Material Notes:
Resinlab™ AR 4315 HP is a 1:1 mix methacrylate-based structural adhesive formulated to bond almost all engineered thermoplastics, thermosets, composites, and metal structural elements together in any combination. It has excellent adhesion to as-received metal surfaces including aluminum, stainless and plated steels, and forms tough, high strength bonds without surface preparation, primers, or chemical wipes. It contains special adhesion promoters to enhance performance on hard to bond materials such as nylon, chrome and rubber. It features a medium cure time for assembly flexibility to allow for positioning and multiple operations, but provides for faster fixturing. AR 4315 HP has outstanding durability and environmental resistance to many common industrial solvents, fuels, lubricants, and environmental conditions. This product is formulated as a non-sag, creamy gel with matched viscosity for both parts, and is easy to dispense through static mixer tubes and other dispensing equipment.Information Provided by Resinlab L.L.C., an Ellsworth Adhesives Company.
Physical Properties Metric English Comments
Viscosity 250000 cP
250000 cP
Part A, Spindle TD, 2.5 rpm; Uncured
280000 cP
280000 cP
Spindle TD, 2.5 rpm; Curing
300000 cP
300000 cP
Part B, Spindle TD, 2.5 rpm; Uncured
Mechanical Properties Metric English Comments
Hardness, Shore D 70
70
Cured
Elongation at Yield 15 %
15 %
Cured
Adhesive Bond Strength 24.1 MPa
3500 psi
alum/aluminum
27.6 MPa
4000 psi
steel/steel
Impact >= 13
>= 13
[J/in^2]; FRP/FRP; auto side impact
Peel Strength >= 5.26 kN/m
>= 30.0 pli
steel/steel
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 121 °C
250 °F
Cured
Minimum Service Temperature, Air -40.0 °C
-40.0 °F
Flash Point 10.6 °C
51.0 °F
LCC; Uncured
Descriptive Properties Value Comments
Color Amber
Part B; Uncured
Off White
Part A; Uncured
Fixture Time (minutes) 18-20
Curing
Mix Ratio 1:1
Weight and Volume; Uncured
Working Time (minutes) 10-12