Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Yield Strength | 99.0 MPa | 14400 psi | ASTM D790 |
NYCOA 512 PA 6 UL and NSF rated nucleated general purpose molding gradeInformation provided by NYCOA, Inc. |
|||
Flexural Yield Strength | 99.0 MPa | 14400 psi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Cycoloy® CX3222ME PC+ABS Cycoloy* resin grade CX3222ME is an extrudable & thermoformable PC/ABS blend with non brominated and non chlorinated flame retardant systems. Key features of low gloss and good impact make it ideal .. |
|||
Flexural Yield Strength | 99.0 MPa | 14400 psi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Cycoloy® CX7510 PC+ABS (Europe-Africa-Middle East) Cycoloy* CX7510 resin is an injection moldable, flame retardant PC/ABS blend, with non-chlorinated & non-brominated flame retardants. Key features of Cycoloy CX7510 resin include high heat, high flo.. |
|||
Flexural Yield Strength | 99.0 MPa | 14400 psi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics Lexan® EXL1810T PC Copolymer Lexan* EXL1810T polycarbonate (PC) siloxane copolymer resin is a transparent injection molding grade. This resin offers cold temperature (0 °C) ductility in combination with very high flow char.. |
|||
Flexural Yield Strength | 99.0 MPa | 14400 psi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics Lexan® EXL1810T PC Copolymer (Asia Pacific) Lexan* EXL1810T polycarbonate (PC) siloxane copolymer resin is a transparent injection molding grade. This resin offers cold temperature (0 °C) ductility in combination with very high flow char.. |
|||
Flexural Yield Strength | 99.0 MPa | 14400 psi | 1.3 mm/min, 50 mm span; ASTM D 790 |
SABIC Innovative Plastics Lexan® EXL1880T PC Copolymer (Asia Pacific) Lexan* EXL1880T polycarbonate (PC) siloxane copolymer resin is a UV stabilized, transparent injection molding grade. This resin offers good low temperature (0 C) ductility in combination with very h.. |
|||
Flexural Yield Strength | 99.0 MPa | 14400 psi | 1.3 mm/min, 50 mm span; ASTM D 790 |
SABIC Innovative Plastics Lexan® EXL1880T PC Copolymer (Europe-Africa-Middle East) Lexan* EXL1880T polycarbonate (PC) siloxane copolymer resin is a UV stabilized, transparent injection molding grade. This resin offers good low temperature (0 C) ductility in combination with very h.. |
|||
Flexural Yield Strength | 99.0 MPa | 14400 psi | 1.3 mm/min, 50 mm span; ASTM D 790 |
SABIC Innovative Plastics Lexan® FXE1810T PC Copolymer Lexan* FXE1810T polycarbonate (PC) siloxane copolymer resin is a transparent injection moldable grade. This specialty PC offers excellent processability, very high flow and improved ductility charac.. |
|||
Flexural Yield Strength | 99.0 MPa | 14400 psi | 1.3 mm/min, 50 mm span; ASTM D 790 |
SABIC Innovative Plastics Lexan® FXE1810T PC Copolymer (Asia Pacific) Lexan* FXE1810T polycarbonate (PC) siloxane copolymer resin is a transparent injection moldable grade. This specialty PC offers excellent processability, very high flow and improved ductility charac.. |
|||
Flexural Yield Strength | 99.0 MPa | 14400 psi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics Lexan® HPF1 PC Copolymer 25 MFR LEXAN High Flow Ductile Copolymer Healthcare Grade |
|||
Flexural Yield Strength | 99.0 MPa | 14400 psi | 1.3 mm/min, 50 mm span; ASTM D 790 |
SABIC Innovative Plastics Lexan® HPM1914 PC Copolymer High flow specialty polycarbonate with enhanced hemocompatibility. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). E.. |
|||
Flexural Yield Strength | 99.0 MPa | 14400 psi | 1.3 mm/min, 50 mm span; ASTM D 790 |
SABIC Innovative Plastics Lexan® HPM1914 PC Copolymer (Asia Pacific) High flow specialty polycarbonate with enhanced hemocompatibility. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). E.. |
|||
Flexural Yield Strength | 99.0 MPa | 14400 psi | 1.3 mm/min, 50 mm span; ASTM D 790 |
SABIC Innovative Plastics Lexan® HPM1914 PC Copolymer (Europe-Africa-Middle East) High flow specialty polycarbonate with enhanced hemocompatibility. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). E.. |
|||
Flexural Yield Strength | 99.0 MPa | 14400 psi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics Lexan® HPX8R PC Copolymer Very high flow specialty polycarbonate with outstanding processability and ductility. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 o.. |
|||
