Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Peel Strength | 3.86 kN/m | 22.0 pli | Bond Strength; Arlon SQA-TMS-011 |
Arlon 4570XB025 0.025" (0.635 mm) Uncured Silicone Rubber with Fiberglass Substrate
(discontinued **)< Design/Construction: Interleave: PolyethyleneSide 1: Uncured Silicone Rubber Substrate: Style 1165 Fiberglass This data represents typical values for the production material. The data should not be .. |
|||
Peel Strength | 3.86 kN/m | 22.0 pli | T-peel, Al to Al |
Master Bond Supreme 11AN Two Component, Heat Resistant Epoxy Adhesive Description: Master Bond Polymer Adhesive System Supreme 11AN is a two component thermally conductive heat resistant epoxy adhesive with a one-to-one mix ratio, by weight or volume. It readily devel.. |
|||
Peel Strength | 3.86 kN/m | 22.0 pli | Bond Strength; ASTM D624 |
Arlon 55578R028 0.028" (0.711 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction: Interleave: LDPESide 2, Layer 2: Uncured Silicone Rubber Side 2, Layer 1: Cured Silicone Rubber Substrate: Style 162 Fiberglass Side 1: Silicone Skim Coat Appearance: Red silico.. |
|||
Peel Strength | 3.86 kN/m | 22.0 pli | 90°, Adhesion to Stainless Steel |
3M Bumpon™ SJ5816 Resilient Rollstock 3M Bumpon Resilient Rollstock Products are opaque, colored polyurethane materials produced with aggressive pressure-sensitive adhesives.Information provided by 3M |
|||
Peel Strength | 3.86 kN/m | 22.0 pli | 90°, Adhesion to Aluminum |
3M Bumpon™ SJ5816 Resilient Rollstock 3M Bumpon Resilient Rollstock Products are opaque, colored polyurethane materials produced with aggressive pressure-sensitive adhesives.Information provided by 3M |
|||
Peel Strength | 3.86 kN/m | 22.0 pli | 90°, Adhesion to Stainless Steel |
3M Bumpon™ SJ5832 Resilient Rollstock 3M Bumpon Resilient Rollstock Products are opaque, colored polyurethane materials produced with aggressive pressure-sensitive adhesives.Information provided by 3M |
|||
Peel Strength | 3.86 kN/m | 22.0 pli | 90°, Adhesion to Aluminum |
3M Bumpon™ SJ5832 Resilient Rollstock 3M Bumpon Resilient Rollstock Products are opaque, colored polyurethane materials produced with aggressive pressure-sensitive adhesives.Information provided by 3M |
|||
Peel Strength | 3.86 kN/m | 22.0 pli | 180° Canvas to Polypropylene |
3M Jet-melt™ 3731 Polyolefin Bonding Adhesive 3M™ Jet-Melt™ Polyolefin Bonding Adhesive 3731 is 100% solids, high heat resistant adhesive that bonds to a variety of substrates including polyethylene and many other plastics.Information provide.. |
|||
Peel Strength | 3.86 kN/m | 22.0 pli | 180° Canvas to Polycarbonate |
3M Jet-melt™ 3731 Polyolefin Bonding Adhesive 3M™ Jet-Melt™ Polyolefin Bonding Adhesive 3731 is 100% solids, high heat resistant adhesive that bonds to a variety of substrates including polyethylene and many other plastics.Information provide.. |
|||
Peel Strength | 3.86 kN/m | 22.0 pli | on canvas |
3M Scotch-Weld™ 3731 Hot Melt Adhesive High heat resistance and Bonds plastics including polyethylene, polypropyleneInformation provided by 3M |
|||
Peel Strength | 3.86 kN/m | 22.0 pli | T-Peel, Aged 71°C for 2 weeks, Substrate failure |
3M Scotch-Weld™ TE031 Polyurethane Reactive Adhesive 3M™ Scotch-Weld™ Polyurethane Reactive Adhesives are a family of one-component, moisture curing, urethane adhesives. These adhesives are applied warm and bond a wide variety of substrates such as .. |
|||
Peel Strength | 3.86 kN/m | 22.0 pli | 180°, Polystyrene |
3M Scotch-Weld™ TE040 Polyurethane Reactive Adhesive 3M™ Scotch-Weld™ Polyurethane Reactive Adhesives are a family of one-component, moisture curing, urethane adhesives. These adhesives are applied warm and bond a wide variety of substrates such as .. |
|||
Peel Strength | 3.86 kN/m | 22.0 pli | T-Peel, Initial, Substrate failure |
3M Scotch-Weld™ TE040 Polyurethane Reactive Adhesive 3M™ Scotch-Weld™ Polyurethane Reactive Adhesives are a family of one-component, moisture curing, urethane adhesives. These adhesives are applied warm and bond a wide variety of substrates such as .. |
|||
Peel Strength | 3.86 kN/m | 22.0 pli | T-Peel, Aged 71°C for 2 weeks, Substrate failure |
3M Scotch-Weld™ TE100 Polyurethane Reactive Adhesive 3M™ Scotch-Weld™ Polyurethane Reactive Adhesives are a family of one-component, moisture curing, urethane adhesives. These adhesives are applied warm and bond a wide variety of substrates such as .. |
|||
Peel Strength | 3.86 kN/m | 22.0 pli | T-Peel, Aged 71°C for 2 weeks, Substrate failure |
3M Scotch-Weld™ TS230 Polyurethane Reactive Adhesive 3M™ Scotch-Weld™ Polyurethane Reactive Adhesives are a family of one-component, moisture curing, urethane adhesives. These adhesives are applied warm and bond a wide variety of substrates such as .. |
|||
Peel Strength | 3.86 kN/m | 22.0 pli | 90°, Adhesion to Stainless Steel |
