Lord Adhesives Versilok® 262 / 254 Acrylic Adhesive

Category Polymer , Adhesive
Manufacturer Lord Adhesives
Trade Name Versilok®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Lord Adhesives Versilok® 262 / 254 Acrylic Adhesive.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
LORD Versilok® 262/254 adhesive is a two-component, epoxy-modified acrylic adhesive used to bond a variety of automotive sheet metals, including hot-dip galvanized, electro-galvanized, bare aluminum, and cold rolled steel. Versilok 262/254 adhesive can be either room temperature cured or heat cured for faster processing.Glass beads are included in the adhesive system providing a mechanical lock between substrates. Versilok 262/254 adhesive also contains an odor suppressant. Versilok 262/254 adhesive is approved by Chrysler (MS-CD-500).All information provided by Lord.
Physical Properties Metric English Comments
Density 1.17 - 1.24 g/cc
0.0423 - 0.0448 lb/in³
262 Resin
1.39 - 1.46 g/cc
0.0502 - 0.0527 lb/in³
254 Hardener
Brookfield Viscosity 40000 - 300000 cP

@Temperature 25.0 °C
40000 - 300000 cP

@Temperature 77.0 °F
254 Hardener; HAT-TD @ 5rpm
195000 - 435000 cP

@Temperature 25.0 °C
195000 - 435000 cP

@Temperature 77.0 °F
262 Resin; HAT-TD @ 5rpm
Mechanical Properties Metric English Comments
Elongation at Yield 25 - 30 %
25 - 30 %
ASTM D638
Impact Test >= 10.2 J
>= 7.50 ft-lb
GM 9751P
Peel Strength >= 5.26 kN/m
>= 30.0 pli
ASTM D1876
Thermal Properties Metric English Comments
Flash Point >= 93.0 °C
>= 199 °F
262 Resin; Closed Cup
>= 93.0 °C
>= 199 °F
254 Hardener; Closed Cup
Processing Properties Metric English Comments
Cure Time 30.0 - 40.0 min

@Temperature 25.0 °C
0.500 - 0.667 hour

@Temperature 77.0 °F
Handling strength
Shelf Life 6.00 Month

@Temperature 25.0 °C
6.00 Month

@Temperature 77.0 °F
Descriptive Properties Value Comments
Appearance Gray
254 Hardener
White/Light Green
262 Resin
Consistency Paste
262 Resin
Paste
254 Hardener
Press Flow (sec) 15-35
20g, 80psi @ 25ºC; orifice #1, 0.052"
20-60
20g, 80psi @ 25ºC; orifice #1, 0.052"