Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Yield Strength | 96.0 MPa | 13900 psi | 2.6 mm/min, 100 mm span; ASTM D790 |
SABIC Innovative Plastics Cycoloy® C2800 PC+ABS (Asia Pacific) Non-chlorinated and non-brominated flame retardant PC/ABS offering balanced flow and impact for various applications. |
|||
Flexural Yield Strength | 96.0 MPa | 13900 psi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Cycoloy® CX7240 PC+ABS (Asia Pacific) Cycoloy* CX7240 resin is an injection moldable PC/ABS blend. It contains non-brominated and non-chlorinated flame retardant systems to meet UL-94 V0 at 0.75mm, V1 at 0.6mm, V2 at 0.4mm and 5VB at 1... |
|||
Flexural Yield Strength | 96.0 MPa | 13900 psi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Cycoloy® CX7240U PC+ABS (Europe-Africa-Middle East) Cycoloy* CX7240U resin is an injection moldable PC/ABS blend with a UV stabilization package. It contains non-brominated and non-chlorinated flame retardant systems to meet thin wall flame resistanc.. |
|||
Flexural Yield Strength | 96.0 MPa | 13900 psi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics Lexan® 121 PC (Asia Pacific) Nonhalogenated. 17.5 MFR, for small intricate parts. |
|||
Flexural Yield Strength | 96.0 MPa | 13900 psi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics Lexan® 124R PC (Asia Pacific) LEXAN 124R is a low viscosity multi purpose grade. FDA food contact compliant in limited colors. Effective January 15th, 2007 this grade is no longer supported with biocompatibility information an.. |
|||
Flexural Yield Strength | 96.0 MPa | 13900 psi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics Lexan® 241 PC (Asia Pacific) 10.5 MFR. Improved flame retardance. |
|||
Flexural Yield Strength | 96.0 MPa | 13900 psi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics Lexan® 244R PC (Asia Pacific) LEXAN 244R resin grade is a medium viscosity multi purpose product with improved flame resistance and release properties. It is also FDA food contact compliant available in limited colors. |
|||
Flexural Yield Strength | 96.0 MPa | 13900 psi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Lexan® ML7667 PC Copolymer (Asia Pacific) Lexan* ML7667 specialty polycarbonate (PC) resin is a 9% GF reinforced, UV stabilized, flame retarded injection molding grade. This medium flow specialty PC resin combines UL94 V0 @ 1.5mm, 5VB @ 3.. |
|||
Flexural Yield Strength | 96.0 MPa | 13900 psi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics Lexan® OQ4320R PC (Asia Pacific) Optical grade with UV cut-off up to 400 nm; greater optical purity than standard grades. For sunglass and sunvisor markets. Internal mold release. |
|||
Flexural Yield Strength | 96.0 MPa | 13900 psi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Lexan® SLX1231T PC Copolymer Low viscosity PC copolymer blend with enhanced UV stabilization and added release agent. Available in transparent and tinted colorsThis data was supplied by SABIC-IP for the Americas region. |
|||
Flexural Yield Strength | 96.0 MPa | 13900 psi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics Lexan® SLX2271T PC Copolymer Low viscosity PC copolymer blend with enhanced UV stabilization and added release agent. V2 rated. Available in transparent and tinted colors |
|||
Flexural Yield Strength | 96.0 MPa | 13900 psi | ASTM D790 |
LG Chemical Lupoy 1200-03 Polycarbonate Resin Description: LUPOY PC 1200-03 resin is designed for extrusion and injection molding products. It exhibits an excellent physical property balance of heat resistance, transparency and impact strength... |
|||
Flexural Yield Strength | 96.0 MPa | 13900 psi | ASTM D790 |
LG Chemical Lupoy 1300-15 Polycarbonate Resin Description: LUPOY PC 1300-15 resin is designed for extrusion and injection molding products. It exhibits an excellent physical property balance of heat resistance, transparency and impact strength... |
|||
Flexural Yield Strength | 96.0 MPa | 13900 psi | ASTM D790 |
LG Chemical Lupoy 1301V-7 Polycarbonate Resin Description: LUPOY PC 1301V-07 resin is designed for extrusion and injection molding products. It exhibits an excellent physical property balance of heat resistance, transparency and impact strength.. |
|||
Flexural Yield Strength | 96.0 MPa | 13900 psi | ASTM D790 |
LG Chemical Lupoy 1302-07 Polycarbonate Resin Description: LUPOY PC 1302-07 resin is designed for extrusion and injection molding products. It exhibits an excellent physical property balance of heat resistance, transparency and impact strength... |