3M SJ5500 Protective Product, Molded Shapes 3M Bumpon Protective Products Molded Shapes – Colored and Clear Series are pressure-sensitive, adhesive-back polyurethane products. They can be used as feet, stops, spaces, and protectors in many a.. |
|||
Peel Strength | 3.86 kN/m | 22.0 pli | 90°, Adhesion to Aluminum |
3M SJ5500 Protective Product, Molded Shapes 3M Bumpon Protective Products Molded Shapes – Colored and Clear Series are pressure-sensitive, adhesive-back polyurethane products. They can be used as feet, stops, spaces, and protectors in many a.. |
|||
Peel Strength | 3.86 kN/m | 22.0 pli | 90°, Adhesion to Stainless Steel |
3M SJ5700 Protective Product, Molded Shapes 3M Bumpon Protective Products Molded Shapes – Colored and Clear Series are pressure-sensitive, adhesive-back polyurethane products. They can be used as feet, stops, spaces, and protectors in many a.. |
|||
Peel Strength | 3.86 kN/m | 22.0 pli | 90°, Adhesion to Aluminum |
3M SJ5700 Protective Product, Molded Shapes 3M Bumpon Protective Products Molded Shapes – Colored and Clear Series are pressure-sensitive, adhesive-back polyurethane products. They can be used as feet, stops, spaces, and protectors in many a.. |
|||
Peel Strength | 3.86 kN/m | 22.0 pli | 180° T-Peel, Etched Al/Etched Al |
3M Scotch-Weld™ DP820 Acrylic Adhesives 3M™ Scotch-Weld™ Acrylic Adhesive DP820 is a two-part, 1:1 mix ratio, toughened acrylic structural adhesives. They exhibit excellent shear and peel strengths along with good impact and durability .. |
|||
Peel Strength | 3.86 kN/m | 22.0 pli | 180° T-Peel, Etched Al/Etched Al |
3M Scotch-Weld™ DP820 Acrylic Adhesives 3M™ Scotch-Weld™ Acrylic Adhesive DP820 is a two-part, 1:1 mix ratio, toughened acrylic structural adhesives. They exhibit excellent shear and peel strengths along with good impact and durability .. |
|||
Peel Strength | 3.86 kN/m | 22.0 pli | 180° T-Peel, Etched Al/Etched Al |
3M Scotch-Weld™ DP820 Acrylic Adhesives 3M™ Scotch-Weld™ Acrylic Adhesive DP820 is a two-part, 1:1 mix ratio, toughened acrylic structural adhesives. They exhibit excellent shear and peel strengths along with good impact and durability .. |
|||
Peel Strength | 3.86 kN/m | 22.0 pli | 180° T-Peel, Etched Al/Etched Al |
3M Scotch-Weld™ DP820 Acrylic Adhesives 3M™ Scotch-Weld™ Acrylic Adhesive DP820 is a two-part, 1:1 mix ratio, toughened acrylic structural adhesives. They exhibit excellent shear and peel strengths along with good impact and durability .. |
|||
Peel Strength | 3.86 kN/m | 22.0 pli | 180° T-Peel, Nitrile/CRS |
3M Scotch-Weld™ DP820 Acrylic Adhesives 3M™ Scotch-Weld™ Acrylic Adhesive DP820 is a two-part, 1:1 mix ratio, toughened acrylic structural adhesives. They exhibit excellent shear and peel strengths along with good impact and durability .. |
|||
Peel Strength | 3.86 kN/m | 22.0 pli | Steel, 180° after aging 1-2 days @ RT and 1 day |
3M Scotch-Weld™ Hi-Strength Postforming 4693 High Performance Industrial Plastic Adhesives Features:Low viscosity grade for spray or brush applicationClear elastomeric adhesives with high immediate bond strength, long tack range and contact bond propertiesExhibits outstanding bond strengt.. |
|||
Peel Strength | 3.86 kN/m | 22.0 pli | Steel, 180° after aging 1-2 days @ RT and 1 day |
3M Scotch-Weld™ Hi-Strength Postforming 4693H High Performance Industrial Plastic Adhesives Features: High Viscosity grade in collapsible tubes for flow applicationsClear elastomeric adhesives with high immediate bond strength, long tack range and contact bond propertiesExhibits outstandin.. |
|||
Peel Strength | 3.86 kN/m | 22.0 pli | 90°, Adhesion to Stainless Steel |
3M SJ5000 Protective Product, Molded Shapes 3M Bumpon Protective Products Molded Shapes – Colored and Clear Series are pressure-sensitive, adhesive-back polyurethane products. They can be used as feet, stops, spaces, and protectors in many a.. |
|||
Peel Strength | 3.86 kN/m | 22.0 pli | 90°, Adhesion to Stainless Steel |
3M Bumpon™ SJ5808 Resilient Rollstock 3M Bumpon Resilient Rollstock Products are opaque, colored polyurethane materials produced with aggressive pressure-sensitive adhesives.Information provided by 3M |
|||
Peel Strength | 3.86 kN/m | 22.0 pli | 90°, Adhesion to Aluminum |
3M Bumpon™ SJ5808 Resilient Rollstock 3M Bumpon Resilient Rollstock Products are opaque, colored polyurethane materials produced with aggressive pressure-sensitive adhesives.Information provided by 3M |
|||
Peel Strength | 3.86 kN/m | 22.0 pli | Bond Strength; Arlon SQA-TMS-011 |
Arlon 44570XB025 0.025" Uncured Silicone Rubber with Fiberglass Design/Construction:Interleave: 2.5 mil PolyethyleneSide 1: Uncured Silicone RubberSubstrate: Style 1165 FiberglassThis data represents typical values for the production material and should not b.. |