Flexural Yield Strength | 99.0 MPa | 14400 psi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics Lexan® HPX8R PC Copolymer (Asia Pacific) Very high flow specialty polycarbonate with outstanding processability and ductility. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 o.. |
|||
Flexural Yield Strength | 99.0 MPa | 14400 psi | 1.3 mm/min, 50 mm span; ASTM D 790 |
SABIC Innovative Plastics Lexan® HPX8R PC Copolymer (Europe-Africa-Middle East) Very high flow specialty polycarbonate with outstanding processability and ductility. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 o.. |
|||
Flexural Yield Strength | 99.0 MPa | 14400 psi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics Lexan® HPXS8R PC Copolymer Very high flow specialty polycarbonate with outstanding processability and ductility. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 o.. |
|||
Flexural Yield Strength | 99.0 MPa | 14400 psi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics Lexan® ML7672 PC (Asia Pacific) Non FR PC + GF, UV-Stabilizer, balanced flow & impact. Available in Opaque only. |
|||
Flexural Yield Strength | 99.0 MPa | 14400 psi | 1.3 mm/min, 50 mm span; ASTM D 790 |
SABIC Innovative Plastics Lexan® EXL1860T PC Copolymer Lexan* EXL1860T polycarbonate (PC) siloxane copolymer resin is a transparent injection molding grade. This resin offers improved release performance, cold temperature (0 °C) ductility in combi.. |
|||
Flexural Yield Strength | 99.0 MPa | 14400 psi | 1.3 mm/min, 50 mm span; ASTM D 790 |
SABIC Innovative Plastics Lexan® EXL1860T PC Copolymer (Asia Pacific) Lexan* EXL1860T polycarbonate (PC) siloxane copolymer resin is a transparent injection molding grade. This resin offers improved release performance, cold temperature (0 °C) ductility in combi.. |
|||
Flexural Yield Strength | 99.0 MPa | 14400 psi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Lexan® SLX1432 PC Copolymer (Europe-Africa-Middle East) Medium viscosity PC copolymer with enhanced UV stabilization and added release agent. Available in opaque colors. Typical minimum color tolerance limit is DE CMC < 1.0 |
|||
Flexural Yield Strength | 99.0 MPa | 14400 psi | ASTM D790 |
Global POM-100 High Viscosity Acetal Homopolymer Information provided by Global Polymers Corporation. |
|||
Flexural Yield Strength | 99.0 MPa | 14400 psi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics LNP LUBRICOMP IFL21 PA6.12 LNP LUBRICOMP* IFL21 is a compound based on Nylon 6/12 resin containing 5% Glass Fiber, 10% PTFE. Added features of this material include: Wear Resistant. |
|||
Flexural Yield Strength | 99.0 MPa | 14400 psi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics Xenoy® X4850 PBT+PC (Europe-Africa-Middle East) Xenoy X4850 is a hydrostable, high modulus, high ductile PC/PBT blend. Furthermore, this resin provides high chemicalresistance, very low creep, low CTE, excellent fatique and high heat dimensional .. |
|||
Flexural Yield Strength | 99.0 MPa | 14400 psi | 2.6 mm/min, 100 mm span; ASTM D790 |
SABIC Innovative Plastics NORYL PX1390 PPE+PS Automotive applications, primarily. Excellent electrical properties, easy processability, high heat, 295F (146C) DTUL. |
|||
Flexural Yield Strength | 99.0 MPa | 14400 psi | 1.3 mm/min, 50 mm span; ASTM D 790 |
SABIC Innovative Plastics Xenoy® X5600WX PC+POLYESTER (Europe-Africa-Middle East) Unreinforced, opaque Polyester+PC alloy. Chemical resistance, dimensional stability and mechanical performance. UV Stabilized. Mold ReleaseThis data was supplied by SABIC-IP for the Europe-Africa-Mi.. |
|||
Flexural Yield Strength | 99.0 MPa | 14400 psi | 2.6 mm/min, 100 mm span; ASTM D790 |
SABIC Innovative Plastics NORYL EN265 PPE+PS Extrusion grade. 254F (123C) DTUL. UL94 V-1 rated. |
|||
Flexural Yield Strength | 99.0 MPa | 14400 psi | 1.3 mm/min, 50 mm span; ASTM D 790 |
SABIC Innovative Plastics Lexan® EXRL0681 PC Copolymer 25 MFR LEXAN High Flow Ductile CopolymerThis data was supplied by SABIC-IP for the Americas region. |
|||
Flexural Yield Strength | 99.0 MPa | 14400 psi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics Lexan® HFD1731 PC Copolymer (Asia Pacific) 25 MFR LEXAN High Flow Ductile Copolymer UV-stabilized, available in transparent colors only |
|||
Flexural Yield Strength | 99.0 MPa | 14400 psi | 1.3 mm/min, 50 mm span; ASTM D 790 |
SABIC Innovative Plastics Noryl FXN2090H PPE+HIPS (Asia Pacific) Noryl* FXN2090H resin is an unfilled, injection moldable grade. Designed for exceptionally high gloss and improved pencil hardness vs. standard Noryl grades, FXN2090H resin uses non-halogenated FR a.. |