Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 1.80 GPa @Temperature 23.0 °C |
261 ksi @Temperature 73.4 °F |
DAM; ISO 527 |
DuPont Performance Polymers Zytel® ST7301 BK356 Nylon 6
(Unverified Data**) Zytel® ST7301 BK356 is a Super Tough, heat stabilized, lubricated, black polyamide 6 resin for injection molding and extrusion. It offers outstanding impact resistance over a wide temperature and h.. |
|||
Tensile Modulus | 1.80 GPa @Temperature 23.0 °C |
261 ksi @Temperature 73.4 °F |
DAM; ISO 527 |
DuPont Performance Polymers Zytel® ST7301 NC010 Nylon 6
(Unverified Data**) Zytel® ST7301 NC010 is a Super Tough, heat stabilized, lubricated polyamide 6 resin for injection molding and extrusion. It offers outstanding impact resistance over a wide temperature and humidity.. |
|||
Tensile Modulus | 1.80 GPa @Temperature 60.0 °C |
261 ksi @Temperature 140 °F |
|
LATI Latamid 66 B H-V0 PA 66, Heat Stabilized, Flame Retardant Polyamide 66 (PA66) based compound. High fluidity. Heat stabilized. UL94 V-0 classified, halogens-based flame retardants and red phosphorous free. Blended with PA6.Availability: Africa & Middle East.. |
|||
Tensile Modulus | 1.80 GPa @Temperature 23.0 °C |
261 ksi @Temperature 73.4 °F |
|
LATI Latene® 7H2W-V0 PP Homopolymer, Heat Stabilized, Flame Retardant Polypropylene homopolymer (PPh) based compound. Heat stabilized. Metal stabilized. UL94 V-0 classified, halogens-based flame retardants and red phosphorous free. Low smoke density and low toxicity i.. |
|||
Tensile Modulus | 1.80 GPa @Temperature 150 °C |
261 ksi @Temperature 302 °F |
|
LATI Later 4 G/30-V0CT2 PBT, 30% Glass Fiber Reinforced, Flame Retardant Polybutylene Terephthalate (PBT) based compound. Glass fibers. UL94 V-0 classified, with brominated flame retardants, PBB/PBDE free. Availability: Africa & Middle East; Asia Pacific; Europe; Latin A.. |
|||
Tensile Modulus | 1.80 GPa @Temperature 90.0 °C |
261 ksi @Temperature 194 °F |
|
LATI Latilon 28D PC Polycarbonate (PC). Unfilled. Low smoke density and low toxicity index. Very high dimensional stability. Very good surface appearanceAvailability: Africa & Middle East; Asia Pacific; Europe; Latin A.. |
|||
Tensile Modulus | 1.80 GPa @Temperature 90.0 °C |
261 ksi @Temperature 194 °F |
|
LATI Latilon 28D-V0 PC, Flame Retardant Polycarbonate (PC) based compound. UL94 V-0 classified, brominated and chlorinated halogens-based flame retardants free. Low smoke density and low toxicity index. Very high dimensional stability. Ve.. |
|||
Tensile Modulus | 1.80 GPa @Temperature 23.0 °C |
261 ksi @Temperature 73.4 °F |
50%RH; ISO 527 |
DuPont Performance Polymers Minlon® EFE6096 GY090A Nylon 66
(Unverified Data**) Minlon® EFE6096 GY090A is a 15% mineral reinforced impact modified nylon 66 resin.Information provided by DuPont Performance Polymers |