Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Peel Strength | 5.26 kN/m | 30.0 pli | Given in psi |
Resin Technology Group UV-S-2051 High Impact, UV Curable Plastic Bonder UV S-2051 is a general purpose, fast cure response, high thermal-shock resistant, UV curing adhesive designed for use in a variety of applications including chip bonding, laminating, tacking, and se.. |
|||
Peel Strength | 5.26 - 7.01 kN/m | 30.0 - 40.0 pli | Average value: 6.57 kN/m Grade Count:4 |
Overview of materials for Epoxy Adhesive, Flexible This property data is a summary of similar materials in the MatWeb database for the category "Epoxy Adhesive, Flexible". Each property range of values reported is minimum and maximum values of appro.. |
|||
Peel Strength | 5.26 kN/m | 30.0 pli | Tensile |
Dielectric Polymers NT-590DL Protective Film
(discontinued **) Crosslinked silicone adhesive with polyimide film backing.Features: U.L. recognized Class 392°FHigh temperature resistantDie cut disks/shapes remove easily from linerClean tape removalApplications:.. |
|||
Peel Strength | 5.26 kN/m | 30.0 pli | Tensile |
Dielectric Polymers NT-590 Polyimide Film Tape
(discontinued **) Crosslinked silicone adhesive with polyimide film backing.Features: U.L. recognized class 392°FHigh temperature resistantClean tape removalApplications: For high temperature masking, protecting gol.. |
|||
Peel Strength | >= 5.26 kN/m | >= 30.0 pli | steel/steel |
Resinlab® AR 4305 HP Metal Bonding Methacrylate Adhesive Resinlab™ AR 4305 HP is a 1:1 mix methacrylate-based structural adhesive designed for general purpose bonding of a wide variety of materials in industrial applications. AR 4305 HP forms tough, dur.. |
|||
Peel Strength | >= 5.26 kN/m | >= 30.0 pli | steel/steel |
Resinlab® AR 4315 HP Metal Bonding Methacrylate Adhesive Resinlab™ AR 4315 HP is a 1:1 mix methacrylate-based structural adhesive formulated to bond almost all engineered thermoplastics, thermosets, composites, and metal structural elements together in a.. |
|||
Peel Strength | >= 5.26 kN/m | >= 30.0 pli | steel/steel |
Resinlab® AR 4340 HP Metal Bonding Methacrylate Adhesive Resinlab™ AR 4340 HP is a 1:1 mix methacrylate-based structural adhesive designed for general purpose bonding of a wide variety of materials in industrial applications. It is an accelerated version.. |
|||
Peel Strength | >= 5.26 kN/m | >= 30.0 pli | steel/steel |
Resinlab® AR 4400 HP Metal & Composite Bonding Methacrylate Adhesive Resinlab™ AR 4400 HP is a 1:1 mix methacrylate-based structural adhesive formulated to bond almost all engineered thermoplastics, thermosets, composites, and metal structural elements together in a.. |
|||
Peel Strength | >= 5.26 kN/m | >= 30.0 pli | ASTM D1876 |
Lord Adhesives Versilok® 253 / 254 Acrylic Adhesive LORD Versilok® 253/254 adhesive is a two-component, epoxy-modified acrylic adhesive used to bond a variety of automotive sheet metals, including hot-dip galvanized, electro-galvanized, bare alum.. |
|||
Peel Strength | >= 5.26 kN/m | >= 30.0 pli | ASTM D1876 |
Lord Adhesives Versilok® 262 / 254 Acrylic Adhesive LORD Versilok® 262/254 adhesive is a two-component, epoxy-modified acrylic adhesive used to bond a variety of automotive sheet metals, including hot-dip galvanized, electro-galvanized, bare alumi.. |
|||
Peel Strength | >= 5.26 kN/m | >= 30.0 pli | ASTM D1876 |
Lord Adhesives Versilok® 262B / 254 Acrylic Adhesive LORD Versilok® 262B/254 adhesive is a two-component, epoxy-modified acrylic adhesive used to bond a variety of automotive sheet metals, including hot-dip galvanized, electro-galvanized, bare alum.. |
|||
Peel Strength | >= 5.26 kN/m | >= 30.0 pli | ASTM D1876 |
Lord Adhesives Versilok® 265 / 254 Acrylic Adhesive LORD Versilok® 265/254 adhesive is a two-component, epoxy-modified acrylic adhesive used to bond a variety of automotive sheet metals, including hot-dip galvanized, electro-galvanized, bare alumi.. |
|||
Peel Strength | 5.26 - 7.01 kN/m | 30.0 - 40.0 pli | |
ITW Devcon Metal Welderâ„¢ Methacrylate Adhesive II, Grey / Beads Information provided by ITW Devcon |
|||
Peel Strength | 5.26 - 7.01 kN/m | 30.0 - 40.0 pli | |
ITW Devcon Metal Welderâ„¢ Methacrylate Adhesive, Grey / Beads Information provided by ITW Devcon |
|||
Peel Strength | >= 5.26 kN/m | >= 30.0 pli | T-peel |
Master Bond EP21TDC-2ND Two component, highly flexibilized, non-drip epoxy resin compound Product Description: Master Bond EP21TDC-2ND is a two component highly flexible epoxy resin system for high performance bonding, sealing and coating with a non-drip consistency. It has a forgiving o.. |
