Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Yield Strength | 75.0 MPa | 10900 psi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics Cycoloy® CX5430 PC+ABS Cycoloy* resin CX5430 is a general purpose PC/ABS blend developed for thin wall applications requiring weld line strength, high flow and impact together with a good balance of other properties. |
|||
Flexural Yield Strength | 75.0 MPa | 10900 psi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Cycoloy® C1100HF PC+ABS (Europe-Africa-Middle East) CYCOLOY C1100HF is the improved flow version of CYCOLOY C1100 and has been developed to better fill long and complex parts while maintaining still excellent mechanical properties. Its superior flow .. |
|||
Flexural Yield Strength | 75.0 MPa | 10900 psi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Cycoloy® CX5430 PC+ABS (Europe-Africa-Middle East) Cycoloy* resin CX5430 is a general purpose PC/ABS blend developed for thin wall applications requiring weld line strength, high flow and impact together with a good balance of other properties.This .. |
|||
Flexural Yield Strength | 75.0 MPa | 10900 psi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics GELOY XTPM405 ASA+PC High flow PC/ASA with improved impact at room and low temperatures. Improved release. Excellent weatherability for outdoor unpainted or clearcoated applications. Injection Moldable with large color .. |
|||
Flexural Yield Strength | 75.0 MPa | 10900 psi | 1.3 mm/min, 50 mm span; ASTM D 790 |
SABIC Innovative Plastics Lexan® DMX6014 PC Copolymer (Asia Pacific) DMX6014 is an injection moldable PC copolymer ABS blend. This resin combines excellent scratch resistance (F-pencil hardness) with ductility.This data was supplied by SABIC-IP for the Asia Pacific r.. |
|||
Flexural Yield Strength | 75.0 MPa | 10900 psi | 6.4 mm; ASTM D790 |
SABIC Innovative Plastics Lexan® FL2000 PC Lexan FL2000 is a medium flow specialty polycarbonate (PC) resin for structural foam molding, allowing for various weight reductions at 0.24"" (6.0mm) wall. This product offers low temperature impa.. |
|||
Flexural Yield Strength | 75.0 - 200 MPa @Temperature -40.0 - 90.0 °C |
10900 - 29000 psi @Temperature -40.0 - 194 °F |
Average value: 136 MPa Grade Count:3 |
Overview of materials for Nylon 66, 20% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 20% Glass Fiber Filled". Specific grades with glass content between 15% and 24% are included. .. |
|||
Flexural Yield Strength | 75.0 - 455 MPa | 10900 - 66000 psi | Average value: 275 MPa Grade Count:245 |
Overview of materials for Nylon 66, 40% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 40% Glass Fiber Filled". Specific grades with glass content between 35% and 44% are included. .. |
|||
Flexural Yield Strength | 75.0 MPa | 10900 psi | ASTM D790 |
Ineos Nova 3101 General Purpose Crystal Polystyrene Good balance of flow and set-up properties, Good crack resistanceApplications: Single service cutlery, Single service drinkware, Consumer electronic packagingExposure to gamma radiation in the 2.02-.. |
|||
Flexural Yield Strength | 75.0 MPa | 10900 psi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics NORYL RN0401 PPE+PS Noryl RN0401 resin is an unfilled Post Consumer Recycle (PCR) based injection moldable modified polyphenylene ether blend comprising at least 20% PCR content. Available in black only. |
|||
Flexural Yield Strength | 75.0 MPa | 10900 psi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics NORYL RN0401 PPE+PS (Europe-Africa-Middle East) Noryl RN0401 resin is an unfilled Post Consumer Recycle (PCR) based injection moldable modified polyphenylene ether blend comprising at least 20% PCR content. Available in black only. |
|||
Flexural Yield Strength | 75.0 MPa | 10900 psi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics NORYL SE90 PPE+HIPS (Europe-Africa-Middle East) NORYL SE90 is an unfilled, flame retardant material with a Vicat B/120 of 110°C according ISO 306. NORYL SE90 is V1 at 1.6 mm according UL94 and halogen free according VDE/DIN 472 part 815. |
|||
Flexural Yield Strength | 75.0 MPa | 10900 psi | 2.6 mm/min, 100 mm span; ASTM D790 |
SABIC Innovative Plastics LNP LUBRICOMP Noryl_SPN422L PPE+HIPS (Europe-Africa-Middle East) LNP* Lubricomp Noryl_SPN422L is a wear resistant, fluorocarbon alloy, 235F (113C) HDT. UL94 HB rated. Check surface aesthetics prior to material specification. |
|||
Flexural Yield Strength | 75.0 MPa | 10900 psi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics Valox® IQ357 PBT+PC (Asia Pacific) Valox* Resin IQ357: Environmentally responsible, low carbon footprint iQ* PBT + PC alloy. UL94 V-0 @0.63 mm. Impact modified. |
|||
