| Category | Polymer , Adhesive , Thermoset , Epoxy |
| Manufacturer | Abatron |
| Trade Name | AboCast |
| Port | Ningbo port,China |
| Trade Terms | EXW, FOB, CFR, CIF |
| Payment Terms | L/C, T/T, PayPal |
| Download PDF | Abatron AboCast 50-3/AboCure 50-12 Epoxy.pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Viscosity | 1.0 cP | 1.0 cP | 50-12 water-like viscosity |
| 11000 - 14000 cP | 11000 - 14000 cP | 50-3 | |
| 2250 cP @Temperature 25.0 °C |
2250 cP @Temperature 77.0 °F |
at 100/13 (50-3/50-12) pbw |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Hardness, Rockwell M | 106 | 106 | |
| Tensile Strength, Ultimate | 78.6 MPa | 11400 psi | |
| Elongation at Break | 4.4 % | 4.4 % | |
| Flexural Yield Strength | 95.83 MPa | 13900 psi | |
| Flexural Modulus | 3.00 GPa | 435 ksi | |
| Compressive Yield Strength | 112.38 MPa | 16299 psi | |
| Compressive Modulus | 3.03 GPa | 440 ksi | |
| Izod Impact, Notched | 0.267 J/cm | 0.500 ft-lb/in |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Maximum Service Temperature, Air | 111 °C | 232 °F | Deflection temperature; load unknown. |
| Electrical Properties | Metric | English | Comments |
|---|---|---|---|
| Electrical Resistivity | 6.10e+15 ohm-cm | 6.10e+15 ohm-cm | |
| Surface Resistance | 7.85e+15 ohm | 7.85e+15 ohm | |
| Dielectric Constant | 3.42 @Frequency 1e+6 Hz |
3.42 @Frequency 1e+6 Hz |
|
| 3.9 @Frequency 1000 Hz |
3.9 @Frequency 1000 Hz |
||
| 4.02 @Frequency 60 Hz |
4.02 @Frequency 60 Hz |
||
| Dissipation Factor | 0.0074 @Frequency 60 Hz |
0.0074 @Frequency 60 Hz |
|
| 0.020 @Frequency 1000 Hz |
0.020 @Frequency 1000 Hz |
||
| 0.032 @Frequency 1e+6 Hz |
0.032 @Frequency 1e+6 Hz |
| Processing Properties | Metric | English | Comments |
|---|---|---|---|
| Pot Life | 30 min | 30 min | 500 g |
| Descriptive Properties | Value | Comments |
|---|---|---|
| Exotherm | 255°C | Peak |