|||
Flexural Yield Strength | 96.0 MPa | 13900 psi | ASTM D790 |
LG Chemical Lupoy 1603-06 Polycarbonate Resin Description: LUPOY PC 1603-06 resin is designed for extrusion products. It exhibits an excellent physical property balance of heat resistance, transparency and impact strength.Main Characteristics: .. |
|||
Flexural Yield Strength | 96.0 MPa | 13900 psi | ASTM D790 |
LG Chemical Lupoy NF1007F 10R Polycarbonate Resin Description: LUPOY NF 1007F10R, eco-friendly UL94 V0/3.0 mm, is designed for extrusion and injection molding products. It combines an excellent physical property balance of heat resistance, transpar.. |
|||
Flexural Yield Strength | 96.0 MPa | 13900 psi | ASTM D790 |
LG Chemical Lupoy NF1009F 08R Polycarbonate Resin Description: LUPOY NF 1009F08R, eco-friendly UL94 V0/2.0 mm, is designed for extrusion and injection molding products. It combines an excellent physical property balance of heat resistance, transpar.. |
|||
Flexural Yield Strength | 96.1 MPa @Thickness 3.20 mm |
13900 psi @Thickness 0.126 in |
10mm/min; ASTM D790 |
LG Chemical LUPOY GN5101RF PC/ABS Mineral Filler Description: Injection Molding, PC/ABS Mineral Filler, General Purpose, High Stiffness, Halogen Free Flame RetardantApplication: E&E (Housing), IT/OA (Notebook PC Housing)CAS: 103598-77-2, 9003-56-9.. |
|||
Flexural Yield Strength | 96.0 MPa | 13900 psi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics LNP LUBRILOY Lexan_WR6300 AES+PC+SAN LNP* Lubriloy* Lexan_WR6300 compound is a wear resistant PC+SAN, with proprietary lubricant, for business equipment applications. |
|||
Flexural Yield Strength | 96.0 MPa | 13900 psi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics Xenoy® X4830 PBT+PC Xenoy X4830 is a hydrostable, high modulus, low temperature ductile PC/PBT blend. Furthermore, this resin provides high chemical resistance, very low creep, low CTE, excellent fatique and high heat .. |
|||
Flexural Yield Strength | 96.1 MPa | 13900 psi | ASTM D790 |
Shinkong Synthetic Fibers Shinite® D201M20 PBT, 20% Mineral Filled Information from Shinkong Synthetic Fibers Corp. |
|||
Flexural Yield Strength | 96.0 MPa | 13900 psi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics Xenoy® X5300WX PBT+PC (Asia Pacific) Unreinforced, opaque PBT+PC alloy. Chemical resistance and good mechanical performance. UV-stabilized. Excellent weatherability. |
|||
Flexural Yield Strength | 96.0 MPa | 13900 psi | 2.6 mm/min, 100 mm span; ASTM D790 |
SABIC Innovative Plastics NORYL EM7301F PPE+PS 10% glass-reinforced. HDT 252F. Good flow and polyurethane foam adhesion. Black only. |
|||
Flexural Yield Strength | 96.1 MPa | 13900 psi | ASTM D790 |
Cheng Yu Plastic C1300 PC/ABS |
|||
Flexural Yield Strength | 95.83 MPa | 13900 psi | |
Abatron AboCast 50-3/AboCure 50-12 Epoxy Data provided by the manufacturer, Abatron, Inc. Light motor oil viscosity, almost colorless. Shelf life is 12+ months. |
|||
Flexural Yield Strength | 96.0 MPa | 13900 psi | 1.3 mm/min, 50 mm span; ASTM D 790 |
SABIC Innovative Plastics Lexan® ML6240 PC Copolymer (Europe-Africa-Middle East) Low viscosity PC copolymer blend with enhanced UV stabilization and added release agent. Available in transparent and tinted colorsThis data was supplied by SABIC-IP for the Europe-Africa-Middle Eas.. |
|||
Flexural Yield Strength | 96.0 MPa | 13900 psi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Lexan® ML6240 PC Copolymer (Europe-Africa-Middle East) Low viscosity PC copolymer blend with enhanced UV stabilization and added release agent. Available in transparent and tinted colorsThis data was supplied by SABIC-IP for the Europe-Africa-Middle Eas.. |
|||
Flexural Yield Strength | 96.0 MPa | 13900 psi | 1.3 mm/min, 50 mm span; ASTM D 790 |
SABIC Innovative Plastics Lexan® SFX123RU PC SFX123RU is a transparent SecurFX grade with improved flow, mold release and UV stabilizer. This grade is for security applications and contains proprietary authentication technology.This data was s.. |
|||
Flexural Yield Strength | 96.0 MPa | 13900 psi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Lexan® SLX2071T PC Copolymer (Europe-Africa-Middle East) High viscosity PC copolymer blend with enhanced UV stabilization and added release agent. V2 rated. Available in transparent and tinted colors |