Polymer Property : 1% Secant Modulus, TD = 145 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
1% Secant Modulus, TD 145 MPa
21000 psi
ASTM D882
LyondellBasell Petrothene® NA362176 Low Density Polyethylene
ApplicationsPETROTHENE NA 362 is a series of low density/EVA copolymers designed for ice bags, bag-in-box, heavy-duty skin packaging and other high strength, easy to seal packaging. NA 362 exhibits..
1% Secant Modulus, TD 145 MPa
21000 psi
ASTM D882
LyondellBasell Petrothene® NA362005 Low Density Polyethylene
ApplicationsPETROTHENE NA 362 is a series of low density/EVA copolymers designed for ice bags, bag-in-box, heavy-duty skin packaging and other high strength, easy to seal packaging. NA 362 exhibits..
1% Secant Modulus, TD 145 MPa
21000 psi
ASTM D882
Westlake Mxsten CV77512 Polyethylene Plastomer
Mxsten CV plastomer CV77512 is a polyethylene plastomer designed for blown film extrusion that contains high slip, high antiblock and high processing aid additives. Films produced with this resin ex..
1% Secant Modulus, TD 145 MPa
21000 psi
ASTM-D822
Westlake Mxsten CV77519 Polyethylene Plastomer
Mxsten CV Plastomer CV77519 is a polyethylene plastomer designed for blown film extrusion that contains no slip and no antiblock. It does contain high processing aid. Films produced with this resin ..
1% Secant Modulus, TD 145 MPa
21000 psi
ASTM D882
Westlake Mxsten CV77523 Polyethylene Plastomer
Mxsten CV plastomer CV77523 is a polyethylene plastomer designed for blown film extrusion that contains high slip, very high antiblock and polymer processing aid additives. Films produced with this ..
1% Secant Modulus, TD 145 MPa
21000 psi
ASTM D882
ExxonMobil LDPE LD 306.57 Low Density Polyethylene Resin
Product Description: LD 306 resins are 5.5% vinyl acetate copolymer, high clarity film resins. Film made from these resins exhibit superior impact strength and heat sealability.Availability: Latin A..
1% Secant Modulus, TD 145 MPa
21000 psi
ASTM D882
ExxonMobil LDPE LD 306.75 Low Density Polyethylene Resin
Product Description: LD 306 resins are 5.5% vinyl acetate copolymer, high clarity film resins. Film made from these resins exhibit superior impact strength and heat sealability.Availability: Latin A..
1% Secant Modulus, TD 145 MPa
21000 psi
ASTM D882
ExxonMobil LDPE LD 317.09 Low Density Polyethylene Resin
Product Description: LD 317.09 resin is a fractional melt index, 6% vinyl acetate copolymer film resin. Film made from LD 317.09 offers excellent impact strength, tensile properties and heat sealabi..
1% Secant Modulus, TD 145 MPa
21000 psi
ASTM D882
ExxonMobil LL 3001.32 Cast Film Resin
Product Description: LL 3001.32 is a hexane copolymer LLDPE designed for the blown or cast film process. Films made from LL 3001.32 have outstanding tensile and toughness properties. The superior st..
1% Secant Modulus, TD 145 MPa
21000 psi
ASTM D882
ExxonMobil LLDPE LL 3001.32 Cast Linear Low Density Polyethylene Resin
Product Description: LL 3001.32 is a hexane copolymer LLDPE designed for the blown or cast film process. Films made from LL 3001.32 have outstanding tensile and toughness properties. The superior st..
1% Secant Modulus, TD 145 MPa
21000 psi
ASTM D882
ExxonMobil LDPE LD 306.38 Low Density Polyethylene Resin
Product Description: LD 306 resins are 5.5% vinyl acetate copolymer, high clarity film resins. Film made from these resins exhibit superior impact strength and heat sealability.Availability: Latin A..