Polymer Property : Tensile Modulus = 1360 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Modulus 9.40 GPa

@Temperature 23.0 °C
1360 ksi

@Temperature 73.4 °F
DAM; ISO 527
DuPont Performance Polymers Zytel® 73G30T BK261 Nylon 6  (Unverified Data**)
Zytel® 73G30T BK261 is a 30% glass fiber reinforced, toughened, black polyamide 6 resin for injection molding.Information provided by DuPont Performance Polymers
Tensile Modulus 9.40 GPa

@Temperature 150 °C
1360 ksi

@Temperature 302 °F
LATI Larton GCE/650 PPS, Glass/Mineral Reinforced
Polyphenylene Sulfide (PPS) based compound. Glass fibers / Mineral filler. Very good chemical resistance. Very good thermal properties. Low smoke density and low toxicity index.Availability: Africa ..
Tensile Modulus 9.40 GPa

@Temperature 23.0 °C
1360 ksi

@Temperature 73.4 °F
LATI Latamid 66 H2 G/30 PA 66, 30% Glass Fiber Reinforced, Heat Stabilized
Polyamide 66 (PA66) based compound. Heat stabilized. Glass fibers. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria Termop..
Tensile Modulus 9.40 GPa

@Temperature 23.0 °C
1360 ksi

@Temperature 73.4 °F
LATI Latamid 66 VH G/30 PA 66, 30% Glass Fiber Reinforced, Heat Stabilized
Polyamide 66 (PA66) based compound. Heat stabilized. Hydrolysis stabilized. Glycol stabilized. Glass fibers.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInfo..
Tensile Modulus 9.40 GPa

@Temperature 120 °C
1360 ksi

@Temperature 248 °F
LATI Latilon 28D K/20 PC, 20% Carbon Fiber Reinforced
Polycarbonate (PC) based compound. Carbon fiber. Low smoke density and low toxicity index.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided b..
Tensile Modulus 9.40 GPa

@Temperature 60.0 °C
1360 ksi

@Temperature 140 °F
LATI Lapex A G/30 PES, 30% Glass Fiber Reinforced
Polyether Sulfone (PES) based compound. Glass fibers. Low smoke density and low toxicity index. Very high dimensional stability.Availability: Africa & Middle East; Asia Pacific; Europe; Latin Americ..
Tensile Modulus 9.40 GPa

@Temperature 23.0 °C
1360 ksi

@Temperature 73.4 °F
LATI Latiblend 6252 H2 G/30 PA6/PP Homopolymer
Blend based on Polyamide 6 (PA6) / Polypropylene homopolymer (PPh). Heat stabilized. Glass fibers. Good thermal properties.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; No..