Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Yield Strength | 117.2 MPa | 17000 psi | ASTM D790 |
Ensinger ENSILON® 6/6 Extruded Nylon 6/6 (PA66)
(discontinued **) ENSILON materials have high mechanical strength and superior resistance to wear and organic chemicals.Ensilon grades have been replaced by Tecamid.Information supplied by Ensinger, Inc. |
|||
Flexural Yield Strength | 117 MPa | 17000 psi | ASTM D790 |
PolyOne Lubri-Tech™ NL-10GF/15TF Nylon 6/12 - 10% Glass Fiber - 15% PTFE Flock
(discontinued **) Data provided by PolyOne. |
|||
Flexural Yield Strength | 117 MPa | 17000 psi | ASTM D790 |
Solvay Specialty Polymers Udel® P-3700 HC Polysulfone (PSU) Udel® P-3700 HC is a high-clarity grade of polysulfone (PSU) that is nearly water-white in color. This grade was designed to eliminate the yellow cast and provide design flexibility and improved .. |
|||
Flexural Yield Strength | 117 MPa | 17000 psi | ASTM D790 |
Techmer ES Luriblend® PA6/6 ML2 Nylon 66 Availability: North AmericaForms: PelletsAdditive: Molybdenum Disulfide Lubricant(2%)Features: Lubricated and Good Wear ResistanceInformation provided by TP Composites, Inc. |
|||
Flexural Yield Strength | 117 MPa | 17000 psi | ASTM D790 |
Techmer ES Luriblend® PA6/6 X Nylon 66 Availability: North AmericaForms: PelletsAdditive: Lubricant Features: Lubricated, Good Wear Resistance and Low FrictionInformation provided by TP Composites, Inc. |
|||
Flexural Yield Strength | 117 MPa | 17000 psi | 2.6 mm/min, 100 mm span; ASTM D790 |
SABIC Innovative Plastics NORYL HS2000X PPE+PS PPE+PS blend. 17% Mineral reinforced. Non-brominated, non-chlorinated FR system. UL94 V0 and 5VA listing. UL746C f1. Radiant panel listing. Dielectric strength. Dimensional stability. Suitable for E.. |
|||
Flexural Yield Strength | 117 MPa | 17000 psi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics NORYL N1150 PPE+PS Noryl* N1150 is an unfilled, injection moldable modified polyphenylene ether resin. Designed for good dimensional stability and good flow, this resin also uses non-chlorinated, non-brominated FR add.. |
|||
Flexural Yield Strength | 117 MPa | 17000 psi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics Valox® SHF4910 PBT (Europe-Africa-Middle East) 6.5% glass reinforced, Super High Flow, flame retardant PBT. |
|||
Flexural Yield Strength | 117 MPa | 17000 psi | ASTM D790 |
Sumitomo Bakelite North America 1907-1 / 1907B-1 Glass Reinforced Hardware Grade Epoxy Epoxy is the premier material for military firewall connectors.Information provided by Sumitomo Bak North America, Inc. |
|||
Flexural Yield Strength | 117 MPa | 17000 psi | ASTM D790 |
PlastxWorld CEVIAN® SUG30 ABS Glass fiber reinforced, high heat resistant and flame retarded ABSThese are typical values and are not intended for specification purposes. UL approved file No. is E47773. Information provided by P.. |
|||
Flexural Yield Strength | 117 MPa | 17000 psi | ASTM D790 |
Tipco Tipcolene® SEB 200 - 20% Chemically Coupled Glass Fiber Polypropylene Homopolymer with High Heat Stability 20% Chemically Coupled Glass Reinforced PP HomopolymerApplications: General PurposeProcessing: Injection MoldingInformation provided by the Manufacturer, Tipco Industries Ltd.,
India. |
|||
Flexural Yield Strength | 117 MPa | 17000 psi | ASTM D790 |
E-Polymers TEKAMID® TA210L Lubricated PA66, DAM LubricatedInformation provided by E-Polymers Co. Ltd. |
|||
Flexural Yield Strength | 117 MPa | 17000 psi | ASTM D790 |
E-Polymers TEKAMID® TA210F Fast Crystallinity PA66, DAM Fast crystallinityInformation provided by E-Polymers Co. Ltd. |
|||
Flexural Yield Strength | 117 MPa | 17000 psi | ASTM D790 |
Chem Polymer Chemlon 212 Nylon 6, Lubricated, GP A medium viscosity, general purpose injection molding grade nylon 6. Internally lubricated for excellent mold release properties.Data provided by the manufacturer, Chem Polymer. |
|||
Flexural Yield Strength | 117 - 228 MPa | 17000 - 33100 psi | Average value: 154 MPa Grade Count:16 |
Overview of materials for Polyphenylene Ether, 30% Glass Filled This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Ether, 30% Glass Filled". Specific grades with glass content between 25% and 34% are inclu.. |
|||
Flexural Yield Strength | 117 MPa | 17000 psi | ASTM D790 |
PlastxWorld CEVIAN® A2603 15% GF PA/ABS Alloy, DAM Property data is for dry as molded (DAM) samples.These are typical values and are not intended for specification purposes. UL approved file No. is E47773. Information provided by PlastxWorld Inc. |
|||
Flexural Yield Strength | 117 MPa | 17000 psi | ASTM D790 |
PlastxWorld CEVIAN® A2604 20% GF PA/ABS Alloy, Conditioned Property data is for samples at equilibrium moisture (1.1%)These are typical values and are not intended for specification purposes. UL approved file No. is E47773. Information provided by PlastxWo.. |
|||
Flexural Yield Strength | 117 MPa | 17000 psi | ASTM D790 |
Techmer ES HiFill FR® PPO/HIPS MM20 FR 20% Mineral Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Mineral Filler, 20% Filler by Weight Features: Flame RetardantInformation provided by TP Composites, Inc. |