Flexural Yield Strength | 75.0 MPa | 10900 psi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics Valox® IQ357 PBT+PC (Europe-Africa-Middle East) Valox* Resin IQ357: Environmentally responsible, low carbon footprint iQ* PBT + PC alloy. UL94 V-0 @0.63 mm. Impact modified. |
|||
Flexural Yield Strength | 75.0 MPa | 10900 psi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics Valox® IQ357M PBT+PC Valox* Resin IQ357M: Environmentally responsible, low carbon footprint iQ* PBT + PC alloy. UL94 V-0 @0.63 mm. Impact modified, easy flow product with mold release. |
|||
Flexural Yield Strength | 75.0 MPa | 10900 psi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Xenoy® CL101 PBT+PC Xenoy CL101 is an unfilled, impact modified PC/PBT blend with excellent solvent resistance and low-temperature ductility. It has a proven track record in off-line painted exterior automotive applica.. |
|||
Flexural Yield Strength | 75.0 MPa | 10900 psi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Xenoy® CL101 PBT+PC (Asia Pacific) Xenoy CL101 is an unfilled, impact modified PC/PBT blend with excellent solvent resistance and low-temperature ductility. It has a proven track record in off-line painted exterior automotive applica.. |
|||
Flexural Yield Strength | 75.0 MPa | 10900 psi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Xenoy® HX5600HP PBT+PC Xenoy HX5600HP is PBT based semi-crystalline blend with balanced flow and impact properties. Improved chemical resistance against lab disinfectants and chemicals for healthcare enclosure and housing.. |
|||
Flexural Yield Strength | 75.0 MPa | 10900 psi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics NORYL GTX GTX944 PPE+PA NORYL GTX944 is an unfilled GTX grade with improved processability and increased impact performance. |
|||
Flexural Yield Strength | 75.0 MPa | 10900 psi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics NORYL GTX GTX944 PPE+PA (Europe-Africa-Middle East) NORYL GTX944 is an unfilled GTX grade with improved processability and increased impact performance. |
|||
Flexural Yield Strength | 75.0 MPa | 10900 psi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics NORYL HN731SE PPE+HIPS (Europe-Africa-Middle East) PPE+PS blend. For medical devices and pharmaceutical applications. NORYL HN731SE is an unfilled material, with a Vicat B/120 of 135C according ISO 306. Healthcare management of change, biocompati.. |
|||
Flexural Yield Strength | 75.0 MPa | 10900 psi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics NORYL N190 PPE+HIPS (Europe-Africa-Middle East) NORYL N190 is an unfilled, flame retardant material with a Vicat B/120 of 105°C according ISO 306. NORYL N190 is V0 at 1.52 mm and 5VA at 3.12 mm according UL94 and halogen free according VDE/DIN.. |
|||
Flexural Yield Strength | 75.0 MPa | 10900 psi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Xenoy® XD1575S PBT+PC (Europe-Africa-Middle East) XENOY XD1575S is a high flow PC+PBT blend with good impact properties and good resistance to occasional solvent and gasoline contact. XENOY XD1575S has been specially developed for coated exterior b.. |
|||
Flexural Yield Strength | 75.0 MPa | 10900 psi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics NORYL PX1007 PPE+HIPS (Europe-Africa-Middle East) NORYL* PX1007 is an unfilled non-chlorinated, non-brominated flame retardant PPE/HIPS grade, targeted for flat panel TV enclosures. It has a Vicat B/120 temperature of 96 degC and UL-94 V0 @ 1.5mm .. |
|||
Flexural Yield Strength | 75.0 MPa | 10900 psi | ASTM D790 |
E-Polymers TEKAMID® TA210ST Super Tough PA66, DAM Super ToughnessInformation provided by E-Polymers Co. Ltd. |
|||
Flexural Yield Strength | 75.0 - 85.0 MPa | 10900 - 12300 psi | ASTM D790 |
Chang Chun Plastic PBT1100L General Purpose PBT Information provided by Dowell Trading Company Ltd. |
|||
Flexural Yield Strength | 75.0 MPa | 10900 psi | 2 mm/min; ASTM D790 |
Solvay Specialty Polymers Solef® 1012 PVDF Homopolymer
(discontinued **) Key features of this grade: High Viscosity, Virgin. Recommended processing is extrusion. Available as powder & granules.General information about SOLEF® PVDF: SOLEF® PVDF is a fluorinated semi-c.. |
|||
Flexural Yield Strength | 75.0 MPa | 10900 psi | DIN 53 452 |
Albis Plastics Tedur® L 9560 PPS, 50% Mineral High Gloss, Highest Surface Finish, Metallization w/o Base Coating. Incandescent wire resistance (2 mm) is 960°C per VDE 0471 T1.2.Applications: Various High Temperature ReflectorsProcessing: Inje.. |
|||
Flexural Yield Strength | 75.0 MPa | 10900 psi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics GELOY XP4025 ASA+PC Available in a wide range of colors and is recommended for unpainted exterior applications. |