Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 1.30 GPa @Temperature 23.0 °C |
189 ksi @Temperature 73.4 °F |
X direction; ASTM D638 |
Rogers Corporation RT/duroid® 5870 Glass Microfiber Reinforced PTFE High Frequency Laminate RT/duroid® 5870 and 5880 glass microfiber reinforced PTFE composites are designed for exacting stripline and microstrip circuit applications. Glass reinforcing microfibers are randomly oriented to.. |
|||
Tensile Modulus | 1.30 GPa @Temperature 23.0 °C |
189 ksi @Temperature 73.4 °F |
50%RH; ISO 527 |
DuPont Performance Polymers Zytel® 45HSB NC010 Nylon 66
(Unverified Data**) Zytel® 45HSB NC010 is a high viscosity, heat stabilized polyamide 66 resin for injection molding and extrusion.Information provided by DuPont Performance Polymers |
|||
Tensile Modulus | 1.30 GPa @Temperature 23.0 °C |
189 ksi @Temperature 73.4 °F |
50%RH; ISO 527 |
DuPont Performance Polymers Zytel® FG42A NC010 Nylon 66
(Unverified Data**) Zytel® FG42A NC010 is a high viscosity polyamide 66 resin for injection molding and extrusion. It has been developed for consideration into applications such as parts for the food industry.Informat.. |
|||
Tensile Modulus | 1.30 GPa @Temperature 90.0 °C |
189 ksi @Temperature 194 °F |
|
LATI Kelon® B FR H2 CE/25-V2HF PA 6, Mineral Reinforced, Flame Retardant, Heat Stabilized Polyamide 6 (PA6) based compound. Heat stabilized. Mineral filler. UL94 V-2 classified, halogens-based flame retardants and red phosphorous free.Availability: Africa & Middle East; Asia Pacific; Eur.. |
|||
Tensile Modulus | 1.30 GPa @Temperature 120 °C |
189 ksi @Temperature 248 °F |
|
LATI Lastilac 11 G/10 ABS/PC, 10% Glass Fiber Reinforced ABS/PC Blend (ABS/PC) based compound. Glass fibers. Good surface appearance. Good impact resistance. Good thermal properties.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; .. |
|||
Tensile Modulus | 1.30 GPa @Temperature 60.0 °C |
189 ksi @Temperature 140 °F |
|
LATI Latan 13 POM Polyoxymethylene (POM). Unfilled. Medium viscosity. Very good tribological properties.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by La.. |
|||
Tensile Modulus | 1.30 GPa @Temperature 90.0 °C |
189 ksi @Temperature 194 °F |
|
LATI Latan 13 S/30 POM, 30% Glass Bead Reinforced Polyoxymethylene (POM) based compound. Glass beads. Medium viscosity. High dimensional stability.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation pro.. |
|||
Tensile Modulus | 1.30 GPa @Temperature 60.0 °C |
189 ksi @Temperature 140 °F |
|
LATI Later 4-V0HF1 PBT, Flame Retardant Polybutylene Terephthalate (PBT) based compound. UL94 V-0 classified, halogens-based flame retardants and red phosphorous free. Availability: Africa & Middle East; Asia Pacific; Europe; Latin Americ.. |
|||
Tensile Modulus | 1.30 GPa @Temperature 23.0 °C |
189 ksi @Temperature 73.4 °F |
50%RH; ISO 527 |
DuPont Performance Polymers Zytel® RS 3061HSL BK039A Nylon 610
(Unverified Data**) Zytel® RS 3061HSL BK039A is a renewably sourced polyamide 610 resin containing a minimum of 60% renewably sourced ingredient by weight. It is an unreinforced, heat stabilized, lubricated black grad.. |
|||
Tensile Modulus | 1.30 GPa @Temperature 23.0 °C |
189 ksi @Temperature 73.4 °F |
ASTM D 638 |
Saint-Gobain Meldin® 2021 Bearing General Notes on Meldin 2000 Series Bearing Products:For High-Temperature, Close-Tolerance Applications. Able to withstand temperatures of 600°F with excursions to 900°F, the Medlin 2000 Series ca.. |