile Modulus | 1.40 GPa @Temperature 60.0 °C |
203 ksi @Temperature 140 °F |
|
LATI Latiblend 7587 E61-V0 PBT/PC, Flame Retardant Blend based on Polybutylene Terephthalate (PBT) / Polycarbonate (PC). Toughened. UL94 V-0 classified, with brominated flame retardants, PBB/PBDE free. Very high dimensional stability. High impact re.. |