Mechanical Properties Metric English Comments
Tensile Modulus 4.80 GPa

@Temperature 23.0 °C
696 ksi

@Temperature 73.4 °F
DAM; ISO 527
DuPont Performance Polymers Minlon® 12TA BKB124 Nylon 66  (Unverified Data**)
Minlon® 12TA BKB124 is a 32% mineral reinforced, toughened, heat stabilized, black polyamide 66 resin for injection molding.Information provided by DuPont Performance Polymers
Tensile Modulus 4.80 GPa

@Temperature 23.0 °C
696 ksi

@Temperature 73.4 °F
LATI Latamid 66 E21 G/15 PA 66, 15% Glass Fiber Reinforced
Polyamide 66 (PA66) based compound. Toughened. Glass fibers.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria Termoplastici..
Tensile Modulus 4.80 GPa

@Temperature 120 °C
696 ksi

@Temperature 248 °F
LATI Lapex R G/20 PPSU, 20% Glass Reinforced
Polyphenylene Sulfone (PPSU) based compound. Glass fibers. Low smoke density and low toxicity index. Very high dimensional stability.Availability: Africa & Middle East; Asia Pacific; Europe; Latin A..
Tensile Modulus 4.80 GPa

@Temperature 120 °C
696 ksi

@Temperature 248 °F
LATI Latamid 66 H2 G/25 PA 66, 25% Glass Fiber Reinforced, Heat Stabilized
Polyamide 66 (PA66) based compound. Heat stabilized. Glass fibers. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria Termop..
Tensile Modulus 4.80 GPa

@Temperature 90.0 °C
696 ksi

@Temperature 194 °F
LATI Latamid 66 H2 G/25-V0CT1 PA 66, 25% Glass Fiber Reinforced, Heat Stabilized, Flame Retardant
Polyamide 66 (PA66) based compound. Heat stabilized. Glass fibers. UL94 V-0 classified, with brominated flame retardants, PBB/PBDE free. Availability: Africa & Middle East; Asia Pacific; Europe; Lat..
Tensile Modulus 4.80 GPa

@Temperature 90.0 °C
696 ksi

@Temperature 194 °F
LATI Latamid 66 H2 G/25-V0KB1 PA 66, 25% Glass Fiber Reinforced, Heat Stabilized, Flame Retardant
Polyamide 66 (PA66) based compound. Heat stabilized. Glass fibers. UL94 V-0 classified, with red phosphorous. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaIn..
Tensile Modulus 4.80 GPa

@Temperature 150 °C
696 ksi

@Temperature 302 °F
LATI Latamid SP1 G/50 PA 6.10, 50% Glass Fiber Reinforced
Polyamide 6.10 (PA6.10) based compound. Glass fibers. Low moisture absorption.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Indus..
Tensile Modulus 4.80 GPa

@Temperature 120 °C
696 ksi

@Temperature 248 °F
LATI Latamid SP2 H2 G/45 PA 6.12, 45% Glass Fiber Reinforced, Heat Stabilized
Polyamide 6.12 (PA6.12) based compound. Heat stabilized. Glass fibers. Low moisture absorption.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provi..
Tensile Modulus 4.80 GPa

@Temperature 23.0 °C
696 ksi

@Temperature 73.4 °F
90°
Hexcel® HexPly® 954-6 Curing Cyanate Resin, K13C-2U Fiber
Information provided by HexCel
Tensile Modulus 4.80 GPa

@Temperature 23.0 °C
696 ksi

@Temperature 73.4 °F
ISO 527
DuPont Performance Polymers Delrin® 577 BK000 Acetal Homopolymer  (Unverified Data**)
Delrin® 577 BK000 is a medium viscosity acetal homopolymer containing 20% glass fiber filler, with high stiffness, low warpage and low creep for superior performance at elevated temperature. It con..
Tensile Modulus 4.80 GPa

@Temperature 90.0 °C
696 ksi

@Temperature 194 °F
LATI Kelon® A FR H2 CETG/300-V0 PA 66, Glass/Mineral Reinforced, Flame Retardant, Heat Stabilized
Polyamide 66 (PA66) based compound. Heat stabilized. Glass fibers / Mineral filler. UL94 V-0 classified, with brominated flame retardants, PBB/PBDE and antimony trioxide free. Low thermal expansion ..