|||
Peel Strength | >= 5.26 kN/m | >= 30.0 pli | |
Master Bond EP21TDC-4 Two Component, Highly Flexible Epoxy System Master Bond Polymer System EP21TDC-4 is a two component, flexible epoxy resin system for high performance bonding, sealing and coating. It is formulated to cure at ambient temperatures or more quick.. |
|||
Peel Strength | >= 5.26 kN/m | >= 30.0 pli | T-peel |
Master Bond EP21TDC-4ND Two component, highly flexibilized epoxy for bonding, sealing and coating Product Description: Master Bond EP21TDC-4ND is a two component, very flexible epoxy system for high performance bonding, sealing and coating with a non-drip consistency. It has a one to four mix ra.. |
|||
Peel Strength | 5.26 kN/m | 30.0 pli | Cure cycle: 1 day @ RT, with Acid Etched 6061-T6 Aluminum |
Zyvex Performance Materials Epovex™ Nano-Engineered Composite Epoxy Adhesive Paste Epovex® Adhesive Paste is a carbon nanotube enhanced two part epoxy adhesive thixotropic paste. Used for bonding or filling, Epovex Paste is ideal for many metals, woods, masonry products, and some.. |
|||
Peel Strength | 5.26 - 12.3 kN/m | 30.0 - 70.0 pli | Varies with substrates. |
Loctite® Durabond® E-214HP Epoxy Adhesive Loctite offers a complete line of one-part and two-part epoxy and urethane adhesives for structural bonding, potting and encapsulating. The Loctite® Durabond® line contains 14 application-specific.. |
|||
Peel Strength | 5.26 kN/m | 30.0 pli | Bond Strength (S2 to S2); Arlon SQA-TMS-011 |
Arlon 55578GA028 0.0280" Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction:Interleave: LDPESide 2 Layer 2: Uncured Silicone RubberSide 2 Layer 1: Cured Silicone RubberSubstrate: Style 162 FiberglassSide 1: Cured Silicone RubberThis data represents ty.. |
|||
Peel Strength | 5.26 kN/m | 30.0 pli | T-Peel |
3M Scotch-Weld™ DP8010NS Structural Adhesive 3M™ Scotch-Weld™ Structural Plastic Adhesive DP-8010NS is a two-part acrylic-based adhesive (10:1 ratio by volume) that can bond many low surface energy plastics, including many grades of Polyprop.. |
|||
Peel Strength | 5.26 kN/m | 30.0 pli | T-Peel, HDPE, Substrate Failure |
3M Scotch-Weld™ DP8010NS Structural Adhesive 3M™ Scotch-Weld™ Structural Plastic Adhesive DP-8010NS is a two-part acrylic-based adhesive (10:1 ratio by volume) that can bond many low surface energy plastics, including many grades of Polyprop.. |
|||
Peel Strength | 5.26 kN/m | 30.0 pli | T-Peel |
3M Scotch-Weld™ DP810 Black Structural Adhesive 3M™ Scotch-Weld™ Low-Odor Acrylic Adhesives are two-part, 1:1 mix ratio, toughened structural adhesives with less odor than most acrylic adhesives. The adhesives have excellent shear and peel stre.. |
|||
Peel Strength | 5.26 kN/m | 30.0 pli | Etched Al/Etched Al after 1 week at RT cure |
3M Scotch-Weld™ DP812 Acrylic Adhesives 3M™ Scotch-Weld™ Acrylic Adhesive DP812 is a two-part, 1:1 mix ratio, toughened acrylic structural adhesives. They exhibit excellent shear and peel strengths along with good impact, durability and.. |
|||
Peel Strength | 5.26 kN/m | 30.0 pli | Bell Peel Adhesion, Aluminum Etched, with KTL N16 Deep Draw Lube Oil, Cohesive Failure; ASTM D3167 |
3M Scotch-Weld™ DP920 Epoxy Adhesive 3M™ Scotch-Weld™ Epoxy Adhesive DP920 is a two-part, 2:1 mix ratio, toughened epoxy structural adhesive with a 20 minute work life. It exhibits excellent shear and peel strengths along with good i.. |
|||
Peel Strength | 5.26 kN/m | 30.0 pli | Adhesion to Polyethylene |
3M EPS-200 Tubing 3M EPS-200 is a 2:1 thin-wall tubing offering the advantages of integral adhesive-lined construction. The tubing is made from a flame-retardant, flexible polyolefin with a thing layer of special the.. |
|||
Peel Strength | 5.26 kN/m | 30.0 pli | Adhesion to Polyethylene |
3M EPS-300 Heat Shrink Tubing 3M Heat Shrink tubing EPS-300 is a 3:1 thin-wall, flexible tubing offering the advantages of integral, adhesive-lined construction. The tubing is made from flame-retardant, flexible polyolefin with .. |
|||
Peel Strength | 5.26 kN/m | 30.0 pli | Adhesion to Polyethylene |
3M EPS-400 Heat Shrink Tubing 3M Heat Shrink tubing EPS-400 is a medium-wall, semi-rigid tubing offering the advantages of integral, adhesive-lined construction. The tubing is made from flame-retardant, flexible polyolefin with .. |
|||
Peel Strength | 5.26 kN/m | 30.0 pli | T-Peel |
3M Scotch-Weld™ DP810 Tan Structural Adhesive 3M™ Scotch-Weld™ Low-Odor Acrylic Adhesives are two-part, 1:1 mix ratio, toughened structural adhesives with less odor than most acrylic adhesives. The adhesives have excellent shear and peel stre.. |