Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Yield Strength | 96.0 MPa | 13900 psi | 2.6 mm/min, 100 mm span; ASTM D790 |
SABIC Innovative Plastics Cycoloy® C2800 PC+ABS (Asia Pacific) Non-chlorinated and non-brominated flame retardant PC/ABS offering balanced flow and impact for various applications. |
|||
Flexural Yield Strength | 96.0 MPa | 13900 psi | 2.6 mm/min, 100 mm span; ASTM D790 |
SABIC Innovative Plastics Cycoloy® C2950HF PC+ABS Non-chlorinated and non-brominated flame retardant PC/ABS offering balanced impact and heat properties plus improved flow for various applications. |
|||
Flexural Yield Strength | 96.0 MPa | 13900 psi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics Cycoloy® C7410 PC+ABS (Asia Pacific) Cycoloy* C7410 resin is a talc-filled PC+ABS, nonhalogenated FR for thinwall molding applications. |
|||
Flexural Yield Strength | 96.0 MPa | 13900 psi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Cycoloy® CX2244ME PC+ABS Cycoloy* CX2244ME resin is a flame retardant PC/ABS blend featuring excellent balance of flow and impact together with UL-94 V0 rating at < 1mm. Cycoloy CX2244ME resin also demonstrates improved che.. |
|||
Flexural Yield Strength | 96.0 MPa | 13900 psi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics Lexan® 124R PC (Asia Pacific) LEXAN 124R is a low viscosity multi purpose grade. FDA food contact compliant in limited colors. Effective January 15th, 2007 this grade is no longer supported with biocompatibility information an.. |
|||
Flexural Yield Strength | 96.0 MPa | 13900 psi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics Lexan® 221R PC (Asia Pacific) 17.5 MFR, for small, intricate parts. Improved flame retardance. Internal mold release. |
|||
Flexural Yield Strength | 96.0 MPa | 13900 psi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics Lexan® 241R PC General purpose polycarbonate with 10.5 MFR and internal mold release. |
|||
Flexural Yield Strength | 96.0 MPa | 13900 psi | 1.3 mm/min, 50 mm span; ASTM D 790 |
SABIC Innovative Plastics Lexan® EXL1192C PC Copolymer High flow, polycarbonate siloxane copolymer resin. Notched izod ductile to -20C ductility. Enhanced processability compared to standard PC resins. Available in a range of transparent colors.
US .. |
|||
Flexural Yield Strength | 96.0 MPa | 13900 psi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics Lexan® FXE121R PC Transparent PC. ILLUMINATE special effects (fluorescent/edge glow colors). MFR 18.2. Internal mold release. |
|||
Flexural Yield Strength | 96.0 MPa | 13900 psi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics Lexan® HP2 PC Med/high flow polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO and steam sterilizable. Contains m.. |
|||
Flexural Yield Strength | 96.0 MPa | 13900 psi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics Lexan® HP4REU PC (Europe-Africa-Middle East) Medium flow polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO and steam sterilizable. Contains mold .. |
|||
Flexural Yield Strength | 96.0 MPa | 13900 psi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics Lexan® HPS2 PC Med/high flow polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO, steam, e-beam and gamma sterilizable.. |
|||
Flexural Yield Strength | 96.0 MPa | 13900 psi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics Lexan® LS2 PC UL rated HB as of 10/97. 200 series recommended when V-2 rating required. Automotive lens applications. Medium viscosity. UV-stabilized. Transparent colors only. |
|||
Flexural Yield Strength | 96.0 MPa | 13900 psi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Lexan® ML7667 PC Copolymer (Europe-Africa-Middle East) Lexan* ML7667 specialty polycarbonate (PC) resin is a 9% GF reinforced, UV stabilized, flame retarded injection molding grade. This medium flow specialty PC resin combines UL94 V0 @ 1.5mm, 5VB @ 3.. |
|||
Flexural Yield Strength | 96.0 - 181 MPa @Temperature 100 - 200 °C |
13900 - 26300 psi @Temperature 212 - 392 °F |
Average value: 119 MPa Grade Count:2 |
Overview of materials for Polyphthalamide (PPA) This property data is a summary of similar materials in the MatWeb database for the category "Polyphthalamide". Each property range of values reported is minimum and maximum values of appropriate Ma.. |
|||
Flexural Yield Strength | 96.0 MPa | 13900 psi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Lexan® SLX1231D PC Copolymer (Europe-Africa-Middle East) Low viscosity PC copolymer blend with enhanced UV stabilization and added release agent. Available in diffusion colors.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
Flexural Yield Strength | 96.0 MPa | 13900 psi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics Lexan® SLX1231T PC Copolymer (Asia Pacific) Low viscosity PC copolymer blend with enhanced UV stabilization and added release agent. Available in transparent and tinted colors |
|||
Flexural Yield Strength | 96.0 MPa | 13900 psi | ASTM D790 |
LG Chemical Lupoy 1200-08 Polycarbonate Resin Description: LUPOY PC 1200-08 resin is designed for extrusion and injection molding products. It exhibits an excellent physical property balance of heat resistance, transparency and impact strength... |
|||
Flexural Yield Strength | 96.0 MPa | 13900 psi | ASTM D790 |
LG Chemical Lupoy 1201-15 Polycarbonate Resin Description: LUPOY PC 1201-15 resin is designed for extrusion and injection molding products. It exhibits an excellent physical property balance of heat resistance, transparency and impact strength... |
|||
Flexural Yield Strength | 96.0 MPa | 13900 psi | ASTM D790 |
LG Chemical Lupoy 1301EP30 Polycarbonate Resin Description: LUPOY PC 1301EP-30 resin is designed for extrusion and injection molding products. It exhibits an excellent physical property balance of heat resistance, transparency and impact strengt.. |
|||
Flexural Yield Strength | 96.0 MPa | 13900 psi | ASTM D790 |
LG Chemical Lupoy 1261-03 Polycarbonate Resin Description: LUPOY PC 1261-03 resin is designed for extrusion blow molding(EBM) and injection stretch blow molding (ISBM) products. It exhibits an excellent physical property balance of heat resista.. |
|||
Flexural Yield Strength | 96.0 MPa | 13900 psi | ASTM D790 |
LG Chemical Lupoy 1302-07 Polycarbonate Resin Description: LUPOY PC 1302-07 resin is designed for extrusion and injection molding products. It exhibits an excellent physical property balance of heat resistance, transparency and impact strength... |
|||
Flexural Yield Strength | 96.0 MPa | 13900 psi | ASTM D790 |
LG Chemical Lupoy 3030-15 Polycarbonate Resin Description: LUPOY PC 3030-15 resin is designed for injection molding products. It exhibits an excellent physical property balance of heat resistance, transparency and impact strength.Main Character.. |
|||
Flexural Yield Strength | 96.0 MPa | 13900 psi | ASTM D790 |
LG Chemical Lupoy 1303-07 Polycarbonate Resin Description: LUPOY PC 1303-07 resin is designed for extrusion and injection molding products. It exhibits an excellent physical property balance of heat resistance, transparency and impact strength... |
|||
Flexural Yield Strength | 96.0 MPa | 13900 psi | 1.3 mm/min, 50 mm span; ASTM D 790 |
SABIC Innovative Plastics Noryl TN240 PPE+PS PPE+PS blend. Unfilled. Transparent. Good flow. Scratch resistant. Injection molding. Suitable for housewares, personal care and small appliance applications.This data was supplied by SABIC-IP for t.. |
|||
Flexural Yield Strength | 96.0 MPa | 13900 psi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics LNP LUBRILOY Lexan_WR6300 AES+PC+SAN LNP* Lubriloy* Lexan_WR6300 compound is a wear resistant PC+SAN, with proprietary lubricant, for business equipment applications. |
|||
Flexural Yield Strength | 96.0 MPa | 13900 psi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Xenoy® IQ4840 PBT+PC (Asia Pacific) Xenoy iQ4840 (PBT+PC) resin is an environmental responsible, sustainable, and low carbon footprint resin. It is a 10% mineral filled resin with high modulus and ductile (HMD) characteristics. Xen.. |
|||
Flexural Yield Strength | 96.0 MPa | 13900 psi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics XYLEX X7507 PC+POLYESTER (Europe-Africa-Middle East) F-1 weathering certified in natural color, specially designed for Pool & Spa applications. Currently available in natural color only. |
|||
Flexural Yield Strength | 96.0 MPa | 13900 psi | 1.3 mm/min, 50 mm span; ASTM D 790 |
SABIC Innovative Plastics Xylex X7509UV PC+POLYESTER (Europe-Africa-Middle East) PC+POLYESTER, Transparent, UV-Stabilized,This data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
Flexural Yield Strength | 96.0 MPa | 13900 psi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics Lexan® HP4NR PC (Europe-Africa-Middle East) Medium flow polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO and steam sterilizable. Contains no m.. |